Heat Treat TV: ECM-USA

ECM-USA’s goal to bring sales and service support closer to their North American customers hasn’t changed in over 20 years. A subsidiary of ECM Technologies in Grenoble, France, they are a worldwide manufacturer of low-pressure vacuum carburizing furnaces and other products.

This video takes us through a brief history of their company, their culture, and what services they offer their customers. Take a brief break to learn more about the products and services they provide to their North American customers.

Click here for more information on ECM-USA.

If you have a video you’d like to see included on Heat Treat TV, please send an email to editor@HeatTreatToday.com and include a link to the video.

(source: ECM-USA)

Heat Treat TV: ECM-USA Read More »

inTEST’s Induction Heating Lab Expands To the West Coast

inTEST Corporation, a global supplier of precision-engineered solutions for use in manufacturing and testing across a wide range of markets including automotive, defense/aerospace, and energy, announced today that its thermal segment subsidiary, Ambrell Corporation, is expanding its applications laboratory capabilities in the United States and Europe.

Ambrell’s applications laboratory, known in the industry as THE LAB at Ambrell (THE LAB), is well known in the induction heating market. With applications laboratory facilities in Rochester, NY, and Hengelo, the Netherlands, Ambrell is expanding its laboratory capabilities to a third location on the west coast. The new lab facility will be located in Fremont, California, specifically to serve customers in the western United States and will include hands-on demonstrations and parts testing of a variety of induction heating applications.

(source: the Wall Street Transcript)

“Customers turn to THE LAB at Ambrell to explore the precision induction heating solutions required to solve their unique heating challenges,” said Jim Pelrin, President and CEO of inTEST. “Our applications laboratory expansion project in Hengelo and California embodies the partnership, collaboration and continued commitment to strengthen the support we provide to our global customer base.”

Scott Nolen, Ambrell’s Vice President and General Manager, added, “Under the direction of Dr. Girish Dahake in the United States and Frank Kuster in Europe, THE LAB at Ambrell now offers an expanded geographical reach and provides state-of-the-art laboratory equipment to deliver innovative and effective heating solutions for the most challenging applications. As a leader in the industry, we’re very excited to announce these important, value-added capabilities to existing and prospective customers worldwide.”

 

inTEST’s Induction Heating Lab Expands To the West Coast Read More »

Heat Treat Radio #28: Heat Treat Modeling With Justin Sims

Welcome to another episode of Heat Treat Radio, a periodic podcast where Heat Treat Radio host, Doug Glenn, discusses cutting-edge topics with industry-leading personalities. Below, you can either listen to the podcast by clicking on the audio play button, or you can read an edited version of the transcript. To see a complete list of other Heat Treat Radio episodes, click here.


Audio: Heat Treat Modeling With Justin Sims

In this conversation, Heat Treat Radio host, Doug Glenn, interviews Justin Sims of DANTE Solutions about heat treat modeling. As the heat treat world moves farther way from mysterious black box processes, find out how the latest advances in heat treat simulation software can help your company model specific processes and materials in advance, leading to less guesswork and more profit.

Click the play button below to listen.


Transcript: Heat Treat Modeling With Justin Sims

The following transcript has been edited for your reading enjoyment.

We're going to talk to Justin Sims, lead engineer at DANTE Solutions, Inc., about heat treat modeling.  It's a pretty interesting topic.  With all the advances and sensors and computing power, the heat treat world is moving further and further away from the mysterious black box processes of yesteryear and is allowing companies to model specific processes and specific materials in advance so that there is less guesswork and more profit.  DANTE provides the means by which companies can accurately predict what is going to happen to their part during the heat treat process.

DG: Justin is not only the lead engineer at DANTE Solutions, he is also the author of an article that just appeared in the March 2020 issue of Heat Treat Today and the title of the article was Process Innovation To Reduce Distortion During Gas Quenching. It was a pretty interesting article, something worth reading if you haven't already.  It has to do with DANTE controlled gas quench.

JS:  I got my bachelors in mechanical engineering degree from Cleveland State.  I graduated back in 2015.  I actually started interning at DANTE in 2014 and went full-time in 2016.  I've been the lead/principal engineer at DANTE with mainly responsibilities of managing projects, training our DANTE users, and offering support to our DANTE users.  I helped develop our patent-pending DANTE controlled gas quenching process, which you had just mentioned, and then also a little bit of IT, marketing, sales, and shipping. Being a smaller company, we can kind of do it all.

 

Fig. 1: Bevel gear axial distortion comparison for an oil quench, high pressure gas quench, and a DANTE Controlled Gas Quench

 

DG: Tell us briefly about DANTE.

