New Connecticut Facility Combines HIP and Vacuum Heat Treating

A new thermal processing facility in Connecticut has opened, combining hot isostatic pressing (HIP), vacuum heat treatment, and brazing capabilities under one roof. The operation expands U.S. processing capacity for aerospace, defense, space, and other advanced manufacturers, allowing clients to consolidate critical thermal processing operations with a single provider.

Aalberts surface technologies celebrated the grand opening of its new Windsor Locks facility on November 11, 2026. The operation encompasses more than 100,000 square feet and is the first in the northeastern United States to combine HIP and advanced vacuum heat treatment capabilities in a single location.

Located in Connecticut’s Aerospace Alley, the facility is designed to streamline supply chains, reduce logistical complexity, and improve turnaround times by limiting the need to transport components between multiple processing facilities.

Steve Wyatt
President
Aalberts surface technologies

“This investment represents an important step in expanding our capabilities and supporting the future of American manufacturing,” said Steve Wyatt, president of Aalberts surface technologies. “By bringing HIP and vacuum heat treatment together under one roof, we’re offering our [clients] a more integrated solution that simplifies their supply chains while reinforcing Connecticut’s position as a center of aerospace and advanced manufacturing excellence.”

The new operation represents an investment in domestic thermal processing capacity and strengthens the regional manufacturing supply chain. Its integrated capabilities are intended to address increasingly complex client requirements across advanced manufacturing industries.

Press release is available in its original form here.