Qatar Extrusion Supplier Switches to Gas Nitriding System

A gas nitriding system configured for treating various sized flat and hollow dies used in the production of aluminum extruded profiles for the construction and transportation markets was installed in January 2018 for a Qatar-based company that manufactures and supplies mill finished and powder coated aluminum extruded products.

Qatar Aluminum Extrusion Company (Qalex) awarded a contract to Nitrex Metals, a nitrding/nitrocarburizing technologies and solutions supplier based in Québec, for the supply and installation of an NX-1015 potential-controlled gas nitriding system which Qalex sought to adopt new technological innovations in nitriding when equipment and die quality requirements could not be met with the existing fluidized bed nitrider.

The NX-1015 furnace has a load capacity of 4400 lbs (2000 kg), and while this is slightly larger than current production needs, the additional capacity will accommodate future growth, when Qalex adds a second extrusion press. The precise interaction between the furnace and advanced control system allows the atmosphere to be adjusted automatically, according to the recipe and parameters entered. Integral to the system operation, Nitreg® technology is customized and pre-tested for extrusion dies to ensure optimum results of the nitrided layer, as well as to obtain repeatable results and higher throughput per die.

Skip to content