JS: DANTE Solutions is an engineering consulting and software company.  We offer consulting services as well as licensing our software.  We mainly focus on the aerospace industry, the auto industry quite a bit as well, and we've been starting to get into the mining and energy sectors also.  As I said, we are a smaller company.  There are six of us right now. Two to three guys mainly focus on the software side, and the rest of us focus on more of the training, the support, and the consulting side of the business.

DG: DANTE is located near Cleveland, OH, and Lynn Ferguson, who has been in the heat treat industry for many, many years, was one of the founders. Let's talk about the genesis of the software. Would you say the software is the core product that DANTE Solutions offers?

JS: Yes, it is. We mainly stay in consulting to stay current and to give those users who don't have the capability to run our software (either they don't have the hardware or they don't have the analysts to be able to do such a thing), so we still offer our consulting services for them. But mainly, software is our main line of business.  DANTE was actually formed back in 1982 as Deformation Control Technology, Inc., and we changed our name in 2014 to actually reflect more of the software side, so that's when we changed to DANTE Solutions, Inc.

The project itself that DANTE came out of actually started in 1994 and 1995.  It was a collaboration between Ford, GM, Eaton Corp. and then four national labs--I believe they were Los Alamos, Sandia, Oak Ridge, and Lawrence Livermore--and then us as Deformation Control Technology.  The whole project came out because those large automakers were claiming millions of dollars of lost scrap from distortion.  It was starting to become a major issue and they wanted a way to be able to model the process and be able to optimize the process a little bit better.  After that project ended, DANTE somehow ended up with the software, which has worked out well, as we've been able to commercialize it and we've been updating all the material models and the material database for the last 20 years.  It's actually come quite a long way.

DG:  How did you segue over from auto industry into aerospace?

JS:  It just happens that the aerospace components cost a whole lot more than the auto industry components.  It was a natural fit once they realized that this software was viable and could do what they needed it to do.  And aerospace seems to be more receptive to modeling because their parts are so expensive.

DG:  Let's try to put a little flesh on the bones here. For a manufacturer who has their own in-house heat treat for aerospace, automotive, energy or whatever, what makes this software attractive?  What makes it viable?  Why would someone want it, and why and how do they use it?

JS:  Let's start with viability.  The first thing is that it is easy to use.  DANTE is a set of material routines that link with Abaqus or Ansys finite element solvers.  These are solvers that engineers and analysts in the industry already know pretty well, so there is not a lot of learning of new software.  DANTE is just a material model, so all you're really responsible for is the material name and what microstructural phases you're starting with.  Then we have the ability to modify a few of our control parameters, activating different models; we've introduced stress relaxation, carbon separation, carbide dissolution, and all these different models that you can activate.  But the biggest thing that trips people up . . . [is] understanding your process.  We like to work with people a lot on trying to help them understand what type of thermal behavior their processes are actually imparting on components.  We've done a lot of work with setting up their essentially quench probes and be able to turn around and be able to take that back to heat transfer coefficients that get put into the model. As far as DANTE is concerned, it is fairly easy to use.

We've also developed what they're calling ACT (Ansys Customization Toolkit).  It is essentially a series of buttons where you would click on these buttons, fill out information, and then essentially run your models. Abaqus, for the new version of DANTE, we've also developed a plug-in that essentially does the same thing.  So DANTE has become very point-and-click.  In this world, I think people like that simplicity.

Fig. 2: Axial distortion of a press quenched bevel gear

The next big one would be the accuracy that everybody is concerned about.  Our accuracy is due to the models that we use and the algorithms that we employ.  There are two types of accuracy.  I've touched on the boundary condition accuracy, and that is how your process behaves thermally.  That accuracy can be tough to get.  It's very doable and we've helped people achieve some really amazing accuracy.  The relationship I like to use here is people know static loading models and a lot of engineers have run static loading models.  The loads that you put on these static models are going to determine what deflections you get.  If your load is not correct, then your deflection will not be correct.  In heat treat modeling, the thermal boundary condition is your load.  The more accurate your heat transfer coefficient can be, the more accurate your results are.  But, with that being said, you can still gain a lot of valuable information from being close enough.  We'll talk a little bit about that with the uses and whatnot.

The first important model type that we use is the mechanical model.  We use a multiphase internal state variable model.  A conventional plasticity model considers stress as a function of strain only, where the internal state variable model actually accounts for the history of deformation by relating the stress to dislocation density.  It actually accounts for the history of deformation, which is very important as the steel goes through all the stress reversals that it does going through the process.  Our mechanical model defines each phase, so austinite, pearlite, ferrite, bainites martensite, tempered martensite, all of them, as a function of carbon, temperature, strain and strain rate.  It also accounts for the trip phenomenon.

