Kolene Corporation

Heat Treat Radio #138: 90 Years in Heat Treat — The W.H. Kay Story


W.H. Kay Company is celebrating 90 years in the heat treating industry. Third-generation owner, Michael Kay, joins publisher, Doug Glenn, on this episode of Heat Treat Radio to look back at nine decades of family ownership, the company’s evolution from a manufacturer’s representative to a major source for used heat treat equipment, and the relationships and persistence that have kept the business moving since 1936.

For a closer look at W.H. Kay’s nine decades in the industry and the business philosophy behind its longevity, read Heat Treat Today’s company profile, “W.H. Kay Marks 90 Years by Staying in the Flow.”

Below, you can watch the video, listen to the podcast by clicking on the audio play button, or read an edited transcript.




The following transcript has been edited for your reading enjoyment.

90 Years of W.H. Kay (00:30)

Doug Glenn: Welcome to another episode of Heat Treat Radio. I’m here with Mike Kay from W.H. Kay Company celebrating their 90th anniversary. I just want to say you look pretty good for 90.

Michael Kay: Thank you very much. That’s called clean living.

Doug Glenn, publisher of Heat Treat Today (left), sat down with Michael Kay, president of W.H. Kay (right) | Image Credit: Heat Treat Today

Doug Glenn: It is. I just want to run down a variety of different questions and get a sense of the company and go from there. So, 90 years means the company started in what year?

Michael Kay: 1936.

Doug Glenn: 1936. Historically, just to give those of us who are not history buffs, 1936 was kind of in the midst of the Great Depression.

Michael Kay: Or right before World War II, which kind of ramped up production of industries, so it was good timing.

Doug Glenn: Do you think that was part of it?

Michael Kay: I’m sure it didn’t hurt them in the first year or two, getting established.

Doug Glenn: Who actually founded the company?

Michael Kay: W.H. Kay is William Henry Kay. That’s my grandfather. He passed away in 1972 of heart failure. Back then, there were no stents or anything like that. He went to Yale. I don’t know what he was doing out east, but Eclipse Combustion at the time gave him the Cleveland territory, so he moved his family to Cleveland.

Doug Glenn: Where was he moving from?

Michael Kay: I believe from Connecticut. He got married, and I had a child at that point, which was my uncle. He took the Eclipse line, and at that time they were selling both heat treat furnaces and burners. In the older heat treat shops you’ll still stub your toe on an Eclipse furnace, a pit temper, or a box furnace. Then they primarily got out of the furnace business around the 1960s.

Doug Glenn: Very interesting. Your grandfather probably would have been a contemporary and friends with Cam Perks, right?

Michael Kay: For sure. There’s a sales meeting picture of them on our wall here from around 1948.

Doug Glenn: Cam was the father of Doug and Lock Perks. Of course, during our growing years, our industry years, they were running Eclipse at that time in Rockford.

Michael Kay: Correct, in the ’80s, ’90s, and 2000s.

Doug Glenn: Right. I find the connections really interesting. It was your grandfather that started it in 1936. He moved to Cleveland, and Eclipse gave him the Cleveland territory. That’s when the company was established, The W.H. Kay Company?

Michael Kay: In 1936, correct. All he had was an office. He might have started out of his house. I’m not even sure of that. But he moved to a little office, with no warehouse or anything.

Doug Glenn: And he was just basically working with Eclipse.

Michael Kay: Yes, as the manufacturer’s rep. Back then, you’d get an order, write it up by hand, and put it in the mail.

Doug Glenn: Can you imagine? A week later, the company would find out they had sold something.

Michael Kay: That’s right. We still have invoices from the ’30s.

Doug Glenn: Is that right?

Michael Kay: Yes, an entire heat treat furnace for $700.

Doug Glenn: Wow. $700 for a heat treat furnace. That’s amazing. How long did your grandfather work by himself, or did he grow relatively quickly after that?

Michael Kay: I think he worked by himself until my Uncle Bill came into the business in, I’d say, the late ’50s. So, it was 20 years by himself. Then my father started in the late ’50s. They took it over in the late ’50s, early ’60s.

Doug Glenn: Your grandfather basically ran it for 20 years, and then your uncle and your dad, Frank, started. I’ve met your dad. I’ve never met your uncle.

Michael Kay: I worked with him for 10 years before he passed away in ’95, unfortunately.

Doug Glenn: At the time that your uncle and your dad got involved, was it still primarily just a rep firm?

