Five Tips for Furnace Preventive Maintenance

 

Source: Lindbergh/MPH 

 

Reactive maintenance is expensive and usually requires downtime, holding up production. In contrast, preventive maintenance keeps these failures from occurring, which results in cost savings for manufacturers. Research shows that preventive maintenance can produce a 12 to 18 percent cost savings as opposed to other reactive maintenance programs.

In this Heat Treat Today Best of the Web feature, Lindbergh/MPH offers important preventative maintenance tips for heat treat furnaces.

Preventive maintenance is a list of regularly performed procedures that decreases the likelihood of a piece of equipment failing. It is performed by operators while the machine is in good working order. Regular maintenance also keeps equipment running at top performance and extends its life.

5 Preventive Maintenance Items for your Heat Treat Furnace

Heat treat furnaces are used in many manufacturing processes, including tempering, preheating, quenching, stress relieving, annealing, and more. Many factors, including high temperatures, place considerable wear and tear on the furnace components. Eventually this can cause bearings to flake, leaks to develop, and other problems to come up. Small issues can lead to mechanical failures over time that in turn lead to reactive maintenance.

Some common preventative maintenance services for heat treat furnaces include:

  1. Tuning Combustion Systems – Component wear, high temperatures, and other factors lead to burner settings drifting over time. This ultimately affects efficiency, fuel usage, emissions, and product quality. Tuning the combustion system maintains optimal performance and efficiency rates, limits excess emissions, and improves product quality.
  2. Bearing Inspections – Functional bearings are crucial to any machine, but even properly installed and operated bearings wear down over the course of time. The contact surfaces of bearings repeatedly withstand compressive loads, which eventually causes the surfaces to flake. Inadequate lubricant, improper lubricant type, breakage, wear, corrosion, and other factors can lead to bearing failure. A broken or seized bearing can stop equipment, potentially bringing the entire production line to a halt.
  3. Leak Testing – Even the smallest leak can reduce production performance and possibly result in system failure. Preventive maintenance for leaks includes testing gas shutoff valves and gas train piping for leakage.
  4. Lining Inspections – Gradually the lining of a heat treat furnace may succumb to chipping, cracking, or bubbling. Disruptions to the integrity of the lining, left unchecked, can lead to contamination that harms the quality of the product. Lining inspections prevent contamination.
  5. Safety and NFPA Testing – Safety and National Fire Protection Association (NFPA) testing protects clients from potential damage. It also ensures that preventive measures against workplace accidents are in place.

Read more, The Benefits of Preventive Maintenance

(source: Lindbergh/MPH)

Five Tips for Furnace Preventive Maintenance Read More »

Current Medical Alloy Trends

Thomas Wingens, Wingens International Industry Consultancy

Heat Treat Today’s Medical and Heat Treating December 2019 issue featured an article on medical alloys. Heat Treat Today talked with respected industry expert, Thomas Wingens of Wingens International Industry Consultancy, about current medical alloy trends. Here are some of his thoughts.

To read the full article to which Thomas Wingens’ comments pertain, go to Medical Alloys Their Uses and Heat Treatments

Heat Treat Today: Who is the new kid on the block in medical metals?

Thomas Wingens: Magnesium. While magnesium is a light metal used in the automotive industry, in the last five years it has become a player within the medical industry. Magnesium occurs naturally in our bodies and because our bodies can absorb it, magnesium is being engineered to last for two years and then it will deteriorate back into the body.

HTT: What are the top metals and alloys that are being used today in medical procedures and why are they beneficial to the patient?

TW: Titanium is one of the top metals because it is neutral due to the titanium oxide on the surface which makes it biocompatible.

One of the most used metals is cobalt chromium, which is highly regarded in joint and dental implants because of its outstanding osseointegration, strength, and wear resistance.

Nitinol is another top alloy. It is composed of nickel and titanium. Nickel by itself is not good for the body as it can cause headaches, however, when paired with titanium, it is a balanced alloy that is used in the spine and to produce stents for the heart. It is also a memory shape alloy that I use in STEM presentations to show students how nitinol can be twisted yet, when heated, will return to its original form.

HTT: What are your thoughts on the market forecast of medical heat treating?

TW: When taking into consideration the components of implants, tooling, and equipment, studies have shown a consistent market growth of 5-6% each year. The top joint replacements are hips with the knees, being a more complicated procedure, coming in second. Couple these with prothesis implants and x-ray tubes with copper coils, and business continues to climb.

HTT: What do you see as an exciting or disruptive heat treating technology or material in the medical field?

TW: DISRUPTION is taking place in personalized medicine. There are a bunch of very small devices for sensors and analytical devices for home use, as well for drug delivery.