For our phase transformation model, we like to use analytical models instead of TTT CCT diagrams, and we do this because you don't get any transformation strain information out of the diagram.  So you have no idea how much it is deforming.  In order to figure that out, we like to use dilatometry tests to fit to our analytical models.  We also account for carbide growth and dissolution during carburizing, which is becoming a major point of interest due to the high alloy content of some of these steels that they're now trying to carburize.

DG:  Let's talk a bit more about where manufacturers, who have their own in-house heat treat, might use DANTE's software tool.

JS:  One of the big things we like to use it for is what we call sensitivity analysis.  This would be, "what happens if my normal process has a little bit of variation?"  Or, "what happens if my process parameters change a little bit?" We've also worked into the model now normal material variation.  So if your alloy content is a little on the high side, how would the material behave?  If it's a little on the low side, how will it behave? [This] is a big deal.  One example would be, "I just designed a new part and I want to make sure that it behaves given the range that I know my process can vary."  All processes will vary.  This is no way to make the process exactly the same every time.  Also, in the sensitivity, you can ask the question, “What process variable is a distortion or stress most sensitive to?"  By finding out what process variables cause the most sensitivity, then those are the process variables you really need to pay attention to during processing, then the other ones you can just make sure they're in range and leave them alone.

Development and design are two of the big ones that we're trying to get out there that this software can be used for.  Everybody knows that it can be used for troubleshooting.  Once something goes wrong, yes, sure the software is great and we help figure out a problem; but why not find the problem before it ever even happens?  We've been trying to get people to use it for development of new carburizing and nitriding schedules as well as new recipe and design, and even novel processes.  You had mentioned our DANTE controlled gas quench.  That actually was conceived through all the modeling that we do and watching the response of the material and saying, “Wait a second.  If we can control the martensite transformation rate, we can really control the distortion, so let's see if we can do this.”  Things like that can come out of the software.  Design as well, of optimizing shapes for quench.  You can even do quench to fit, which is, "I know my part distorts this much, so let me machine it distorted and then it will fall into shape."  Optimizing processes.  All of that can be done through design development, and you can find these problems before they ever happen.

Another really big one that I like, and Lynn, our owner, is really keen on this one, is the understanding of your process.  When you start to set up these models, you have to ask a lot of questions about your process.  What is the HTC of my process, which relates back to agitation in the tanks, part racking, flow directions?  You really need to know times and temperatures of every step in your process.  So not just the heat to quench, but what about all those transfers in between?  All of that needs to be done.  So you end up asking a lot of questions like that.

The other one that I always like to say is that the heat treat software removes the black box.  In the past, you know what goes in and you know what comes out, but what happens in the middle is kind of a mystery.  The software helps you figure out what exactly goes on during your process.  It can be very eye-opening.

Fig. 3: Minimum Principal stress of a carburized and oil quenched spur gear

DG:  I've talked with James Jan and Andrew Martin over at AVL, and we talked about a variety of ways they use some of their software, and they mentioned that they work with you guys as well, and they were talking about not even just like a quench agitation, flow direction, and things of that sort, but part orientation as it goes into a quench.  I assume that would be something also that you guys would be able to help analyze, right?  Which way to even put the part into the quench?

JS:  Sure, sure.  And we've done that.  The one that comes to mind is a long landing gear.  This landing gear was about 3 meters in length, and we looked at even slight angles going into the quench tank can have serious consequences on the distortion.  That is definitely something that we've looked at in the past.

DG:  Just that orientation would help, but maybe eliminate vapor stage, or whatever, I assume?  Or pockets?

JS:  Right. And even beyond that, it sets up thermal gradients in different locations of the part.  So now instead of cooling one section faster, you're cooling it a little slower and that kind of thing.  That also relates back to actual vapor stages and how bubbles get trapped.  But that goes back to defining boundary conditions, which is where software like AVL's FIRE can really be helpful in understanding flow patterns.  There is a beneficial relationship there.

DG:  There are a host of different materials that people are using.  How broad is the database, as far as the different types of materials, that you can analyze and model?

JS:  That is a good question.  We have a lot of low alloy, medium alloy, and carburizing grades of steel, the 1000 series, the 8600 series, 9300 series, those types of materials.  We've also worked with some of the high alloy aerospace grades like C64 and the Pyrowear 53 and that sort of thing.  But right now, it's all steel.  There is a lot of talk about being able to do aluminum.  We get that question a lot.

