AUTOMOTIVE HEAT TREAT NEWS

Wrocław University of Science and Technology Enhances Metallurgy Research Capabilities with Nitriding System

Wrocław University of Science and Technology (WUST) is expanding its R&D capabilities in heat treatment and materials testing with a horizontal nitriding system. The furnace will support the university’s efforts in metallurgical research and collaborations with regional manufacturing industries, including testing forging dies for the automotive industry.

Marcin Stokłosa
Technical Sales Manager
NITREX Poland

The newly acquired Nitrex system is equipped with Nitreg® controlled nitriding technology for optimizing surface hardness, and Nitreg®-S technology for nitriding stainless steel. The system enables Poland-based WUST to conduct next-level materials research and leverage new technological and scientific capabilities to support industrial projects, optimizing heat treatment processes and enhancing the surface properties of metal parts. Furthermore, the furnace meets the stringent AMS 2759/10 standard for nitriding steel and AMS 2750 standard for temperature uniformity.

“While Nitrex primarily serves businesses in sectors such as automotive, aerospace, and manufacturing,” said Marcin Stoklosa, technical sales manager – EMEA region at Nitrex Poland, “our partnership with WUST underscores our commitment to advancing academic research and fostering innovations that directly benefit practical applications and advance metallurgical science globally. . . . I look forward to seeing WUST’s continued leadership in metallurgical research and its impact on both academia and industry.”

The press release is available in its original form here.



Wrocław University of Science and Technology Enhances Metallurgy Research Capabilities with Nitriding System Read More »

Cincinnati Radiator Bolsters Aluminum Brazing Capabilities with New VAB Furnace

Cincinnati Radiator, a manufacturer of radiators and cooling products, recently expanded its production capabilities at its Fairfield, Ohio, facility with the addition of a vacuum aluminum brazing (VAB) furnace. This acquisition will enable the company to perform in-house radiator core brazing.

The VAB furnace, with a weight capacity of up to 2,000 lbs, is the third manufactured and installed by Ipsen.

Prasenjit Ray
General Manager
Cincinnati Radiator
Source: Ipsen

“This furnace has so many recipes for us to use,” said Prasenjit Ray, general manager of Cincinnati Radiator. “We were planning to test it out for two months, but we weren’t expecting to get production-quality within those two months. What shocked and surprised me was that the first cores that came out were perfect. We’ve produced 10 (in the first month) and it runs like a new Cadillac.”

“We knew that we needed a way to make cores here. When customers had to rely on cores processed in China, it could mean a four-month lead time. If we had our own furnace, we could operate a just-in-time production,” said Ray. “We went with John Pease (Ipsen Regional Sales Representative) and Patrick McKenna (Ipsen USA President & CEO) to California to see a company operating two Ipsen VAB furnaces. Our team knew that, once we saw them in operation, we wanted to work with another company within the United States. Ipsen could offer great aftermarket support, and the delivery was worth the wait.”

Main image (left to right): All of Cincinnati Radiator: Abhilash Uppala, Manufacturing Engineer; Prasenjit Ray, General Manager; Michael Petitt, Assistant Operations Manager; and James “Tom” Aynes, Accounting Manager. Source: Ipsen.

The press release is available in its original form here.



Cincinnati Radiator Bolsters Aluminum Brazing Capabilities with New VAB Furnace Read More »

Automotive Radiator Manufacturer Bolsters Aluminum Brazing Capacity

A car radiator manufacturer has expanded its heat treatment capacity with an EV/CAB line adapted for the production of oversized battery coolers. The aluminum brazing furnace facilitates the ability to make quick modifications and switch from gas to electric heating in order to meet climate change challenges.

Piotr Skarbiński
Vice President of Aluminum and CAB Products Segment
SECO/WARWICK
Source: LinkedIn

SECO/WARWICK designed the CAB line with temperature uniformity across the entire belt width in order to accommodate the size specifications of the battery coolers.

“This order is for an aluminum brazing furnace adapted to the production of oversized battery coolers,” said Piotr Skarbiński, vice president of the aluminum and CAB product segment at SECO/WARWICK. “The EV/CAB line with a belt width of 2100 mm (6.89 ft) is designed to produce oversized battery coolers. It consists of a preheating and main heating chamber, a radiation brazing furnace, an air jacket cooling chamber, a final cooling chamber and a control system.”