 

A Quick Guide to Alloys and Their Applications

Titanium

Catheter Wire
(Image source: Medical Design Briefs)
  • Implants
  • Neurostimulators
  • Orthopedic Rods
  • Pins and Plates
  • Heart Valve Housings
  • Prosthetic Eyes
  • Surgical Instruments
  • Drills
  • Forceps
  • Retractors
  • Scissors
  • Needles

Cobalt Chromium

  • Bearing Surfaces Hip/Knee Replacements
Pacemaker Parts
(Image source: Medical Design Briefs)

Niobium

  • Pacemakers

Tantalum

  • Bone Implants,
  • Vascular Clips,
  • Flexible Stents

Nitinol

  • Stents
  • Heart Valve Tools
  • Staples
  • Bone Anchors
  • Septal Defect Devices
  • Diagnostic Guide Wires
  • Arch Wires for Braces

Copper

  • Antigerm Surfaces
  • Medical Electric Devices

 

(Image source: Medical Design Briefs)

 

Current Medical Alloy Trends Read More »

Scientific Breakthrough Treats Metals to Kill Bacteria

Purdue University may have developed a solution that helps address the issue of certain viruses lingering for up to several days on metal surfaces. According to a recent press release, the university’s engineers have created a laser treatment method that intends to morph metal surfaces from bacteria carriers to bacteria killers.

The approach uses a one-step laser texturing technique that changes the texture of a surface’s finish. In the first study, the group used copper, which is apparently well known for its bacteria-killing properties. But what traditionally would take hours is now an instantaneous process, and researchers actually demonstrated this by observing the texturing process’s ability to instantly kill a superbug like MRSA.

Purdue says the process isn’t exactly tailored for specific viruses like COVID-19 at this point, but they have been testing the process on new metals and polymers. The other benefit to this specific approach is that it’s not toxic like other antibacterial coatings can be. They also say that the simplicity and scalability of the technique has allowed researchers to believe that it could make its way into existing medical device manufacturing processes.

(source: Thomasnet.com)

Scientific Breakthrough Treats Metals to Kill Bacteria Read More »

Furnace Temperature Control Options

Ernesto Perez,
Director of Engineering,
Nutec Bickley

In today’s Heat Treat Today Technical Tuesday feature, Ernesto Pérez, Director of Engineering, at Nutec Bickley, introduces readers to different options when it comes to furnace temperature control.

 

The main aim of the temperature control function is to keep a furnace operating within certain predefined values and it is composed of two main parts:

  • Electronic control element, usually a PID (proportional–integral–derivative) controller
  • Mechanical components

In this article we will look at the various control modes used in industrial furnaces, and their applications for various heat treatment processes.

Back to the Beginning: “Zero Control” Mode

Figure 1

Before considering the modes currently used, we should briefly mention the “zero control” mode found in earlier furnace models, employed some time back, also known as “atmospheric mode.”

This mode operates by taking air from the environment by means of the venturi effect to perform combustion without controlling the air flow, resulting in an inefficient use of energy. (Figure 1)

Fuel-Only Control System

Figure 2

This operates in a similar way to zero mode, where only the gas is controlled. However, instead of the air being introduced by the venturi effect, there is a turbo fan that provides a constant flow to the process, while the gas is regulated during the different stages of combustion. (Figure 2)

  • Economic system having a single line of control.
  • It provides good temperature uniformity in applications where all items being fired in the furnace need to be at the same temperature.
  • Ideal for low temperature furnaces, kilns for ceramics and applications that require high-level heating homogeneity.

Possible Disadvantages
This technique leads to high gas consumption due to the heating of all the air present, irrespective of the size of the load in the furnace.

Proportional Control System

Figure 3

With this control mode, the air and the gas are controlled proportionally. (Figure 3)

The operation starts with a small flame, and as the temperature rises, it grows as the air and gas levels increase.

  • This system allows you to adjust the amount of gas based on the air present in order to achieve perfect combustion and optimal fuel consumption.
  • Ideal for any type of furnace, for example for heat treatments such as aging, tempering, forging and normalizing.

Possible Disadvantages
At the beginning of the heating process, it can be the case that temperature uniformity across the entire furnace is not so good due to the small flame, so it is not a system recommended for the treatment of very fragile pieces that can break.

Mass Flow Control System

Figure 4

This system controls air/gas in the same as the previously described method, but it also gives allowance to vary the air/gas ratio during combustion process in order to optimize the fuel. (Figure 4)

  • It enables for the achievement of optimal combustion conditions with less energy input.
  • If more air is needed in a particular heat treatment stage (usually at the beginning), it can be temporarily increased.
  • Ideal for any type of furnace, like heat treatments such as aging, tempering, forging, normalizing and applications involving fragile products.

Possible Disadvantages
Because of the technology behind the system, it is more expensive.

Pulse Control System

Figure 5

This is one of the most recently introduced methods that provides a fixed air/gas ratio, but unlike the previous mentioned systems, flame velocity for product heating is always high, which generates ideal temperature uniformity right from the beginning of the cycle. (Figure 5)

The burners pulse from high-fire to low-fire, repeating this cycle every 15 to 60 seconds.

  • It is cheaper to operate than the mass flow system, allowing users to handle the entire range of products with a smaller investment.
  • It provides greater fuel efficiency by heating the product evenly from the beginning.
  • Ideal for any furnace, for example for heat treatments such as aging, tempering, forging, normalizing and applications involving fragile ceramic products.

Possible Disadvantages
The radiation of the flame can affect certain products; however, by installing an additional instrument it is possible to control this effect and to reduce flame radiation.

Experts in Temperature Control

Nutec Bickley can offer all current systems, advise on the most appropriate choice with the best cost benefits, update old systems with current technology, and provide repair and spare parts services for existing temperature control systems.

 

About the author: Ernesto has been sharing his expertise at Nutec for 18 years. As an electronic system engineer with a master’s degree in artificial intelligence, the 25-year industry veteran has been focused on the control aspect of software and hardware.