DG:  I was wondering about that specifically- aluminum and/or of course, when we talk aerospace, we're talking titanium.  So titanium is not on the table at the moment?

JS:  It is, but it isn't.  The interesting thing is that there is a phenomena precipitation hardening that goes on in aluminum and titanium.  But it also goes on in these high alloy steels.  It is a secondary hardening mechanism.  We've been working on that and we feel that once we can handle secondary hardening in steel, then the jump to aluminum and titanium should be pretty straightforward.

DG:  So to recap, for those of us who are not as well-versed in the product as you are, basically you've got a simulation software that takes into account the material that is being used, also the thermal process (the recipe), which would include both a controlled heat up and potentially a controlled quench.  Is that a reasonable way to describe it in a very broad way?

JS:  Yes. And also, even the steps before that, like carburizing.  If the part is carburized, you would carburize it first.  Or nitriding; we've just introduced those models.  You can literally do the entire process.  And it's not just quenching either.  We've done martempering, austempering, normalizing, all of these things.  Most all normal thermal processing, DANTE can handle.

DG:  The last question I want to ask is, Who is the ideal person/company that would really find the product/service that you're providing useful? I know you mentioned aerospace and automotive, but can we be more specific than that? Where are you finding the most success?

Fig. 4: Displacement versus temperature curves showing the shift in martensite start temperature for 3 carbon levels

JS:  That's a tough question. Generally, everybody that has used our software has found real benefit in it.  We've tried to get testimonials from a lot of folks, but this can be difficult because of their companies.  But from Cummins, we've gotten good responses and also from GM we've gotten good responses.  One of them has used it to actually introduce new material and replace legacy material that is now saving them quite a bit of money.  GM has used it to look at process design and optimization.  But I would say mainly the people that are going to benefit the most are the folks that have an analyst to be able to do the simulation almost on a daily basis.  It's one of those things where the more you do, the more you see and the more you understand what is happening.  But really anybody that does heat treatment can benefit from understanding what's going on in their process.

DG:  You mentioned Cummins, and I'm looking at your website, and I just want to read a paragraph:

DANTE heat treat simulation software has been a great boon to Cummins.  Since we've started using their software, we have gone through several projects that have increased our understanding of heat treatment and some of which have saved us production costs.  One example was enabling us to gain the leverage needed to make a material and process change on a legacy product that is now saving us at least 25% on material costs.  The team at DANTE Solutions has always been very accommodating and is very quick to give assistance and feedback whenever troubles arise, even when the troubles are caused by other parts of the simulation and not DANTE itself.  I look forward to working with DANTE team in the coming years as we expand our list of engineers who use this software. -- Brian W. at Cummins

So that leads me to one other question.  When a person interacts with you, are they buying software as a service?  Is it cloud-based or is it something that they purchase a license for one computer, one user?  How does it work?

JS:  There are a couple of different ways.  They can lease it annually or they can essentially buy the software and lease a license annually.  The software can go either on their computer or it can go on a server at their company.  We also have options for corporations where you can essentially get software at different locations.  We have a lot of options and we can work with customers if they [have] unique needs.  That's one of the benefits of being a smaller company, we're pretty flexible like that.

DG:  DANTE's mission statement from their website has a nice ring to it: “DANTE Solutions is determined to promote the use of simulation in the heat treat industry.  From design to troubleshooting, DANTE Solutions believes everyone can benefit from a little simulation in their life.”

If you'd like to get in touch with Justin Sims at DANTE, please email me, Doug Glenn, directly at doug@heattreattoday.com and I'll put you in touch with Justin.

Doug Glenn, Publisher, Heat Treat Today
Doug Glenn, Heat Treat Today publisher and Heat Treat Radio host.


To find other Heat Treat Radio episodes, go to www.heattreattoday.com/radio and look in the list of Heat Treat Radio episodes listed.

Heat Treat Radio #28: Heat Treat Modeling With Justin Sims Read More »

Heat Treat Tips: Induction Heating

One of the great benefits of a community of heat treaters is the opportunity to challenge old habits and look at new ways of doing things. Heat Treat Today’s 101 Heat Treat Tips is another opportunity to learn the tips, tricks, and hacks shared by some of the industry’s foremost experts.

For Heat Treat Today’s latest round of 101 Heat Treat Tipsclick here for the digital edition of the 2019 Heat Treat Today fall issue (also featuring the popular 40 Under 40).

Today’s tips come to us from Rob Medeira and Florie Grant of Inductoheat, covering Induction Heating. This includes advice about correcting irregular part distortion and finding solutions to cracked parts.

