MANUFACTURING HEAT TREAT NEWS

Recognizing the U.S. Veterans Within the Heat Treat Industry

Although Veteran’s Day, set aside to honor military veterans — those who served in the United States Armed Forces — is November 11, because this year the date falls on a weekend, Monday, November 12, is the day the U.S. observes the celebration and commemoration of this federal holiday.

Veterans Day coincides with other international holidays, including Armistice Day and Remembrance Day, celebrated in countries that mark the anniversary of the end of World War I. (Major hostilities of World War I formally concluded at the 11th hour of the 11th day of the 11th month of 1918, when the Armistice with Germany went into effect.)

A number of heat treating and heat treat-related businesses are owned and operated by veterans of U.S. military branches, and it is our honor to recognize some of those companies below. In addition, we feature 3 members of our class of 2018 40 Under 40 who are U.S. veterans.

Baker Furnace, based in Brea, California, designs and manufactures industrial ovens, heat treat furnaces, and pollution control equipment. Acquired in 2015 by Thermal Product Solutions.

Century Inc., headquartered in Traverse City, Michigan, provides precision machining, heat treating, welding and cladding, and testing and inspection services for a variety of industries, including aerospace, automotive, defense, and energy sectors.

Certified Metal Craft is a brazing, cryogenics, and heat treating company based in El Cajon, California.

Nick Suchoski

Global Furnace Materials, based in Janesville, Wisconsin, is a leading distributor for semi-finished refractory metal products. Owner Nick Suchoski, who served in the US Army as a combat engineer, was featured in a previous Veterans Day article on Heat Treat Today, “Veteran-Owned Heat Treat Supplier Commits 1% of Profits to Warrior 360” and was selected for Heat Treat Today‘s 40 Under 40 inaugural class of 2018.

Quality Calibration Servies LLC, based in New Berlin, Wisconsin, an ISO/IEC: 17025 accredited full service metrology lab.

RIS Enterprises, based in Oxnard, California, provides calibration services, industrial instrumentation, and products to manufacturers, laboratories, and industrial companies in Southern California, Utah and Nevada. (including Nadcap certification).

40 Under 40 recipients and Honorable Mentions:

 

Lee Rothleutner

In addition to Nick Suchoski, Lee Rothleutner, Prinicipal Development Engineer with The Timken Company, and a veteran of the U.S. Coast Guard, was represented in our 40 Under 40 class of 2018. Recipient of an Honorable Mention for the 40 Under 40 class of 2018, Matt Watts, Business Development Manager with Ultra Furnace Parts, served in the United States Air Force as an Avionics Test Station and Analysis Technician on the B1 Bomber.

Matt Watts

We ask our Heat Treat Today readers to join with us in honoring our U.S. veterans, including those who work among us in the heat treating industry.

Recognizing the U.S. Veterans Within the Heat Treat Industry Read More »

Heat Treat Today’s Meet the Consultants: Adeel Karim

Heat Treat Today recently unveiled its Heat Treat Consultants page in the October 2018 print edition (available in digital format here) and at FNA in Indianapolis, Indiana. We offer this comprehensive listing of heat treat industry consultants as part of our efforts to help minimize the effects of heat treat “brain drain.” With so many heat treat brains growing older, the expertise that once used to reside inside of manufacturing operations is dwindling. Where, then, do manufacturers with in-house heat treat departments go when they need heat treat answers?

Turn to Heat Treat Today and our comprehensive list of heat treat industry consultants, which we will introduce to you one by one in this occasional feature, “Meet the Consultants”. There is no more comprehensive list of heat treat consultants. Learn more about Adeel Karim in below’s inaugural entry, and then click through to the page to read more details about each consultant. We are adding more regularly. Contact them directly, or call us and we’ll introduce you to them. Whether it’s a technical process question, a safety concern, a compliance issue, or a business related question, one of our heat treat consultants will be able to help. If you are a consultant and would like to be listed, please contact Doug Glenn.