Michael Kay with a furnace from Surface Combustion | Image Credit: W.H. Kay Company

Michael Kay: They kept Eclipse, and then they repped for a couple more companies, like Upton Furnace in Detroit and Surface Combustion. They repped Surface for 10–12 years, maybe longer, in the late ’70s and early ’80s. Then they eventually started repping for SBS, the oil cooler guys.

Doug Glenn: Jeff Smith.

Michael Kay: Right, Jeff Smith.

Doug Glenn: His son George still owns the company.

Michael Kay: I think they’re in Florida.

Doug Glenn: Correct; they moved down to Florida.

Michael Kay: So, it was all around process heating. You had to be careful. You couldn’t represent companies that competed against one another.

Doug Glenn: Still happens to this day, where the reps need to be careful.

Michael Kay: That’s right.

Doug Glenn: Do you consider yourself now to be a rep firm?

Michael Kay: Yes, we’re still repping. Honeywell bought Maxon and Eclipse. They call us a distributor, but we still design burner systems. I think if you’re just taking orders, you’re kind of in trouble. You have to be proactive.

Doug Glenn: Be able to provide other services.

Michael Kay: You have to apply the product.

Doug Glenn: Are you repping any furnace manufacturers?

Michael Kay: We represent an oven manufacturer, JPW Oven Design out of PA, up to 1400 degrees, which covers most tempering and aluminum. I think we kind of found a niche of aluminum heat treat, so we’ve sold a bunch of those.

Doug Glenn: I know them, north of Williamsport.

Michael Kay: Now they’ve expanded towards Williamsport with a bigger facility.

Doug Glenn: So at the time your dad and uncle took over, though, it was still pretty much just Eclipse.

Michael Kay: Manufacturer’s rep and several furnace manufacturers. Upton with salt.

Doug Glenn: Yes, salt baths.

Michael Kay: And Surface’s IQs. We competed against Lindberg, who was manufacturing IQs and other similar equipment.

Doug Glenn: Upton is now owned by Kolene Corporation.

Michael Kay: That’s correct. They’re still around, I think, in the Detroit area.

Doug Glenn: Ken Minoletti, I assume he’s still working with Kolene now.

Michael Kay: I think so. I’ve seen Dennis McCardle at the shows.

Doug Glenn: Good people and good company. It was your grandfather, then your uncle, and your dad joined in, let’s say, late ’50s-ish. Did anybody else join before you joined, or were you basically the next heir apparent?

Michael Kay: I think they had a sales rep for a time, a retired guy they took on just to help. But pretty much, that was only for two or three years.

From Manufacturer’s Rep to Used Equipment (10:06)

Michael Kay: Eclipse phased out of furnaces. They still had customers that wanted these furnaces. They took the prints and had furnaces built, and they needed a warehouse, so they built a place to actually build furnaces for a time.

Doug Glenn: When you say “they”, you’re talking about your family.

Michael Kay: Right. My father and uncle. This is in the ’60s. They would redo a print and do a pit draw, a standard pit temper. Then they would have someone fab it in a shop. So, they built a little shop, and then, just in the course of sales, you’d sell a new one and the customer would say, “What am I going to do with the old one?” So, we’d take it in on trade, and that’s how we got our toes in the water on used equipment.

We would get the equipment in, sell the customer something new, and then take the trade. That’s how they got into it in the ’60s.

Doug Glenn: That’s kind of interesting. When Eclipse stopped making furnaces, you still had customers that wanted furnaces, so your family actually started building a few new ones based on the designs of the Eclipse one.

Michael Kay: Yes, just with existing customers. They weren’t marketing it. They weren’t going to be a new furnace maker. But if a customer had 12 Eclipse and he wanted 15, you could easily build it.

Doug Glenn: Then he would have used equipment that he wanted to get rid of, which was a service you could provide.

Michael Kay: Right.

Doug Glenn: So that’s how you got into it.

Michael Kay: Then they stopped making new ones.

Doug Glenn: When did they stop that?

Michael Kay: I’d say in the ’60s.

Doug Glenn: So primarily the ’60s is when the company basically evolved to what it is now. It’s mostly used equipment.

Michael Kay: We got more into the used equipment in the ’80s. In the ’70s, we had to be careful because we repped Surface. So, we didn’t want to sell used to nix a sale on a new one. It was always kind of on the back burner.

Doug Glenn: I wanted to ask you about your relationship currently with a lot of new equipment manufacturers. I could see there could be potential synergies there with them. I could also see where they could what you guys are doing and why you are helping them. I’m assuming if you need to rebuild or if your customers need to rebuild, obviously they’re going to be potentially going back to those manufacturers and asking for parts. How is your relationship with those equipment manufacturers?