If you have a heat treat-related tip that would benefit your industry colleagues, you can submit your tip(s) to anastasia@heattreattoday.com  or editor@heattreattoday.com.


Heat Treat Tip #13

Correcting Irregular Part Distortion

(source: Inductoheat)

Situation: Part is distorting irregularly after induction heat processing
Solution:
1. Check quench concentration, flow, & pressure.
2. Make sure there is proper quench uniformity.
3. Check TIR of the spindles and part holding fixtures
4. Check to ensure the part dimensions are accurate & center drills are on center.
5. Check part nest clearance when the part is cold.
6. Check to make sure the heating time is not too long.

HINTS:
· Check the part holding fixtures and spindles to ensure proper positioning.
· Some processes use a negative quench delay, quench on before heating stops, typically 0.05-0.3 seconds to improve TIR of the part.
· The part nest should not fit snug when the part is col – it will grow during the heating & warp the part.
· If the spline area has distortion or the “Go” gage is tight, try a quench delay of 0.2 to 0.4 seconds.


Heat Treat Tip #14

Cracked Parts?

(source: Inductoheat)

Situation : Cracked Parts
Solution:
1. Check parts positioning.
2. Make sure there are no unexpected hot spots; lack of rotation may be the cause.
3. Check for excessive grain growth around the crack surface area.
4. Check if quench condition is out of spec.
5. Check surface finish of part prior to hardening.
6. Apply temper ASAP.
7. Confirm & inspect steel conditions.

HINTS:
· If the part has excessive grain growth, that may lead to cracking.
· If cracking appears around hole area, then the proper chamfering might help.
· Parts out of higher carbon steels (0.55%C or higher) use higher quenching concentration & avoid surface overheating.


 

Heat Treat Tips: Induction Heating Read More »

West Coast Aerospace Company Purchases Custom Batch Tempering Furnace

A commercial heat treating company located in the heart of the aerospace industry on the West Coast of the United States recently commissioned a custom built batch tempering furnace. With a working load size of 168” wide, 48” deep, and 48” tall, coupled with a max load weight of 10,000 pounds, the furnace from Gasbarre Thermal Processing Systems can accommodate a number of differently sized parts within its market.

The gas fired air furnace passes survey at +/- 10℉ over a temperature range of 850℉ to 1350℉ per AMS2750E. At the customer’s request, the electrical controls are UL approved and include the latest in Eurotherm brand temperature controlling instrumentation.

(source: Gasbarre Thermal Processing Solutions)

(Image source: John Torcasio, unsplash.com)

West Coast Aerospace Company Purchases Custom Batch Tempering Furnace Read More »

Aerospace Standards in the Heat Treating Industry

Have you ever wondered how to create or revise AMS specifications? In this original Heat Treat Today Technical Tuesday feature, come along with Andrew Bassett, president of Aerospace Testing and Pyrometry and an expert in aerospace pyrometry specifications, as he shares his experience and knowledge in the process.

Andrew Bassett, President, Aerospace Testing and Pyrometry

Author’s Note: These comments are the non-binding opinion of the author and do not constitute an interpretation by SAE. Such opinions do not replace the need to ensure agreement between the supplier, customer, and cognizant engineering organization.

This article originally appeared in Heat Treat Today’s  March 2020 Aerospace print edition.


Those who are familiar with aerospace heat treating are accustomed to Aerospace Material Specifications (AMS) that guide heat treaters on how to process parts and raw materials. These specifications will mandate equipment requirements, atmospheres to be used, cleaning methods, soaking times and temperatures, and testing requirements, to name a few. The working committee, Aerospace Metals Engineering Committee (AMEC), is in charge of revising these specifications, which is required every five years. This is a long and sometimes tedious process of revising specifications with many knowledgeable experts involved.

There are various types of specifications that have been established by the SAE Technical Standards Board:

  1. Aerospace Material Specifications (AMS)
    • These technical reports contain specific performance requirements and are used for material and process specifications conforming to sound established engineering and metallurgical practices in aerospace sciences and practices.
  2. Aerospace Standards (AS)
    • These technical reports contain specific performance requirements and are used for design standards, parts standards, minimum performance standards, quality, and other areas conforming to broadly accepted engineering practices or specifications for a material, product, process, procedure, or test method.
  3. Aerospace Recommended Practice (ARP)
    • These aerospace technical reports are documentations of practice, procedures, and technology that are intended as guides to standard engineering practices. Their content may be more general in nature, or they may offer data that has not yet gained broad acceptance.
  4. Aerospace Information Report (AIR)
    • These aerospace technical reports are compilations of engineering reference data, historical information, or educational material useful to the technical community.

