Partner for NASA and F1 Increases Productivity with Vacuum Furnace

A supplier of aviation and defense industry components, a NASA and Formula 1 partner has recently purchased a  horizontal two-chamber furnace with oil quenching and LPC. The furnace will be used for the heat treatment of aviation parts.

SECO/WARWICK is supplying the CaseMaster Evolution® two-chamber, horizontal vacuum furnace with oil quenching consisting of a heating chamber and a quench bath equipped with a loading and unloading vestibule. The load cooling can be carried out in two different centers: dynamically in inert gas (1.5 bar abs) and in quench oil. This solution enables users to implement a variety of heat treatment and thermo-chemical processes, such as vacuum carburizing.

Noted Maciej Korecki, vice president of the Vacuum Segment at SECO/WARWICK, “[This model] is one of the most frequently chosen furnaces for metalworking by the aviation industry."

The furnace can be switched on and off without additional time and energy expenditure. It does not require users to maintain the system at specific temperature parameters when at standstill, as is the case of traditional gas furnaces.


Find heat treating products and services when you search on Heat Treat Buyers Guide.com


Skip to content