Name: Adeel Karim
Company Name: Doctor Furnace, Inc.
Location: Tampa, Florida, USA
Years in Industry: 15+
Consulting Specialties: Pyrometry /Nadcap Implementation

Email: Adeel@doctorfurnace.com | Phone: 614-519-0740, 352-315-9090

Briefly:

Adeel Karim is Doctor Furnace, the role he took on not long after he founded Heat Treat Professionals, Inc., in 2002 to provide clients with Nadcap and heat treating consulting. He went on to launch Doctor Furnace Inc. which continues to contribute to the industry today by offering clients expertise in pyrometry and Nadcap implementation (specification knowledge includes: AMS 2750,  PWA F40, BAC 5621, RPS, DPS 1.700, GE P10TF1 and F3, and Bell Helicopter to name just a few), as well as the latest and best products and services to the heat treatment industry. Adeel operates as a training specialist and private consultant in pyrometry in all aspects of the industry, including to Fortune 500 companies in aerospace and defense, and is currently on the lecturing circuit for pyrometry. In addition, Adeel is also part owner of ZK SONS, Inc, a holding company of IT, agriculture, and vocational education companies, and a concierge jeweler specializing in custom diamond and luxury watches with offices in Tampa, Dubai, and Karachi under the business name of Carats & Cents.

Publications or Significant Accomplishments:

  1. Founded Heat Treat Professionals Inc. (2002).
  2. Founded Doctor Furnace Inc. (2004).
  3. Nadcap heat treat consultant and pyrometry expert for Boeing, Lockheed, Rolls Royce, GE Aircraft, Pratt & Whitney, and Safran Snecma Group amongst others. Implementation of Nadcap in heat treatment, chem processing, welding, and NDT amongst others.
  4. Author of “The Latest on AMS 2750 Rev. E”, published at Industrial Heating (2014).
  5. GAP analysis, procedure writing, training, cap ex survey , and Nadcap response development support.
  6. Record 228 companies with zero failures in any discipline in attaining Nadcap Accreditation.
  7. Global Lecturer & Consultant for the latest revisions of AMS 2750, CQI 9, BAC 5621, RPS 953, PWA F40, and GE P10 T F3.
  8. Consultant with GE Aviation (2011-2013).

Links to Other Resources from This Consultant

References available upon request from the Consultant

Heat Treat Today’s Meet the Consultants: Adeel Karim Read More »

Specialty Alloys Firm Enhances AM Capabilities with Powder Lifecycle Technology Acquisition

A Pennsylvania producer and distributor of premium specialty alloys recently announced it has acquired a leader in the development and supply of advanced metal powders and powder lifecycle management solutions.

Carpenter Technology Corporation, based in Philadelphia, Pennsylvania, broadens its role as a leader in solutions provider in additive manufacturing with the approximately $81 million purchase of LPW Technology Ltd (LPW), based in Widnes, Chesire, United Kingdom, with additional processing operations near Pittsburgh, Pennsylvania. The acquisition incorporates metal powder lifecycle management technology with quality control and traceability.

Tony R. Thene, Carpenter’s president and CEO

Carpenter’s alloy production includes titanium alloys, nickel- and cobalt-based superalloys, stainless steels, alloy steels, and tool steels and is used in applications within the aerospace, transportation, medical, and energy sectors.

“Our aggressive development in key aspects of Additive Manufacturing (AM) demonstrates our commitment to build on our industry-leading position in this space,” said Tony R. Thene, Carpenter’s president and CEO. “The acquisition combines LPW’s metal powder lifecycle management technology and processes with our technical expertise in producing highly engineered metal powders and additively manufactured components.”

Phil Carroll, LPW’s founder

Lifecycle management technology is becoming increasingly important to understanding how materials behave before, during, and after production in the powder-bed fusion process.  Understanding powder behavior is critical as AM becomes more widely adopted and implemented across various industries.

“LPW’s innovative platforms and enabling technology further solidify Carpenter’s position as a preferred provider of end-to-end next generation Additive Manufacturing solutions,” said Phil Carroll, LPW’s founder. “I’m extremely proud of the accomplishments we’ve achieved at LPW and I’m excited to be part of Carpenter’s continued growth and leadership in AM.”