The press release is available in its original form here.



Automotive Radiator Manufacturer Bolsters Aluminum Brazing Capacity Read More »

Automotive Component Manufacturer Bolsters Heat Treat Operations

An automotive component supplier has digitized its heat treatment operations with the implementation of a digitalization platform, an upgrade intended to align the company’s operations with the accuracy and precision requirements of the global automotive market.

Daniel Gonschorek
Sales Manager
UPC-Marathon Technical
Source: LinkedIn

With this upgrade, the manufacturer has transitioned from using multiple systems to manage its heat treatment processes, streamlining furnace operations with the QMULUS digitalization platform from UPC-Marathon, a Nitrex company.

“Our collaboration with this tier 1/2 supplier has yielded significant improvements in their operational workflows,” said Daniel Gonschorek, technical sales manager at UPC-Marathon.

“The integration of QMULUS is not only advancing their internal processes but also delivering tangible gains in efficiency and performance,” he added. “By enhancing production efficiencies and reducing waste, QMULUS supports their commitment to innovation and aligns with the highest quality and sustainability standards. This digital transformation positions them strongly within the competitive automotive supply chain.”

The press release is available in its original form here.



Automotive Component Manufacturer Bolsters Heat Treat Operations Read More »

Automotive Parts Supplier Acquires Vacuum Furnace To Conduct Aluminum Brazing Tests

An automotive supplier has acquired a vacuum furnace for brazing aluminum components. The VAB furnace was designed according to the client’s guidelines and will be used by the R&D department to conduct development tests in the field of aluminum vacuum brazing.

SECO/WARWICK previously provided vacuum technology systems to the automotive parts manufacturer and built the VAB furnace based on the design of a single-chamber VECTOR furnace.

Maciej Korecki
Vice President of Vacuum Business Segment
SECO/WARWICK
Source: SECO/WARWICK.com

“Orders requiring a specific approach always make us happy, because it builds, inspires, and develops both our body of knowledge and the technology. This project was certainly a challenge for the entire SECO/WARWICK Team, because the partner’s assumptions, in relation to the requirements placed on our furnace, were really high,” said Maciej Korecki, vice president of the vacuum furnace segment at SECO/WARWICK. “They required a very complicated and individual solution in the form of a cuboid shape of the heating chamber equipped with flat, large-surface heating elements. They were arranged in twelve independent temperature control zones, ensuring very high dynamics of load heating and ideal temperature uniformity.”

Lukasz Chwiałkowski
Sales Manager
SECO/WARWICK
Source: SECO/WARWICK

“We were tasked with creating a VAB furnace with unique solutions: a special square heating chamber equipped with flat heating elements made of Inconel 600 material, arranged in twelve independent temperature control zones” said Lukasz Chwiałkowski, sales manager at SECO/WARWICK.  

The press release is available in its original form here.



Automotive Parts Supplier Acquires Vacuum Furnace To Conduct Aluminum Brazing Tests Read More »

PAI Industries Bolsters Capabilities With In-House Carburizing Vacuum System

PAI Industries, a manufacturer of parts to the heavy-duty truck industry, has expanded its in-house heat treatment with a NANO vacuum furnace system.

The Georgia-based company partnered with vacuum furnace manufacturer ECM USA to transition its production line from out-sourced heat treatment to in-house vacuum technology in order to perform low pressure carburizing and through hardening around the clock.

The upgraded system will increase capacity and expedite production at PAI’s 112,000 square foot manufacturing facility. The NANO furnace system is comprised of one module with three stacked up heating cells (which can be extended to six heating cells, corresponding to two heating modules) and gas quenching cells to quench the parts. The carburizing cells are stacked up to reduce the footprint’s installation as much as possible. The furnace system integrates directly into the production line which allows it to reduce the cycle time while simplifying the flow between the machining and heat treatment.

The press release is available in its original form here.



PAI Industries Bolsters Capabilities With In-House Carburizing Vacuum System Read More »

2 Specialty Auto Components Manufacturers Expand Heat Treating Capabilities

Two different specialty automotive components manufacturers have expanded their heat treating processing lines in order to meet the growing needs of their clients. The new furnace equipment will replace existing systems and bolster oil quench hardening and salt quench austempering capabilities. 