 

(All images: Nutec Bickley)

Furnace Temperature Control Options Read More »

Heat Treat Tips: Thermocouples

One of the great benefits of a community of heat treaters is the opportunity to challenge old habits and look at new ways of doing things. Heat Treat Today’s 101 Heat Treat Tips is another opportunity to learn the tips, tricks, and hacks shared by some of the industry’s foremost experts.

For Heat Treat Today’s latest round of 101 Heat Treat Tipsclick here for the digital edition of the 2019 Heat Treat Today fall issue (also featuring the popular 40 Under 40).

Today’s tips come to us from Pelican Wire, covering Thermocouples. This includes advice about correcting irregular part distortion and finding solutions to cracked parts.

If you have a heat treat-related tip that would benefit your industry colleagues, you can submit your tip(s) to anastasia@heattreattoday.com  or editor@heattreattoday.com.


Heat Treat Tip #65

Introducing Your Common Thermocouple Types

What are the common thermocouple types?

Thermocouple material is available in types K, J, E, N, T, R, S, and B. These thermocouple types can be separated into two categories: Base and Noble Metals.

Types K, J, E, N, and T are Base Metals. They are made from common materials such as Nickel, Copper, Iron, Chromium, and Aluminum. Each base metal thermocouple has preferred usage conditions.

Types S, R, and B thermocouples are Noble Metals because they are made of one or more of the noble metals, such as Ruthenium, Rhodium, Palladium, Silver, Osmium, Iridium, Platinum, and Gold. Noble metals resist oxidation and corrosion in moist air. Noble metals are not easily attacked by acids. Some Noble metal thermocouples can be used as high as 3100°F.


Heat Treat Tip #66

Culprits of a Stable Thermocouple

Factors affecting the stability of a thermocouple:
The EMF output of any thermocouple will change slightly with time in service and at elevated temperatures. The rate and change are influenced by metallurgical and environmental factors. The four factors that can induce EMF drift are: Evaporation, Diffusion, Oxidation, and Contamination.


Heat Treat Tip #67

Does Length Matter?

Does the length of a thermocouple wire matter?
In a word, “Yes.” There are several factors when considering the maximum length of a thermocouple assembly. Total loop resistance and electrical noise. Total loop resistance should be kept under 100 ohms for any given thermocouple assembly. Remember, the total loop resistance would include any extension wire used to complete the circuit. Motors and power wires can create noise that could affect the EMF output.

Type K Thermocouple Wire with PFA Heavy Bond (source: Pelican Wire)

Heat Treat Tip #69

Thermocouples Pros & Cons

Pros of thermocouples
1. high accuracy,
2. adaptable to harsh environments as well as high vibration,
3. fast thermal reaction,
4. wide operating temperature range,
5. good reproducibility,
6. low cost.

Cons of thermocouples?
1. Stray voltage pick is possible;
2. The cold junction and lead compensation are essential;
3. They are nonlinear;
4. They have a low output voltage, i.e., less sensitivity.


Heat Treat Tip #70

Type N Thermocouple (Nicrosil/Nisil)

Type N Thermocouple (Nicrosil/Nisil): The Type N shares the same accuracy and temperature limits as the Type K. Type N is slightly more expensive and has better repeatability between 572°F to 932°F (300°C to 500°C) compared to type K.


 

Heat Treat Tips: Thermocouples Read More »

Don’t Wait to Apply for 2020 MTI Scholarships!

Are you a student who is interested in a career in metallurgy, materials, engineering, industrial, mechanical sciences? Do you know anyone who is seeking a degree or technical school certificate in materials science, metallurgy, engineering, mechanical/industrial/electrical sciences?

If so, the MTI Educational Foundation Board of Directors is awarding $51,000 in scholarships in 2020. This includes 7 college scholarships at $5,000, and 4 technical school scholarships at $1,500. If one of the recipients’ application rises above all others, he/she will be awarded an extra $10,000 with the Founder’s Scholarship.

Scholarship applications opened on March 1, 2020, for approved scholarships to be distributed by June 20, 2020.  Check out the current criteria and scholarship application for candidates.  These are subject to final approval.

Full information, criteria, and applications for scholarships may be found when you Click Here.

NOTE:  To complete your application, you will need a digital copy of your latest high school or college transcripts, a copy of your acceptance letter to your college, and two (2) letters of recommendation.  You will be asked to upload these documents in the online form.

DEADLINE FOR APPLICATIONS:  May 31, 2020

Don’t Wait to Apply for 2020 MTI Scholarships! Read More »

Global Tool Manufacturer Acquires Third Vacuum Furnace

An international company producing, among other things, cutting tools, with a rich history and branches in 40 countries, ordered a vacuum furnace, their third order from them to date.

Vector Vacuum Furnace
(source: SECO/WARWICK)

The horizontal, front-loading furnace, from SECO/WARWICK, will accommodate the customer’s needs with an all-metal hot zone for clean vacuum processing. As with the earlier furnaces, one of which was installed at a different facility, the new furnace includes a convection fan and a pressurized gas quench for quick cooling.