Michael Kay: Yeah, in the course of 40 years, I’ve never seen a used take over a new account. If people are buying new, they’re buying new. If they’re buying used, they’re buying used. Generally. Now, Surface used to be a little nervous when we had IQs here, but when Midland-Ross bought Surface, they got rid of all the reps anyhow. Back in ’77 or something like that.

Doug Glenn: In the ’70s, I believe.

Michael Kay: Right. In general, it goes along with new sales. If a customer calls and says, ” I need an oven, like tomorrow,” I could quote him a new one in 16 weeks, or we could have a used one in 4 days.

Doug Glenn: Yeah, exactly.

Michael Kay: It helps the customer out, and then we’ll lease it to the customer. We might sell him a new one, buy the used one back, the one we rented him. It helps get the customer what they need. It’s more of a service than a detriment to the new manufacturers. That’s what we found.

Doug Glenn: Currently, do you have any established or closer relationship with any one furnace company than another?

Michael Kay: Only JPW, The Oven Guys.

Doug Glenn: We don’t hear much of them in the higher temperature heat treating. Although 1400 degrees, that’s relatively high. Like you said, aluminum.

Michael Kay: We’ve done some big ovens. When I say big, I mean 12 x 20 x 12 tempering furnaces.

A variety of equipment at the W.H. Kay facility | Image Credit: Heat Treat Today

Doug Glenn: I want to jump back to the founders for a little bit. Is there anything that you can recall, or any interesting stories about either your grandfather or your father when he was doing business?

Michael Kay: They were all kind of straight shooters. They had funny customers who would call. We had a couple of heat treaters that would just show up, look on our shelves, and they’d find some valve. “You know, I’ve been looking for this.” Then they’d say, “Just bill us for it.” There were those kinds of guys.

Doug Glenn: Back in the day, you had a Cleveland territory for Eclipse, and so I’m guessing most of your business was relatively regional, like in the Midwest?

Michael Kay: The Northern Ohio area. It went through Toledo all the way to Youngstown and Warren. Youngstown and Warren were big into steel.

Doug Glenn: Absolutely.

Michael Kay: And automotive as well. So down through Mansfield.

Doug Glenn: What about today?

Michael Kay: It’s about the same.

Doug Glenn: What about your used equipment?

Michael Kay: Used equipment can go anywhere.

Doug Glenn: I thought you were all over the country, or maybe even out of the country, for used equipment.

Michael Kay: Out of the country. We’ve shipped stuff to Mexico occasionally. I think the furthest one we’ve ever shipped was to Korea. Not North Korea, South Korea. And I think we shipped stuff somewhere to Europe. We shipped a vacuum furnace to Ireland like 8 years ago.

Doug Glenn: But the bulk of the equipment is going to be North America. Canada, U.S., Mexico.

Michael Kay: That’s correct.

Doug Glenn: Are there any other historical milestones that you can think of?

Michael Kay: In the last 15 years, when Honeywell bought Eclipse, that kind of changed things. We’ve always been a rep for Eclipse since 1936, and still rep Eclipse, which is amazing. 90 years with one company.

Doug Glenn: Exactly. I was going to say, I think you’re probably the only one.

Michael Kay: We’re the oldest rep, for sure. And then what changed things was that we would compete with Maxon. So, then Honeywell bought Maxon first. And then four or five years later, round numbers, I don’t remember, then they bought Eclipse too, so now we sell both.

Doug Glenn: They bought Maxon, Kromschröder, Hauck.

Michael Kay: Right. So, we sell all that stuff.

Doug Glenn: Interesting. So that was a milestone, a pretty significant change for this organization.

Michael Kay: That was a milestone. And then the other one was when we moved into this building, which was in 2000. My father and uncle built a 5,500-square-foot office warehouse, which had a crappy dock. It was not the right size, so trucks would pull up and we’d have to ramp them up, ramp them down, in the snow. We had wooden ramps.

Doug Glenn: Accident waiting to happen.

Michael Kay: Yes. And this old lift truck didn’t start half the time. Then we moved here in 2000, and we still call this the new building, which is kind of funny, 26 years later.

Doug Glenn: 26 years, and it’s still the new building. And we took a quick walk through this building, which is in Solon, Ohio, in the Cleveland area. How many pieces of used equipment do you have?

Michael Kay: I’d say a couple hundred, give or take.

Doug Glenn: Primarily made up of what type of equipment?

