U.S. Defense Contractor Expands Heat Treat Capabilities

HTD Size-PR Logo

Vacuum Sintering Furnace from Signature Vacuum Systems, Inc.
Source: Signature Vacuum Systems, Inc.

A United States defense contractor will expand their heat treat capabilities with a custom ceramic sintering vacuum furnace. The furnace will be provided with a 36” diameter x 48” high work zone in a graphite hot zone rated for 3362°F (1850°C).

The Model VBS-12 ordered, will increase production capacity and is the fifth furnace from the supplier, Signature Vacuum Systems, Inc., to be manufactured and installed in this contractor’s facility.

“Our strength[…] is solving problems and delivering solutions,” said Greg Kimble, president of Signature Vacuum Systems, Inc. “We have enjoyed the progression of this relationship over the years and we are committed to providing quality products and dependable services.”

 

 

 

 

 

 

 