Maciej Korecki, VP, Vacuum Furnace Segment at SECO/WARWICK (source: SECO/WARWICK)

Maciej Korecki, VP, Vacuum Furnace Segment at SECO/WARWICK says, “Precision, high uniformity in heat treated parts, high consistency in workloads and high speeds in batch processing along with low energy and gas consumption makes our product most desirable solution on the market. Often our clients demand just one thing – for instance: high uniformity in heat treated parts which solves problems of distortions they experience using different technology. All the other features come as a surprise and an added value.”

Piotr Zawistowski, president, SECO/VACUUM (source: SECO/WARWICK)

According to Piotr Zawistowski, President, SECO/VACUUM, “This third repeat order is a testament to SVT’s on-time delivery and the performance of our . . . vacuum furnace to meet all promised parameters, including producing clean finished parts, all as promised.”

Global Tool Manufacturer Acquires Third Vacuum Furnace Read More »

Mikros Technologies Increases Production Capacity with Vacuum Furnaces

Mikros Technologies, located in New Hampshire, designs and produces liquid cooling systems and micro-machined nozzle plates for applications requiring micron-level dimensions and sub-micron accuracy. So when Mikros needed new multipurpose furnaces for vacuum brazing and diffusion bonding that could withstand continuous production and allow operators to seamlessly change recipes and easily pick up where the last person stopped, they turned to Ipsen USA. Mikros increased production capacity by purchasing two more TITAN® H2 2 bar vacuum furnaces. The first was installed in January 2019, the second in October 2019.

The furnaces met their needs by supporting a variety of heat-treating processes, providing tight temperature uniformity and delivering clean parts. With the high-efficiency design and fast door-to-door cycle times, the furnaces helped Mikros gain manufacturing volume to accommodate the company’s rapid growth.

(source: IPSEN USA)

As a leading provider of complex thermal management solutions for critical applications in power computing, laser optics, semiconductor testing, renewable energy generation, artificial intelligence, and electric vehicle systems, Mikros plays a critical role in allowing data centers and equipment used for transportation, aerospace, and defense to perform optimally and keeping high heat-generating components from overheating and failing prematurely. Some of the microchannel cold plates they manufacture are small and delicate, no larger than a penny. Others are large assemblies that occupy a full computing server rack. Specialized parts like these require careful planning when it comes to heat treatment.

In the last five years, Mikros doubled their workforce and expanded their manufacturing facilities. Mikros makes over 10,000 cold plates per year, and the addition of the furnaces has helped them quadruple their production capacity.

Mikros Technologies Increases Production Capacity with Vacuum Furnaces Read More »

Heat Treat Radio #29: Heat Treating and Coal with Brian Joseph, CEO Touchstone Research

Welcome to another episode of Heat Treat Radio, a periodic podcast where Heat Treat Radio host, Doug Glenn, discusses cutting-edge topics with industry-leading personalities. Below, you can either listen to the podcast by clicking on the audio play button, or you can read an edited version of the transcript. To see a complete list of other Heat Treat Radio episodes, click here.


Audio: Heat Treating and Coal with Brian Joseph, CEO Touchstone Research

In this conversation, Heat Treat Radio host, Doug Glenn, interviews Brian Joseph, the founder, CEO, and president of Touchstone Research Laboratories, about the emerging part that coal is playing in the heat treat world. Listen to find out more about the surprising uses of coal in heat treating, the development of the world's strongest aluminum, and some tips for how to make your organization run at its best.

Click the play button below to listen.


Transcript: Heat Treating and Coal with Brian Joseph, CEO Touchstone Research

The following transcript has been edited for your reading enjoyment.

We are headed to coal country, just outside Wheeling, West Virginia, to talk to Brian Joseph, founder, CEO, and president of Touchstone Research Laboratories as well as several other companies pertinent to the heat treat industry.  If you thought coal was a commodity of the past, I suggest you buckle up for one of the most interesting Heat Treat Radio episodes that will widely expand your appreciation for coal and its future uses in the heat treat industry.

I was introduced to Brian Joseph by Heat Treat Today's lead editor, Karen Gantzer, who just happens to be a relative of Brandon Robinson, a young, very sharp engineer working for one of Brian Joseph's companies, Touchstone Advanced Composites.  Brian and Brandon hosted both Karen and I at their campus in Triadelphia, WV, earlier this year, and were gracious enough to spend an entire afternoon showing us around and talking with us about some of the exceptionally fascinating esoteric work they're doing for all sorts of world leading companies in aerospace, defense, and energy as well as a host of other government agencies and national labs.  I think you'll find this episode fascinating, and I bet you're going to learn something new about coal.

Brian Joseph, Founder, CEO, and president of Touchstone Research Laboratories (source: TouchstoneAC)

Brian Joseph is the president, CEO, and founder of Touchstone Research Laboratory, as well as Touchstone Advanced Composites, Touchstone Testing Laboratory, and CFOAM Limited.

BJ:  I grew up in the panhandle of West Virginia and went to a local university, West Liberty University, and did a little bit of graduate work at Ohio State.  I then started my own business.  I never had a "job."  I've only owned my own business, and that is Touchstone Research Laboratory.  At Touchstone, we invent all kinds of things.  We put out, sometimes, a patent a month, and then we spin businesses out.  We've spun out three businesses in the last three years, and we have probably three more in the works today.

DG:  If I remember correctly, you're doing stuff for the aerospace industry and the automotive industry.  What other major markets are you hitting on?

