Bharat Forge Expands in U.S. with Tennessee Acquisition

  Source:  Forging

Directors of Bharat Forge Ltd., in Pune, India, approved the company’s acquisition of 100% of the shares of Walker Forge Tennessee LLC (WFT), in Surgoinsville, TN, making it a subsidiary of its Bharat Forge America holding.

Read More:  Bharat Forge Expands in U.S. with Tennessee Acquisition

Bharat Forge Expands in U.S. with Tennessee Acquisition Read More »

Jorgensen Forge Acquired

Source:  Forging

Jorgensen Forge, a Tukwila, WA, open-die forger and ring-rolling operation, has emerged from Chapter 11 bankruptcy as one of three companies now owned by CE Star Holdings LLC, a company formed to buy the assets from Constellation Enterprises, which filed for creditor protection in May.

The Seattle-area plant forges low alloy and stainless grades of steel, aluminum alloys, titanium alloys, and nickel-based alloys. Production equipment includes four open-die presses and two ring-rolling mills. It also offers heat-treating and machining, and it has special capabilities for “marine shafting” as well as full testing and inspection services. Its customers are manufacturers supplying aerospace, energy, defense, and general industrial markets.

Read More: Jorgensen Forge Acquired, “Even Better Positioned” by Robert Brooks

Jorgensen Forge Acquired Read More »

3D TUS Software Released to Heat Treat Market

Photography by Quang Nguyen

Long-time heat treating expert, Peter Huskek of Phoenix Heat Treating, a fourth generation commercial heat treating institution, is branching out into the computer simulation arena with a very impressive, 3D temperature uniformity survey (TUS) reporting tool called Virtual Visual Surveys (www.virtualvisualsurveys.com). What Mr. Hushek and his team, including key developer Jeff Murch, have developed under the company name of Thermal Innovation Technologies, Inc., is a 3D visualization tool capable of showing furnace operators what their furnace uniformity looks like. This 3D visualization software helps quality personnel know if a furnace will pass a TUS, and if not why. It also allows maintenance personnel the opportunity to isolate and diagnose problem areas within the work area of the furnace. The 3D visualization package is offered as a service. For more information, visit www.virtualvisualsurveys.com.

3D TUS Software Released to Heat Treat Market Read More »

Heat Treat Basics: Nitriding and Carburizing

Pattern Energy, Siemens Determine Cause Of Ocotillo Wind Collapse, Energy Heat Treating  Source:  Metlab

Nitriding and carburizing are the two most common heat treatment practices for surface hardening functional components. The main difference is that in nitriding, nitrogen atoms are made to diffuse into the surface of the parts being processed, whereas in carburizing, carbon is used. There are advantages and disadvantages to both processes.

This excellent blog post by Metlab in the Philadelphia area is a great primer for both processes.

Read More:  Nitriding and Carburizing

Heat Treat Basics: Nitriding and Carburizing Read More »

Effective Furnace Scheduling

 By John Young, Young Metallurgical Consulting

Effective furnace scheduling requires the inclusion of several key elements.

“Customer” Demands:  Manufacturers with in-house heat treat departments have internal customers who, like customers the world over have one thing in common, they want to provide parts to you tomorrow and have them processed and ready yesterday.  These internal customers cause frustration and angst but their work is what pays the bills.

Product & Process Variables:  There are numerous product and furnace process variables all of which must be considered when scheduling.  Common variables include:

  • Material grade and chemistry
  • Atmosphere carbon potential
  • Hardening and tempering furnace temperatures
  • Ammonia addition for carbonitriding and the purge time required when finished
  • Belt speeds
  • Cycle times
  • Variable quench programs

Process changes are necessary but minimizing the degree of variation between consecutive product runs is the goal.  The more significant the change, the longer the gap time required to allow the furnace to stabilize with the new furnace parameters.  Gap time is an unrecoverable cost – wasted time and money.

Sample Furnace Scheduling Sheet

 

 

Sample Furnace Scheduling Sheet

Quality issues can also be caused by not allowing sufficient time between significant process parameter changes.  If the proper gap time is not provided, the end of one lot or the beginning of the next may experience quality issues.

Each heat treat department must determine the balance of efficiency and customer service that works best for their operation.

Developing a close working partnership with your internal customers is beneficial for both parties.  Heat treating is typically at or near the end of the manufacturing cycle and all the lead time has been utilized by the previous steps.  Teach them the basics of your operation and explain the ways they can help you provide better service and delivery. By providing as much information as possible about their delivery requirements, you can schedule to meet their demands.

Rush jobs are the nature of the business and will always be with us. They are inevitable but they can be reduced. I know of one customer who provided parts at 3:00 PM and asked for impossible results for the next morning.  After numerous conversations with the heat treat department, the part supplier finally understood the heat treat process and now allows one, two, or even 3 days for results. Encourage part suppliers to give you next week’s Hot List at the end of the current week.

Heat treat scheduling is never easy but it can be improved to help your operation.


About Young Metallurgical Consulting

Young Metallurgical Consulting works with in-house heat treat departments to teach the day-to-day processes necessary to manage and improve their area of operation. In-house heat treaters will learn the aspects of heat treating that are not taught in a classroom and can only be gained through direct, hands-on experience. Contact John Young at john@youngmetallurgicalconsulting.com.

John Young
John Young, Young Metallurgical Consulting

 

Effective Furnace Scheduling Read More »

Jewelry Industry Purchases Annealing Furnaces from C.I. Hayes

C.I. Hayes, a Gasbarre Furnace Group company, is pleased to announce the recent installation
of multiple “Solitaire” Conveyor Belt Furnaces for annealing of precious metals to be used in the
jewelry industry. In total, this project consisted of three identical conveyor belt furnaces, all manufactured and installed for the same customer. Named for its compact design and initially developed for brazing and bright annealing of jewelry pieces, the C.I. Hayes “Solitaire” Conveyor Belt Furnace has found great acceptance in other markets requiring brazing and bright annealing of small, intricate parts.
C.I. Hayes continues to enhance the proven design of its “Solitaire” Furnace Line improving the overall lifetime value. Its robust and simple design allows for ease of manufacture, installation and maintenance, ensuring success for those processes that are driven by both technical and commercial demands. The “Solitaire” Conveyor Belt Furnace is equipped with belt widths of 6-12 inches and effective heat lengths of 27-72 inches. Four-sided heat surrounding the muffle provides excellent uniformity and power input with temperature capabilities to 2100°F (1148°C). The furnace remains compact and may be shipped as a single piece, fully assembled, with single point connections for power, water and atmosphere.

Jewelry Industry Purchases Annealing Furnaces from C.I. Hayes Read More »

Enhanced Properties for Bright 17-7 PH Stainless Steel

  Source:  Today’s Medical Developments

Already extensively used in aerospace, semiaustenitic stainless steel 17-7 PH is finding new applications in the medical industry. The material is most often used in sheet and strip form, with springs, clips, and bellows being widely produced. The high alloy content of 17-7 provides excellent corrosion resistance, an attractive attribute to the medical industry.

Read more to find out how this material behaves after annealing at 1,950°F…….

Enhanced Properties for Bright 17-7 PH Stainless Steel Read More »