Michael Kay: Mostly ovens, some vacuum, some internal quench, and a lot of pit furnaces.

Doug Glenn: A lot of pit, okay.

Michael Kay: Tempering, those types of processes. We do get into kilns occasionally. Belt furnaces and ovens.

Doug Glenn: When I hear “ovens,” I think lower temperature. Is that what’s primarily out there? Although we also saw a pusher.

Michael Kay: We have a pusher furnace, which is mostly for gears that fed a quench press. They’re running at 1600 degrees.

Doug Glenn: You also have some IQs out there and some generators.

Michael Kay: Yes, Endo generators.

Doug Glenn: All different types of equipment, which are listed on your website for those who want to find out.

A Family Business Through the Generations (23:31)

Doug Glenn: The company’s been in the Kay family since the beginning, right?

Michael Kay: Right.

Doug Glenn: Family-owned business. How’s that been?

Michael Kay: It’s been good. Working with my father and uncle was fine.

Doug Glenn: No problems?

Michael Kay and Doug Glenn showing what an old sales catalog looks like | Image Credit: Heat Treat Today

Michael Kay: When I started in ’85, this is what I was given. It weighs about 15 pounds. You would haul that catalog out and make sales calls.

Doug Glenn: I remember seeing these on shelves in furnace companies.

Michael Kay: This is all the Eclipse burner information.

Doug Glenn: Wow. So, this is how you sold back in the day.

Michael Kay: Back in the ’80s. Before faxing.

Doug Glenn: Before fax, exactly right. That was a big deal when the fax came out.

Michael Kay: Fax was huge to get an order. Fax the order in.

Doug Glenn: Now you don’t see it, except unless you’re in a medical office, for security.

Michael Kay: That saved at least a week.

Doug Glenn: You could fax the order to the manufacturer instead of mailing it.

Michael Kay: And then they’d fax the acknowledgement back. Back in the day, you’d mail it in, and then you’d get an acknowledgement a month later that they got it. How did they get anything done back then?

Doug Glenn: So as far as transitions, obviously you mentioned your grandfather passed away, so passing it on to the next generation was not a problem. You guys all got along fairly well.

Michael Kay: Yeah, we got along. My brother-in-law came in 25 years ago.

Doug Glenn: Talking about Roger Hird.

Michael Kay: Roger, right. And then we hired another sales rep who’s still here.

Doug Glenn: That’s good. You’re into the third generation. Do you have succession plans or sales plans? 

Doug Glenn: Let’s talk a bit about your dad, because we were talking about him when we walked in. You don’t need a succession plan, at least for another 30 years, right? Because your dad’s still going at it. Tell us a bit about him.

Michael Kay: Right. He just turned 93. And he comes to the office three days a week. It keeps him active.

Doug Glenn: That gives you another 30 years before you have to worry about it.

Michael Kay: Exactly.

Doug Glenn: That’s crazy.

The Business of Used Heat Treat Equipment (28:16)

Doug Glenn: Would you be comfortable laying out what the ballpark percentage is between used equipment sales versus burner sales versus burner design?

Michael Kay: It’s probably 50/50. It gets more active some days, some months than others. We’ve had ovens and furnaces here for 15 years. It’s always a chess match at what’s selling and what’s not. If we put something in the corner, for sure it’ll sell, because then I’ve got to move nine furnaces to get it out. It’s always an active chess match.

Doug Glenn: You’re saying the oldest furnace that you’ve got here has been here 15 years, waiting for an owner.

Michael Kay: Right.

Doug Glenn: It must be a bit of a challenge knowing what to buy and what not to buy just based on what you think is going to be resellable.

Michael Kay: Right. I’d say it’s more of a question of what the condition is. We kind of go on the theory of good equipment. If you have something that you’re not exactly familiar with, like, for example, a blaster, if it looks nice, then we might buy that with a couple of furnaces.

Doug Glenn: Even though it’s not a thermal piece.

Michael Kay: Yeah, we don’t know much about blasters. But we know people.

Doug Glenn: You’re talking about like shot peen type stuff?

Michael Kay: Shot peeners, something like that. So, we might buy that if it’s nice, because we know people who know blasters. And then a lot of heat treaters use blasters anyhow.

Doug Glenn: Yes, for deburring.

Michael Kay: Right. So, it’s more the condition of the piece. You try and get different size ovens and not load up on little lab equipment.

Doug Glenn: I noticed you didn’t have much on the desktop or tabletop.

Michael Kay: We do. They’re on the other side, though. You couldn’t see them. We have probably 30 or 40 of that type of equipment. But we could have 300 of them. They’re kind of a dime a dozen. Most people throw them in the dumpster anyhow.