BJ:  As you can envision, an innovative company like Touchstone Research Laboratory is far ranging.  We do a lot of work in aerospace, we do work in automotive, we do work in general manufacturing; we're inventing all kinds of things all the time.  And then there are our spin-out companies.  Touchstone Laboratory has three locations.  We do a lot of aerospace testing for virtually every aerospace company at those facilities. We test all kinds of materials at Touchstone Testing.

Then we spun out CFOAM, which is probably what we'll talk mostly about today.  This is a foam we make from coal.  In the research lab, we do a lot of coal-to-products research.  This is a foam that is extremely strong and can withstand really high temperature.  CFOAM is a publicly traded company today on the Australian stock exchange.  The applications for that are in numerous markets, one of which is in heat treating.

The third business is called Touchstone Advanced Composites.  Touchstone Advanced Composites takes the foam that CFOAM makes and builds the molds for next generation carbon fiber airplanes, rockets, etc.  Many of these are companies that you would recognize--all of the big aerospace companies, all of the commercial launches to space; we work with virtually everyone to build the molds to make their carbon fiber parts, and we do that on coal, which I think is sort of surprising to people.

DG:  I get excited about this.  This is what I want to tease our audience about a little bit, if you will, is coal.  The place of coal in heat treat.  Where might we find it currently, if at all?  And, in your mind, because I know you're very much a forward thinker, where do you see coal being used in the heat treat market, or even outside the heat treat market in the future?

BJ:  Today, the big uses for coal are electricity, to make electricity to run kilns and things.  In steel making, the coke for steel making and in cement production, we often burn coal to heat the cement.  These are current uses.

Many years ago when I was a kid, there was this basketball player that was named Lou Alcindor, and he was dunking the basketball at will and just dominating college basketball.  So they outlawed it.  They said nobody's allowed to dunk anymore.  In general, you would think that would be devastating.  But no, he just invents a special hook shot called the “sky hook” and now, all of a sudden, he can score from 20' out at will.  He became one of the highest scorers in basketball.  To me, that's what is going on in coal right now.  The things that it is dominating today, that is its primary markets, are under a lot of pressure.  But when I look out, what do I think is going to happen, is a huge number of products.

Let me tell you what we're doing right now.  We take the coal in the CFOAM business, we grind it into powder, we heat it under pressure, and we blow it up into beautiful black foam.  (Think Styrofoam only a thousand times stronger and good to enormously high temperatures, like probably up to 3000°C.)

Over at Touchstone Advanced Composites, they're building the molds to make carbon fiber airplane parts because the foam is high temperature so it will go in the autoclave.  It's very strong. It also does not expand and contract hardly at all with changes in temperature, and that's what you want in the best mold-making material.  What I get a kick out of is, you take coal out of the ground and all of a sudden we're making parts for the James Webb space telescope.

Where else will it be used?  Wow, anywhere you could think of a really high temperature.  Just imagine Styrofoam a thousand times stronger and fireproof.  Where would you use it? Everywhere.  When I think heat treatment, where do I think the obvious applications are? Kiln furniture--the strength of this stuff compresses strength of the low density material is over a thousand pounds per square inch.  Kiln insulation because it is very insulating--especially kiln floors.  Now all of a sudden, you've got a carbon floor you could walk on that is an insulator.  And, by the way, the higher density material that we make has a compressive strength so high you could set a car on one square inch and it wouldn't crush, so we're talking really high strength.

CFOAM carbon foam used as kiln furniture (source: TouchstoneAC)

You can pass electricity through it and use it as a heating element, and we've done that at times.  I could envision someone building some kilns where you lay it up like you do refractory brick today, only a carbon version of refractory brick.  One of the other ones that we don't typically think about, and is this in the heat treatment area?  I don't know, but it's sort of interesting.  CFOAM has a program with Argon National Laboratories.  Argon is working on concentrated solar power. This is the thousands of mirrors in the desert that reflect light up to a single point, and then that heats a fluid and it goes underground and it melts like a salt (like sodium chloride, like the stuff you eat) or magnesium chloride.  You're over 1400°F, so the salt is great material to hold the heat, but it's a really bad material to conduct the heat.  So we're taking the salt, putting it in the pores of the foam, and then using the ligaments of the coal foam to conduct the heat to store the energy in the salt.  Again, what I like about that is we're going to store solar power in coal, which is, again, counterintuitive.

DG:  And a bit of an irony, right?

BJ:  Yes!  I think you're going to see these carbon foams everywhere.

DG:  When we think of the heat treat industry, we certainly don't think about using coal; but in some of these new applications, like you say, being pressed in their major markets, whether it's energy production and things of that sort, there are new applications, and Touchstone Research Labs is developing some of these things.  That to me is what is interesting.

Let's talk outside of heat treat for just a minute.  I want to prime you on one of them, and then if you think of others, feel free to run with them.  You and I spoke previously about the use of coal as architectural structures in the future in place of concrete structures.  Can you hit on that a bit, and if there is anything else outside of the thermal part of coal being used outside the heat treat industry, just go ahead and roll right into those?