To create or revise an Aerospace Specification, a “sponsor” of the specification will request to either create a new or revise an existing standard with the approval of the chairperson. Once the approval has been granted, the sponsor will work to create and/or revise the existing document. When the draft document is complete, the draft is balloted for a 28 Day Ballot. Members of AMEC can make comments on the ballot with either a “T” comment or an “I” comment. The “T” comment is a technical error, missing requirement, or improper requirement that needs action by the committee. All technical comments should be accompanied by a reason for the comment and a suggested improvement to resolve the issue. The “I” comment is a non-technical correction. These may include spelling and grammatical mistakes, incorrect paragraph numbering, and the like. Each “T” comment must be discussed and voted on by the committee members and approved or disapproved. During the ballot process, members are asked to “Approve” or “Disapprove” the ballot. This process goes on until no more changes are required to the draft before the document is sent to the appropriate commodity committees.

The illustration (Figure 1) describes the creation/revision process for given specifications.

 

(Click on image to enlarge)

Figure 1. Ballot Process Flowchart from SAE

 

The projects for the revisions to AMS-2759 series of specifications started in 2009/2010 with many of the draft revisions waiting in “parking lots” until all the specifications were completed. Since their release in 2018, several of these specifications had to be revised again due to missing or omitted requirements or small changes to clarify issues.

Over the last eighteen months, the heat treat industry has experienced new revisions to the following specifications (revision dates):

  1. AMS-2759 Rev G Heat Treatment of Steel Parts General Requirements (04-23-19)
  2. AMS-2759/1 Rev H Heat Treatment of Carbon and Low Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517MPa) (09-19-19)
  3. AMS-2759/2 Rev J Heat Treatment of Low Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517MPa) and Higher (07-15-19)
  4. AMS-2759/3 Rev H Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging and Secondary Hardening Steel Parts (01/07/19)
  5. AMS-2759/4 Rev D Heat Treatment Austenitic Corrosion-Resistant Steel Parts (04-28-18)
  6. AMS-2759/5 Rev E Heat Treatment Martensitic Corrosion-Resistant Steel Parts (04-28-18)
  7. AMS-2759/6 Rev C Gas Nitriding of Low Alloy Steel Parts (06-11-18)
  8. AMS-2759/7 Rev D Carburizing and Heat Treatment of Carburizing Grade Steel Parts (04-15-19)
  9. AMS-2759/8 Rev B Ion Nitriding (06-11-18)
  10. AMS-2759/9 Rev E Hydrogen Embrittlement Relief (Baking) of Steel Parts (10-18-18)
  11. AMS-2759/10 Rev B Automated Gaseous Nitriding Controlled by Nitriding Potential (06-11-18)
  12. AMS-2759/11 Rev A Stress Relief of Steel Parts (04-28-18)
  13. AMS-2759/12 Rev B Automated Gaseous Nitrocarburizing Controlled by Potentials (07-02-18)
  14. AMS-2759/13 Gaseous Nitrocarburizing (06-11-18)
  15. AMS-2769 Rev C Heat Treatment of Parts in Vacuum (07-12-19)
  16. AMS-2770 Rev P Heat Treatment of Wrought Aluminum Alloy Parts (04-08-19)
  17. ARP-1962 Rev B Training and Approval of Heat Treating Personnel (06-11-19)
  18. ARP-7446 Vacuum Gauge Calibration (03-06-19) New ARP

There are several more projects underway that include the revision of AMS-H-6875, Heat Treatment of Steel Raw Materials that will become a four-digit AMS Specification, AMS-2774, Heat Treatment Wrought Nickel Alloy and Cobalt Alloy Parts, AMS-2801, Heat Treatment of Titanium Alloy Parts and AMS-2750, Pyrometry, to name a few. As new technology emerges, such as additive manufactured metal parts, AMS standards will need to be revised or created to address the thermal processing of these parts.

AMS-2750 (Pyrometry) is one of the more contentious specifications, which is currently under revision, because it is the main specification for the testing of thermal processing equipment. This specification not only has an effect on commercial heat treaters working in aerospace, but this specification has been adopted in chemical processing/coatings for baking/drying ovens, composites for curing and bonding laminates, and as of January 28, 2018, the FDA Center for Devices and Radiological Health has added this standard to its list of recognized consensus standards database. For those who are heat treating medical devices such as needles, heart wires, titanium staples, and metallic joint replacements, AMS-2750 is now governing how the thermal processing equipment will be tested.