CAN-ENG Furnaces International Ltd, based in Niagara Falls, ON, Canada, will supply mesh belt furnace systems, oil quench and salt quench systems, post quench wash systems, CAN-ENG PET™ SCADA system, and integrated controls. The automotive parts manufacturers chose designs that provide low energy consumption, reduced part mixing, reduce part damage and part distortion potential, and high uptime productivity.

The press release is available in its original form here.



2 Specialty Auto Components Manufacturers Expand Heat Treating Capabilities Read More »

Automotive Manufacturer Expands Brazing Capabilities with Vacuum Furnace

A U.S.-based automotive manufacturer is expanding its production capacity for brazing stainless heat exchangers with the order of a single-chamber vacuum furnace. The equipment will be integrated into an existing line’s thermal process operations, which is located at their Mexico facility.

Peter Zawistowski
Managing Director
SECO/VACUUM TECHNOLOGIES, USA
Source: SECO/WARWICK

The heat treater ordered the furnace from SECO/VACUUM specifically for immediate delivery, allowing brazing of automotive components to begin without delay.

“We built this furnace to be ready to be shipped and put into operation very quickly, which is just the solution they were looking for,” said Piotr Zawistowski, managing director of SECO/VACUUM.

The press release is available in its original form here.


Automotive Manufacturer Expands Brazing Capabilities with Vacuum Furnace Read More »

Two Manufacturers Expand Operations With Nitriding Systems

Nitriding systems have expanded the operations at two global companies: a gear manufacturer for the automotive industry and a fuel injection systems manufacturer for the marine machinery industry. In both cases, the systems will be integrated into existing installations in order to increase production capacity.

NXHL-910512 nitriding furnace
Source: Nitrex

A Chinese gear manufacturer has added a fourth Nitrex nitriding furnace to its automated gear production, which includes the manufacturing of transmission gears, transfer case gears, synchronizers, and engine-gear rings for both local automotive OEMs and global markets.

“This expansion goes beyond capacity enhancement; it elevates the manufacturer’s in-house capabilities and tightens production controls,” said Tao Liu, sales manager at Nitrex China. “It allows the company to focus resources on driving innovation and sustainability across domestic and international vehicle markets, including the growing new energy vehicle (NEV) sector.”

A third Nitrex nitriding system has been installed at a manufacturer specializing in high-performance fuel injection systems for diesel engines in maritime vessels. The new NX-815 batch furnace with a 3300 lb. (1,500 kg) load capacity is specifically tailored for processing carbon steel and stainless steel parts and meets stringent requirements of the shipbuilding and industrial marine industries.

“As environmental regulations propel the shift towards alternative energy-powered ships, our advanced nitriding technologies play a crucial role. We are proud to support their expansion into stainless steel applications,” said Tao Liu.

Press releases are available in their original form here and here.


Find Heat Treating Products And Services When You Search On Heat Treat Buyers Guide.Com


 

Two Manufacturers Expand Operations With Nitriding Systems Read More »

EV Chassis Production Expands With Retort Furnace

ev chassis production expands with retort furnace

An international manufacturer of electric vehicles (EVs) is adding an advanced retort pit furnace for the production of EV chassis. The equipment’s larger working space will allow for the nitriding of very large die elements needed to produce this automotive equipment.

Maciej Korecki
Vice President of Vacuum Business Segment
SECO/WARWICK
Source: SECO/WARWICK.com

“This is the fourth SECO/WARWICK furnace for this global manufacturer of electric vehicles. Our product solves the challenge of nitriding dies for the production of large-sized chassis, using a working space with a diameter of 1,600 mm and a height of 2,800 mm. We delivered a similar solution to this partner last year,” said Maciej Korecki, vice-president of the SECO/WARWICK Vacuum Segment. 

The equipment provided to the company has a compact design with vacuum purging, electric heating supported by an internal circulation fan, and an external cooling system. The retort and heating system’s special design as well as the gas installation ensures long and reliable operation in industrial conditions. The solution is based on a standard vertical VR retort furnace with an enlarged working space (Ø 1600 mm/63 in and 2800 mm/110.2 in effective height), which will allow the manufacturer to nitride the huge dies used for electric car chassis. 

The press release is available in its original form here.


Find Heat Treating Products And Services When You Search On Heat Treat Buyers Guide.Com