BJ:  We're working with a gentleman named Mark Goulthorpe.  He is an architect at MIT.  He has a program called Carbon House with the Department of Energy.  Specifically, it's an ARPA-E program, that's their real advanced technology area, and he presents this story.  He says the world population has been increasing at a very high rate of speed, but the wealth didn't spread around the world for a long time, so people didn't have much money, they didn't make much, and they didn't buy much, so we didn't notice them so much.  But what's happened in the last 20 years, maybe the greatest accomplishment of man in the last 20 years, is we've reduced that extreme poverty 80% worldwide, which is just extraordinary.  So now, all of a sudden, the complex part of this is that these people are moving to cities at a rate of a million people a week.  That means, inside 30 years, we will need to double the number of houses and buildings on the surface of the earth inside 30 years.  The construction boom has already started.  Imagine you've got to build a million, I'll say apartments, and office buildings and things every week until after the year 2050.  He points out, what are we going to build all of this out of?  There is not enough wood on this planet.  You can't use concrete.  If we're concerned about global climate change and that puts out more carbon dioxide than burning coal, so what are our options?  He points out that the answer is probably buried in our hydrocarbons.  Things like methane to carbon nanotubes where we take the carbons and the methane and we make carbon nanotubes.  That will be part of the structure.  Take the hydrogen and make that the fuel.

And at MIT, that's what they're thinking the future is.  And CFOAM will probably play a major role in these kinds of structures because at the end of the day, the coal that we make the foam from is very inexpensive, available in extraordinarily large quantity, and can make fireproof structures that are inexpensive and with a pretty low carbon footprint.  The production of the foam is a very small carbon footprint production.  It does not produce much pollution or production of much CO2 and that kind of thing.  So it's fairly green.  It's funny to talk about coal in a green way, but it really is a pretty green product.  And that may be the thing that gets us there.

DG:  Yes. And compared to the manufacturing of concrete, it's a lot greener manufacturing the CFOAM panels, let's say, as opposed to concrete.

Clean Room (source: TouchstoneAC)

BJ:  Yes, absolutely.  Some fun things to talk about for just a minute:  Over at Touchstone Advanced Composites, we've made the molds to make parts for the James Webb space telescope.  This will be the greatest telescope, I think, the world has ever produced.  I think it's 8 times bigger than Hubble, it will be located a million miles from earth, just so everyone can have a little yardstick, that's four times the distance to the moon, and it will see back in time till to the creation of some of the first galaxies.  We've made all of these parts on molds made from coal.

We just finished building the molds to make the communications dish antenna for the NASA wide field infrared telescope, which is the size of Hubble, and that is going up soon.  We just finished the structures that will be on a solar sail for NASA.  Let me tell you what a solar sail is:  Imagine a kite, only square.  So you have two sticks on a kite.  We're going to make those out of carbon fiber, but we're going to make them in a special way that collapse, so that they go into a box 2' x 2', but when you get up into space, you open this box up and this rolls out 54 ½ ' in all directions.  You end up with this 110' solar sail that is up in space.  What's going to happen is, the light from the sun moves this thing.  Just the light, no propellant.  It will go 240 thousand miles an hour.  And we've built all the molds from CFOAM that we make from coal.

We do work with virtually every one of the commercial launches to space.  We just did the front end of a supersonic aircraft and dozens of other new aircraft that are being built.  All of that is being done on CFOAM.  That's a whole group of fun things we do.

DG:  Can you tell us about MetPreg?

BJ:  At Touchstone Research Laboratory, we're developing the world's strongest aluminum.  This is aluminum with fibers in it.  It's aluminum oxide fibers in aluminum.  What's really interesting about it is it's the highest temperature aluminum that exists, so this will be useful at temperatures up to 1000°F.  It will keep 80% of its strength.  It's 3 times stronger than the world's strongest aluminum alloy.  This is not made from coal.  This is aluminum with fibers.  We either make it in a tape form or pultruded form, or we make it into cylinders by film winding it, like you do polymer composites.  It is a whole new class of materials, and our plan is to spin that out into a separate company, probably within the next year or so.  Right now we're developing the business plan.

We are doing this on-scale already.  It's already been put on a ship.  One of the applications, by the way, is repairing the structures in large ships, especially aluminum hold ships, for fatigue in particular.  Some of these ships are tracking hundreds of fatigue cracks in the structural component, and we can use this as a patch to repair the ships while at sea and have a permanent repair.  This is an application, by the way, that I wouldn't have even come up with.  This is one that the navy came to us and said, is this something you guys could do? So we've been working in a development program with the navy.  It about a million dollar program.  While in the program, we're already on our first ship and we're really excited about that.  That application is ready to go but many of the other applications are still in development.

DG:  You've already run down a list of some of your customers, but maybe just give us a sense of the breadth and depth of your customer base, as many as you're comfortable telling us about.

MetPreg Rocket Motor Casing (source: TouchstoneAC)

BJ:  On the aerospace side, it's virtually everyone in aerospace, from your Boeing and Airbuses, Embraer, to some of your smaller ones that are suppliers to that industry.  We have hundreds and hundreds of people, especially using the CFOAM.  In terms of MetPreg, we're not there yet with flying on airplanes, but I'm really confident we will get there.  We can probably mention the work we do with Virgin. I love Richard Branson, by the way. He is a hero of mine; I think the world of him.  We've done work with some of his companies--Virgin Orbital, Virgin Galactic. They are two separate companies. Virgin Galactic is the one that's going to take people into space.