 

Photo credit: Additive Manufacturing Magazine

 

Specialty Alloys Firm Enhances AM Capabilities with Powder Lifecycle Technology Acquisition Read More »

Steel Rail Producer Looks to Invest in Mill Expansion

A leading North American steel rail producer is looking to invest at least $200 million into the expansion of its footprint in Pueblo, Colorado.

Evraz Rocky Mountain Steel has three mills in Pueblo and is considering building another or replacing one of the existing mills in the Steel City. The Pueblo city council approved a $15 million incentive package for the company.

“It is hard to find anybody in Pueblo who has not had a family member work at the steel mill in the last 135 years. The investment the community looks to make in this project celebrates the incredible workforce at the steel mill who will continue to make Pueblo proud. We look forward to 135 more years,” said Jeff Shaw, President and CEO of Pueblo Economic Development Corp. “Since 1882, the year that the first rail came out of the Colorado Fuel and Iron Plant, Pueblo has been known as the Steel City. The steel industry and the CF&I steel mill, now EVRAZ, has literally been the backbone of the community. Not only does the mill produce steel that is used all over the world, it also provides thousands of direct and ancillary jobs that bolster the local economy and help keep Pueblo moving forward in a strong and thriving direction. ”

Evraz has until December 2019 to make a final decision.

 

 

Steel Rail Producer Looks to Invest in Mill Expansion Read More »

CNC Machined Components Manufacturer Acquires Like Company

An industry leader in the production of CNC machined components recently announced the completion of the acquisition of a Summerville, South Carolina, manufacturer of similar products for the commercial truck, agricultural, utility vehicle, automotive and appliance markets.

Skyway Precision, based in Plymouth, Michigan, has added Bellwright Manufacturing LLC to its footprint, which includes manufacturing facilities in Michigan and Wisconsin. The Summerville location is now operating as Skyway Precision South, Inc.

“We are excited to work with the Bellwright team to enhance our value proposition to our customers,” said Bill Bonnell, President of Skyway. “This transaction demonstrates our continued commitment to leadership in our core products and technologies and to creating long-term, value-added partnerships with our customers. We will continue to pursue disciplined organic growth with our customers, as well as strategic acquisitions.”

Skyway is a leader in the machining of complex, close tolerance, iron and aluminum drivetrain components for the transportation and general power markets, including light and heavy commercial truck, recreational vehicle, automotive, marine, construction, agricultural, and power generation equipment applications.

CNC Machined Components Manufacturer Acquires Like Company Read More »

The Heart of a Vacuum Furnace System

 

Source: VAC AERO International

 

Heat treaters know that the heart of a vacuum furnace system is the pumping system. As broad as the variety of furnaces is, so is the selection of pump types.

A roots blower, which also goes by the name “booster pump” and “intermediate stage vacuum pump,” is a dry, gas transfer pump that boosts the performance of the primary pump, providing an increase in pumping speed and pressure. This article from VAC AERO International’s Vacuum Pump Technology: Education and Training page provides an exhaustive analysis of the heart of a vacuum furnace system: the pump.

“Roots blowers have the reputation of being virtually indestructible and run for years seemingly unattended while the primary (mechanical) and high vacuum (diffusion pumps seem to receive all the attention. While they need little day-to-day maintenance, monitoring of the oil level in the pump is required. The main function of these booster pumps is to improve pump-down rates and ultimate vacuum levels.” ~ VAC AERO International

Read more: “Roots Blowers (aka Booster Pumps)”

The Heart of a Vacuum Furnace System Read More »

Passenger Pod Unveiled as Race to Hyperloop Technology Speeds Up

 

Source: ThomasNet.com

 

A company which has been moving hyperloop transport technology closer to reality is Hyperloop Transportation Technologies, which recently unveiled its full-sized Hyperloop passenger pod, expected to allow for the comfortable transportation of 28 to 40 passengers. The capsule skin is made of Vibranium, carbon fiber with embedded sensors.

Read more here: "Hyperloop Heats Up with Unveiling of New Passenger Pod"

 

Passenger Pod Unveiled as Race to Hyperloop Technology Speeds Up Read More »

Industrial-Scale Metal Alloy Powder Plant Launched in U.K.