When I first became involved with AMEC in June 2008, the AMS-2750D (Pyrometry) was starting to be revised to AMS-2750E. I attended my first meeting in Niagara Falls, New York, with the expectation that I would be working only with a group of aerospace primes who write these standards. As it turned out, many of the members at AMEC are end users, such as captive and commercial heat treaters who are experts in the specifications in which they are involved. Since being in the field of pyrometry, I thought I would volunteer my time and expertise on the revision of AMS-2750. The sub-team group consisted of experts from Boeing, Honeywell, Carpenter Technology, Alcoa, Performance Review Institute (PRI), and Bodycote Thermal Processing with each team member bringing to the table his/her own knowledge and expertise in pyrometry. The process of revising this specification took four years to complete with numerous team meetings to discuss and propose changes to better clarify the previous revision. The final revision was finally published in July of 2012. Since then, I have been involved with other specifications such as AMS-2769 (Heat Treatment of Parts in a Vacuum), ARP-7446 (Vacuum Gauge Calibration), and the next revision of AMS-2750F.

Getting involved with AMEC and the various commodity groups is rewarding as it allows you to have a voice in the specifications that affect your business. You work with other members in the heat treat community to develop and create specification to enhance the industry, better the process, and continually strive to deliver quality parts or materials.

About the Author: Andrew Bassett is the president of Aerospace Testing and Pyrometry and is an expert in aerospace pyrometry specifications. He has 25 years of experience in the calibration and testing of thermal processing equipment. This article originally appeared in Heat Treat Today’s  March 2020 Aerospace print edition.

 

(source: Stefan Fluck on Unsplash)

Aerospace Standards in the Heat Treating Industry Read More »

Choosing the Right Vacuum Furnace

Source: TAV, the Vacuum Furnaces Blog

It pays to carefully consider the key factors to buying a vacuum furnace (source: TAV, the Vacuum Furnaces Blog)

When and why is it a good idea to purchase a vacuum furnace? Does your company really need one? A company that wants to play its cards best, in terms of investment and yield, knows about the advantages offered by vacuum heat treatments in both the short and long term. But choosing the ideal furnace best suited to your company’s needs isn’t as easy as it might appear.

In this Heat Treat Today Best of the Web feature, TAV Vacuum Furnaces gives readers a handy guide over at its blog to consider the crucial factors in choosing a vacuum furnace for your company, including tips on who needs a vacuum oven, why comparing two or more systems is a bad idea, and the role of the heat exchanger, vessel performance, and the pumping unit.

An excerpt: “There are many fields, ranging from the vacuum sintering of metal powders or ceramics to the vacuum brazing of aluminum alloys to continue with high temperature brazing, in which technological avant-garde stands out. In these sectors, the decision to use a vacuum furnace is linked to the possibility of implementing an advanced development production process, for which the focus was on high-yield plants.”

Read more: “Do I Really Need a Vacuum Furnace?”

 

Choosing the Right Vacuum Furnace Read More »

Happy Easter from Heat Treat Today!

Heat Treat Today wants to wish everyone a happy Easter weekend! At this time of the year, and especially during this uncertain season, we celebrate the life and work of our Savior, Jesus Christ, with confident hope and joy. In times of darkness, we are blessed to have a light that never goes out as we look back on Jesus’ victory over death and look forward to His coming. May you all have a safe and blessed holiday!

(source: Brooke Lark on Unsplash)

Happy Easter from Heat Treat Today! Read More »

16 Quick Heat Treat News Chatter Items to Keep You Current

Heat Treat Today offers News Chatter, a feature highlighting representative moves, transactions, and kudos from around the industry.

Personnel & Company Chatter

  • Bill Gornicki was recently appointed Director of Sales at ECM-USA, Inc. in Pleasant Prairie, WI.
  • AFC-Holcroft, in Wixom, MI, recently moved its European satellite office from Delémont, Switzerland, to Swiebodzin, Poland, as necessitated by the retirement of their Director of European Operations. The new director, Marek Kedzierzynski, will be based out of Poland.
  • Wire Experts Group, the parent company to Pelican Wire and Rubadue Wire, recently announced the newest members of their leadership team and their respective roles: Brinson White will now lead the Engineering & Maintenance teams at both Pelican and Rubadue as WEG Director of Engineering; Mike Skorupa has been named Director of Continuous Improvement across all business units; and Kevin Clements has been named Global Supply Chain Manager. 
  • RETECH Systems, LLC, a SECO/WARWICK Group company, has finalized plans to relocate its headquarters from Ukiah, CA, to Buffalo, NY.
  • Charlie Li, of DANTE Solutions, began teaching a new master-level Mechanical Engineering class entitled “Advanced Manufacturing Processes: Heat Treatment of Steels” at Cleveland State University.