I want to spin back around and talk about what that means, taking people to space.  The thing we think about is rich people going for joy rides, which is good, and there is a market.  But don't think of it like that.  I think he's building this next generation aircraft that, for example, we'd take off from LA.  Well, it's just as easy to drop you in Chicago as it would be back to LA, in fact I think it's easier.  So I see this is as the beginning of a new way to fly around the world.

I'll give you another one--SpaceX.  They have a similar vision. SpaceX rockets are very different.  They're going to land vertical.  Richard Branson's is going to look like an airplane.  It's going to be more normal looking, but they won't go that fast; they'll go a couple thousand miles/hour maybe, whereas SpaceX is going to go like 18,000 mph.  I saw the president of SpaceX give a talk.  (In fact, by the way, one of our people got to meet Elon Musk just a few weeks ago, and he came back with the biggest grin on his face.)  So the president of SpaceX, says, "I do a lot of business in Riyadh, and I can't wait for the day that I take off from here in California, fly to Riyadh, (it will take about 40 minutes and most of that is landing), and then we'll fly back home in time to fix dinner for the family." It just made me smile. Gwynne Shotwell is awesome in every way.

Now Virgin Orbital is different.  Virgin Orbital shoots rockets up in the air.  They come off of a Boeing 747 that they've named 'Cosmic Girl,' and then it goes into orbit.  That does go fast.  It is not to carry humans, it's to put satellites in orbit.  It's an inexpensive way to put satellites in orbit.  You fly the 747 as high as you can, you tilt it a little bit upwards and you shoot your rocket right into orbit.  It's a lot less expensive than launching from the ground.  That's another one of Richard Branson's businesses and they have a great team of people working there.  I'm really optimistic about it.

For your heat treatment people, think about the temperatures we're dealing with.  The rocket motors are all super high temperature, just through the atmosphere.  It takes you up into the thousands of degrees.  So all the things your client base works with is what the outside of all of these vehicles is.  It's just interesting.  And yet, I don't know that they think in that world right now.  When you look at the number of launches going into space right now, we in the United States don't track what's going on around the world so much, so I'll give you just one example.  Rocket Lab has what they call the Electron rocket.  It will be launched from New Zealand.  Now, I was unaware that New Zealand ever launched a rocket, it's just not something I was aware of.  They're planning to launch 300 launches a year--in New Zealand!  So, what do you think the worldwide going in and out of space is going to be here in the next decade or two? I think it's going to be really large.  And markets for things like thermal protection systems or high temperature components is going to be much bigger than anyone realizes.

DG:  Shifting just a little bit.  Obviously, the organization that you've developed, Touchstone Research Laboratory, etc., your whole organization, all of them, have been very innovative.  Can you speak to the, let's say, culture there and the method by which you push the innovation?  How do you make such an innovative organization?

BJ:  You may have picked up on something with that question.  You've been here, you've walked through, and you have a feel for how we sort of work.  I went to Dearborn, Michigan, once and I went to the Henry Ford Museum in Greenfield Village.  (If anyone has never been there, you've got to go, especially if you like technical things.)  And there, Henry Ford bought Edison's first research laboratory and rebuilt it there.  It's four buildings, so you walk through the world's first industrial research laboratory.  I went there one day about 4 years ago, and I was not necessarily a big Edison fan.  I knew who he was and everything, but when I walked into this building, it was like something was overly familiar.  So I said to my wife, “I have to go back there and spend a day by myself just in the buildings and just look around.”

Here's what I figured out:  As you know, I never "got a job." I went to graduate school, came out, and started my own research laboratory from scratch.  I didn't know all of the modern processes to manage a laboratory.  So I'm sort of figuring out from scratch as a kid in my twenties and trying to work my way through.  And what I ran into was a process that ends up being almost identical to what Edison did.  I'm not saying I'm smart like Edison, I'm just saying that my invention process ended up remarkably similar.  Here's how it goes: In R&D, you need some well educated people, they've got their PhD from Berkeley or MIT or wherever, for example.  But then there is this other group that fabricates stuff.  This person, maybe from MIT, says, “Hey, what if we make this vacuum chamber and heat in this way with microwaves and then we put UV light in?” and that's my idea on Monday morning.  Now it's about how fast can we turn that into something real, run our experiments, and get to the next thing.  In R&D, the thinking part is seconds, minutes, or hours, but the doing part is usually days, weeks, and months.  So if you want to collapse your time of invention, you work on that second side, and you get the best technicians you can.  And they make the people with the high degrees look really smart.  So it's how you blend those together that I think can create this really unique environment, and I think that's sort of money that tricks behind what we do.

(source: TouchstoneAC)

In addition to that, we're a real flat organization and things like that. There are a lot of things that people don't know about Edison's management approach, but he dressed down for work. He didn't want to be seen as the boss at work. He just blended in and went from person to person. When investors would show up, people would be running around, saying, “Get him cleaned up!” At work, he didn't have any airs about him, which is the right answer. The more central control you have, the less your organization has that ability to just run. You've got to handle your organization very gently. He was the first guy to ever build an industrial research facility. He did amazingly well with it, but he was less than perfect. In recent years, there's been a lot of complaints about the details of what he did, but he was the guy out there blazing the trail, so I give him a lot of credit for that.