A U.K.-headquartered company with a solid-state alloy powder technology recently announced its launch of the world’s first industrial-scale metal alloy powder production facility based on the company’s process.

Metalysis will produce valuable alloy powders at the new plant, located in the company’s Materials Manufacturing Centre in Wath upon Dearne, South Yorkshire, U.K.

The Generation 4 (“Gen4”) project was mechanically completed on time in Q4 2017. It has since undergone hot commissioning, trial runs, optimization and handover to Operations, signaling Metalysis’ transition into commercial production following more than a decade of phased technology development.

Dr. Dion Vaughan, Chief Executive Officer, Metalysis

Gen4 is the first facility to take Metalysis’ solid-state, modular, electrochemical process to industrial scale and can produce tens-to-hundreds of tonnes per annum of high value, niche and master alloys. It creates a new U.K. source of supply for global end-users in advanced manufacturing disciplines including aerospace, automotive, batteries, light-weighting, magnets, mining and 3D printing consumables.

A standout benefit of Metalysis’ technology is its multi-metal capability, which enables it to produce alloy “recipes” that comparable processing routes cannot. Where conventional technologies are unable to elegantly combine elements with melting and density differentials, this technology can because it is a solid-state process. Gen4 enables Metalysis to commercially produce a demand-driven product mix of titanium alloys; master alloys including Scandium-Aluminide, which continues to pose excellent launch product potential as announced on 11 June 2018; compositionally complex alloys including High Entropy Alloys; magnet materials; high-temperature materials; and Platinum Group Metal alloys.

“In powering up and operating our industrial plant, Metalysis is poised to achieve its target to generate significant profits from our new South Yorkshire production facility,” said Dr. Dion Vaughan, Chief Executive Officer. “Ours is a true British success story with international implications. Metalysis has grown from the ‘lightbulb moment’ at Cambridge University in the late-1990s, relocated to South Yorkshire to benefit from regional excellence in operational skillsets in the early-2000s, and now onwards towards a bright commercial future.”

 

Industrial-Scale Metal Alloy Powder Plant Launched in U.K. Read More »

SBQ Alloy Manufacturer Acquired by Steel Producer

A U.S. steel producer recently announced the completion of the acquisition of substantially all of the assets of a manufacturer of special bar quality (SBQ) alloy and carbon steel bar flats.

Glenn Pushis, Senior Vice President, Long Products Steel Group

The assets of Kentucky Electric Steel acquired by Steel Dynamics are located outside of Ashland, Kentucky, and are comprised of a rolling mill with an annual capacity of 250,000 tons.  The operations were closed earlier this year by the prior owner, and Steel Dynamics plans to reopen the rolling mill in November 2018.  The facility will be operated as part of Steel Dynamics’ Steel of West Virginia (“SWVA”) operations, which is located within 20 miles of Ashland.  The acquisition will provide product diversification for SWVA through the addition of flats and specialty alloy bars.

“KES has been a loyal customer of our SWVA and Roanoke Bar divisions,” said Glenn Pushis, Senior Vice President, Long Products Steel Group.  “We believe that the complementary product offerings will provide value to our customers.  We currently anticipate that roughly 100,000 to 150,000 tons of billets will be shipped each year from our long products steel mills to be further processed at Ashland, providing additional value-added capability and higher through-cycle utilization for our steel mills.”

SBQ Alloy Manufacturer Acquired by Steel Producer Read More »

Marc Glasser on Heat Resistant Alloys — RA330®

This is the second of three articles by metallurgist Marc Glasser on three individual heat resistant alloys. This article will feature RA330®. Please submit your questions about heat-resistant alloys for Marc to editor@heattreattoday.com.


RA330® is a nickel alloy containing 35% nickel, 19% chromium, and 1.2% silicon. Over the years, it has become one of the most widely used wrought heat-resistant alloys due to the combination of its versatility, availability, properties, and cost-effectiveness.

 

The Chemistry of RA330

The chemistry of RA330 is shown below in Table 1.

