Analysis of Heat Treat on Carburized Ring Gear and Multivariate Regression Model Development

BOTW-50w  Source:  Thermal Processing for Gear Solutions

Like most other heat treatments, the carburizing and hardening process is known to introduce dimensional changes and gear distortion [4]. If these size and shape changes can be anticipated and controlled, it is possible to eliminate post–heat treatment machining by designing ring gears that would allow for the heat treat change. Such gear manufacturing would significantly reduce cost and machining-to-assembly time, both of which are critical in a commercial environment and large-scale production.

Read More:  Analysis of Heat Treat Growth on Carburized Ring Gear and Multivariate Regression Model Development

Analysis of Heat Treat on Carburized Ring Gear and Multivariate Regression Model Development Read More »

Improved Materials and Enhanced Fatigue Resistance for Gear Components

BOTW-50w Source:  Thermal Processing for Gear Solutions

“When trying to improve fatigue properties, two important areas need to be addressed: improvements of material and improvements in heat treatment technology.”

Read More: Improved Materials and Enhanced Fatigue Resistance for Gear Components

Improved Materials and Enhanced Fatigue Resistance for Gear Components Read More »