DG:  Let's circle back around to CFOAM for just a moment.  CFOAM, current and future, especially where it hits on the heat treat market.  Where would we see CFOAM?  You mentioned the fact that the mechanical properties are very strong, it could be used for floors and furnaces, it could be used for hearth piers, hearth rails, could be used for the sides of furnaces.  One of the issues in the heat treat market that we have to be careful about is, you know, the guys on the forklifts who smash the trays into the sides of the furnace during loading and unloading.  I assume there is some strength here in the CFOAM that you might not have another especially ceramic materials, but also maybe some of your metal walls, if you will.

BJ: The foam can be made in a wide range of densities too.  When you were here, I think I showed you two densities that we predominantly manufacture today. One is 20 pounds/cubic foot and the other is 30 pounds/cubic foot. But you can make it up to 90 pounds/cubic foot, which at that point it is massively strong and very high temperature, but not as insulating.  There is a trade-off between insulation and strength.  So what we can do for some of those applications is dial in "what is the appropriate mechanical properties versus thermal properties for an application?" because the technology is really robust that way. In fact, one of the challenges to new materials like this is deciding what is the thing I want to make this week.  Because you can offer all kinds of things, so you have to figure out what are the things you think your customers want.  If customers look at our properties and they're not exactly what they need, there is a good chance we could make some adjustments and make something with either more conductivity, less conductivity; in fact, there is a whole group of things we haven't talked about, which is the other end of the spectrum--very high thermal conductivity foams.  We have some foams that we can make with the thermal conductivity of aluminum at one-fifth the weight.  To me, is there a market?  Does this relate to heat treaters?  It's not obvious to me, and I'm not down on the details of that business, but it wouldn't surprise me at all if someone listening doesn't say, “You know, that's exactly what we need! A carbon that's very thermally conductive.”  So that's the other end of the spectrum.

DG:  So you can make the foam either thermally insulative or conductive, either way?

BJ:  That's right.  And we can bury the electrical properties through ten orders of magnitude, from 10 million ohm centimeters to .1 ohm centimeters.

DG:  The question that jumps into my mind, and this may not be a fair question to ask you, but let me ask it anyhow: The commercial viability of these CFOAM products in the heat treat market.  You can use them as heating elements, I assume.  I don't think we see much.  We see a lot of graphite heating elements, but heating elements, I assume for structural parts, perhaps.  The one that jumps to my mind, and I think I mentioned it to you when I was there, was radiant tubes, which are the metal tubes are somewhat, they have a life cycle, let's put it that way.  Because of thermal cycling, they do tend to, at some point in time, crack or whatever.  We have some companies that are making radiant tubes out of ceramic-type material, but there are sometimes issues with breakage.  My thinking is, is it possible that perhaps we could get coal based radiant tubes even, that are very strong yet very thermally conductive?

BJ:  Yes, I think such a thing would be possible.  I can't tell you that I could give it to you tomorrow afternoon, but absolutely.  I think the material can do it.  I think we can figure out how to actually make that on volume. I think that's very doable.

Another thing: the foam is porous.  Are there situations where you want to bring nitrogen in through the wall at really, really low speeds for some reason, while heating to very high temperature? I don't know; or any other gas--hydrogen or whatever.  I haven't had that need, but I'm not in that particular marketplace that might have that need.

Doug Glenn, Publisher, Heat Treat Today
Doug Glenn, Heat Treat Today publisher and Heat Treat Radio host.


To find other Heat Treat Radio episodes, go to www.heattreattoday.com/radio and look in the list of Heat Treat Radio episodes listed.

Heat Treat Radio #29: Heat Treating and Coal with Brian Joseph, CEO Touchstone Research Read More »

New Additions to the 2020-2021 IHEA Board of Directors and Officers

Scott Bishop, incoming president of IHEA (source: IHEA)

Jeff Valuck, incoming VP of IHEA (source: IHEA)

The Industrial Heating Equipment Association (IHEA) recently announced its 2020 – 2021 Board of Directors and Executive Officers. The new executive officers are Scott Bishop of Alabama Power Company as president, Jeff Valuck of Surface Combustion as vice president, and Brian Kelly of Honeywell Thermal Solutions as treasurer. Outgoing president Michael Stowe of Advanced Energy assumes the role of president emeritus.

Brian Kelly, incoming treasurer for IHEA (source: IHEA)

IHEA also welcomes new board member Alberto Cantu of Nutec Bickley. Alberto has been involved with IHEA since 2011 and participates on the Safety Standards and Codes Committee.

Alberto Cantu, incoming board member of IHEA (source: IHEA)

IHEA President Scott Bishop, who is highly involved in IHEA’s Infrared Division, says, “It is an honor to serve as IHEA’s president for the 2020-2021 term.  I look forward to continuing the great work IHEA has done for more than 90 years.  Also, during this unprecedented time I would like to encourage our members to be proactive in finding ways to better serve our industry and make an impact.” Bishop has served as IRED chairman, presented at numerous workshops and seminars, and provided key support in the recent revision of the Infrared Process Heating Handbook for Industrial Applications. 

Michael Stowe, outgoing president of IHEA (source: IHEA)

“I am very excited about this new role,” Cantu states. “I think it will be a great opportunity to connect with colleagues in the industry and help move it forward,”

 

New Additions to the 2020-2021 IHEA Board of Directors and Officers Read More »