There are several important benefits to this alloy including:

  1.  Oxidation resistance up to 2100°F
  2. Usable creep resistance up to 1850°F
  3. Utility up to 2100°F when there are no loads applied and some deflection can be tolerated
  4. Resistance to many heat treating atmospheres including carburizing and nitriding
  5. Sufficient nickel content to prevent sigma phase formation and embrittlement

The oxidation resistance of various alloys is shown in Table 2 below¹.

Table 2: Oxidation limits of various materials.

 

The oxidation limit for RA330 is higher than that of any stainless steel, comparable to alloy 600, and only exceeded by nickel alloys with much higher nickel content.

RA330 Creep Strength

Table 3² shows the creep strength required to produce 1% strain in 10,000 hrs.

 

The creep strength of RA330 is better than all heat-resistant stainless steel grades except RA 253 MA. It is comparable to alloy 600 but less than the higher nickel alloys 601, RA333, and RA 602 CA. When comparing the economics of RA330 with those of the more expensive nickel alloys, RA330 often has enough creep strength for many heat treating applications and is often the most economical option. There are companies who use RA330 above 1800°F and sometimes as high as the 2100°F oxidation limit. They compensate for the very low creep strength at these temperatures by using braces such as gussets or supports. These supports may be made of ceramic or a different alloy with significantly higher creep strength at this temperature.

Strength Variables and Value

One of the excellent attributes of RA330 is its ability to resist the various atmospheres used in surface or case hardening operations. Thermodynamically, the formation of nickel carbides and nitrides are not favored. With 35% nickel, RA330 has sufficient nickel content to resist carburization, nitriding, and combinations of both. The alloy is not immune to surface hardening, just resistant. The length of resistance time is a function of the process and process variables. For example, field experience shows that 310 muffles used in carburizing atmospheres can completely carburize in as little as 1 month, especially at high temperatures. After that, the material is brittle and can rupture easily. Often, the usable life will be between 1 and 3 months depending on process temperature. A corresponding RA330 muffle under the same atmosphere will last up to 1 year.

Stainless steels are subject to sigma phase formation and embrittlement. Sigma phase is an intermetallic phase that consists of iron and chromium. It precipitates between approximately 1100 and 1600°F. Sigma phase does not embrittle materials at these relatively high temperatures, but at room temperature, sigma phase can reduce charpy impact values to single digits. One sudden impact can cause catastrophic failure. RA330, with 35% nickel, has enough nickel to prevent sigma phase formation.

Applications of RA330

RA330 is available from stock in many product forms. In addition to the traditional plate, sheet, and round bar, RA330 is also available in expanded metal, pipe, and hexagonal nuts. Round bar can quickly be turned into threaded bar. The ability to draw on all these items from stock make RA330 the ideal alloy for maintenance and repair.

RA330 is resistant to thermal fatigue. This property lends RA330 to be the wrought alloy of choice for alloy fixtures and baskets that require quenching a least once a day.

For all of these reasons, RA330 is often an excellent choice for heat treating applications. It has good oxidation resistance, good resistance to case hardening atmospheres, no sigma phase formation, and thermal fatigue resistance. It is available from stock in many forms and sizes. RA330 may not always be the best solution, but often it is the solution that works best.

One of the few atmospheres in which RA330 is not a good choice is sulfur. Like other nickel alloys, the nickel forms a nickel-sulfur intermetallic at a low temperature. In such environments, a lower nickel stainless steel such as 309 or 310 is often a better choice.

RA330® is a trademark of Rolled Alloys.

1. Glasser, Marc, “Selecting an Appropriate Heat-Resistant Alloy,” Industrial Heating. September 2014: 59-65.

2. Condensed from “High-Temperature Environments: Alloy Properties,” https://www.rolledalloys.com/technical-resources/environments/high-temperature/


Marc Glasser is Director of Metallurgical Services at Rolled Alloys and is Heat Treat Today‘s resident expert in process metallurgy, heat treatment, materials of construction, and materials science and testing.

Marc Glasser on Heat Resistant Alloys — RA330® Read More »