U.S. Steel has broke ground on a $1.9 billion direct reduced iron (DRI) production facility in Osceola, Arkansas, marking the next phase of a project that will connect iron ore production in Minnesota with electric arc furnace (EAF) steelmaking in Arkansas. The facility will supply hot DRI directly to EAF operations, strengthening the company’s domestic steelmaking capabilities.
U.S. Steel held the groundbreaking ceremony at its Big River Steel Works campus on October 30, 2026. Preliminary site preparation is underway, with construction expected to begin in late 2026. The investment is expected to create approximately 200 full-time jobs and an estimated 2,000 construction jobs at peak.
As previously reported in June 2026, the project is part of U.S. Steel’s investment in an integrated domestic steel supply chain, linking its Minnesota Ore Operations with steel production at Big River Steel Works. The planned facility will be located adjacent to Big River 2, allowing hot DRI to be fed directly into its EAFs.
DRI is produced by removing oxygen from iron ore without melting it, creating an ore-based feedstock for EAF steelmaking. The material can replace prime scrap, improving cost competitiveness and supply reliability. DRI produced at the facility can also be formed into hot briquetted iron (HBI) for transportation and use at other destinations.
The project follows the completion of U.S. Steel’s $3 billion Big River 2 expansion, which began producing steel in 2024. Together, Big River Steel and Big River 2 house four EAFs and produce more than six million tons of steel annually.
The new DRI facility will further integrate the company’s iron ore mining, ironmaking, and steel production operations within its U.S. manufacturing network.
Press release is available in its original formĀ here.