  • Solar Atmospheres has purchased two microscopes, one a ZEISS AxioVert A1 Inverted Materials Microscope and the other a a Hitachi smart Scanning Electron Microscope, to enable them to better serve the needs of their customers.
  • Magnetic Specialties, Inc. recently shipped two 510KVA, three phase step down 6-pulse rectifier transformers and DC inductors for use in industrial rectifier applications.
  • The Grieve Corporation recently installed their new electrically-heated 2000°F inert atmosphere heavy-duty box furnace to be used for heat treating titanium at a customer’s facility.
  • Gasbarre Thermal Processing Systems recently commissioned a model CVPQ Continuous Vacuum Furnace with 5 BAR pressure quench capabilities, and a precision gas nitriding and ferritic nitrocarburizing furnace, in the Midwestern United States.
  • Ipsen USA offers free evaluations of any brand of vacuum heat-treating system in the United States. An Ipsen Customer Service team member will check all major components of the furnace and provide a written health report with a suggested 18-month maintenance plan.
  • Tenova recently received the official notice to proceed with the new Hot Dip Galvanizing (HDG) line for NLMK Group in Lipetsk, Russia.
  • Pries Enterprises finished a 50,000 sq ft expansion and installation of a state-of-the-art anodizing line, making them the only vertically integrated extruder-anodizer fabricator in their immediate area.

  • Grupo Mess was recently named an exclusive Buehler distributor of metallographic and hardness equipment in Mexico.
  • Aerospace Testing & Pyrometry recently announced the opening of their newest regional office in Greenville, SC. The territory will include North Carolina, South Carolina, Virginia, Georgia, Tennessee and Alabama.
  • Constellium SE was recently recognized with the “Best Performer Award” by Airbus.
  • Advanced Heat Treat Corp. recently announced that it has added gas nitriding to its Nadcap® accreditation.

Grupo Mess


Heat Treat Today is pleased to join in the announcements of growth and achievement throughout the industry by highlighting them here on our News Chatter page. Please send any information you feel may be of interest to manufacturers with in-house heat treat departments especially in the aerospace, automotive, medical, and energy sectors to editor@heattreattoday.com

16 Quick Heat Treat News Chatter Items to Keep You Current Read More »

Thermal Processing Manufacturer Helps Sterilize PPE Masks

A global manufacturer of thermal-processing and sterilizing equipment announced they are working with hospitals to prove the efficacy of their Gruenberg product line for dry heat sterilization on PPE and N95 masks for re-use.

Picture 1: Gruenberg Tabletop Sterilizer (source: Thermal Processing Solutions)

Recent tests at a research hospital show positive results in the dry heat sterilization of masks, face shields, gowns and other PPE, with minimal deterioration of the material. During the process, Thermal Product Solutions, LLC (TPS) heated masks to a specified temperature for a calculated period of time that resulted in sterilization of the material. After the sterilization process, fit tests were performed on the masks that passed filtration efficacy, structural integrity, and mask fit. TPS is continuing to work with facilities to further confirm test results.

Greg Jennings, president and CEO, Thermal Product Systems

“We are dedicated to finding methods that aid in protecting the health and safety of all those serving on the front lines during the COVID-19 pandemic,” said president and CEO Greg Jennings. “Our dry heat sterilizers have been used for decades in the decontamination and sterilization of all forms of microbial life and it only made sense to begin testing their efficacy on sterilizing PPE for hospitals and emergency personnel. We are looking to find additional testing partners quickly and ultimately receive FDA approval to help fight the COVID-19 spread.”

Picture 2: Gruenberg Truck- In Sterilizer (source: Thermal Product Solutions)

The Gruenberg sterilizers utilize convection airflow and dry heat for the process. Heat is absorbed by the item being sterilized for a period of time until it reaches the proper temperature needed to destroy microorganisms and achieve sterilization. Dry heat sterilizers range in size from small tabletop models (Picture 1) starting at 1.25 cubic feet (cf) to large truck-in models (Picture 2) offering 1,000cf of sterilization capacity.

Gruenberg’s smaller dry heat sterilizers feature a unique design where the process chamber is sealed throughout the entire cycle, containing any airborne particulates and sterilizing them.  Larger chamber systems are easily customized and feature intake and exhaust HEPA filters and several door seal options.

Thermal Processing Manufacturer Helps Sterilize PPE Masks Read More »