Doug Glenn: I’m curious how you go about finding the equipment. Do you have to proactively go out, or do you find most people are asking you to buy equipment?

Michael Kay: We used to buy equipment at auctions. Now, since it’s on the internet, it’s tougher to buy at an auction. It’s mostly with existing customers that have equipment they don’t need anymore that reach out asking what equipment we have that they can trade with. We got a call the other day, a customer we sold a furnace to seven years ago. He’s done with it, so he asked if we buy it back. That is helpful for our customers, to know that we’re around.

Doug Glenn: You’re not obliged to do that, right? But I assume with established customers you would try, just to keep them happy.

Michael Kay: As long as they didn’t blow it up. Which happens.

Doug Glenn: “We’ve got this furnace. We’d like to return it to you, and we’ve got it in three pieces now.”

Michael Kay: Exactly.

Doug Glenn: That would make it a bit rough.

Michael Kay: But mostly from established people we know. Now, there are people that call in and say they have an oven that they don’t want.

Doug Glenn: Are the people that you’re doing business with predominantly manufacturers who want to do their own heat treat, or are they commercial heat treaters?

Michael Kay: I’d say they’re both. I would say commercial heat treaters are a big part. We know most of them, being around for 90 years and all. They know us; we know them. But there are guys getting into it, just starting out. They need a tempering furnace to stress relieve welds, or they’re doing aluminum aging type of processes. So, I would say it’s both.

Doug Glenn: Tell me a bit more. I am seeing a bit of an uptick in the aluminum world as well. What are you comfortable saying about that? Because you mentioned that you’re doing more in that area.

Michael Kay: Since we’ve done ovens, we have customers who request aging, because that’s more of a longer process, so you see more aging ovens. And since we have partnered with JPW Oven, they build drop bottom furnaces, horizontal quench, and aging ovens. If we don’t have a used unit, then we say, “Well, we can sell you a new one,” because it’s hard to find a used drop bottom on the market. So, we found a little niche. We have sold five or six of them in the last four years.

Doug Glenn: Any sense of why that market is picking up at all?

Michael Kay: I think it’s perhaps that they’re trying to make products lighter, like vehicles. They’re trying to make them more fuel efficient as well. There are also composite components that need to be cured out. We do a lot of that.

Doug Glenn: You’re just talking about composite materials.

Michael Kay: Plastic composites, resins, and curing. It must be a Class A, solvent-rated product. All sorts of different processes use some sort of heat. It’s amazing. From Frito-Lay to Alcoa.

Doug Glenn: I’m curious what percentage of your equipment is going into metals or ceramics, as opposed to the lower temperature?

Michael Kay: That’s hard to say. All the new stuff we sell is going into low temperature ovens. But we sold a couple of car bottoms this year that are doing 1500 to 1600 degree annealing.

Doug Glenn: What’s the one or two pieces of equipment out there you’d really like to get rid of? Maybe there’s more than two.

Michael Kay: The electric car bottom would be nice to sell.

Doug Glenn: Tell me about it a little bit.

Michael Kay: Well, it’s a 1400-degree electric car bottom that kind of comes up like this.

Doug Glenn: Oh, long ways.

Michael Kay: Long ways. Like you’re trapping a squirrel. It’s designed for tempering stainless steel 30-foot-long bars. It’s a pretty good sized car bottom, but most people want gas-fired car bottoms.

Doug Glenn: And this is electric.

Michael Kay: This is electric. You could convert it, but that would be…

Doug Glenn: That’d be an expense. You might as well buy a new one.

Michael Kay: Yeah. The pieces of equipment that take up a lot of floor space, we want to keep moving in our warehouse.

Doug Glenn: I think it’s an interesting business, because you want to turn your inventory, just like most.

Stories & Lessons Learned (36:47)

Doug Glenn: Do you have any memorable customers, projects, or situations?

Michael Kay: Eclipse always tried to sell against the North American Tempest burner. So, we finally came out with a ThermJet back in, I’d say, the late ’80s, early ’90s.

Doug Glenn: I remember them advertising it. I think it was the early ’90s.

Michael Kay: It’s still a great burner. But we were the first ones to sell the burner on a big roller hearth in Mansfield.

Doug Glenn: Is that right?

Michael Kay: And literally there were 56 burners, and it was my job, and we had no idea whether they were going to work or not. On the startup, amazingly we had two or three engineers from Eclipse making sure it was right, and they all lit up the first time. And they work, like, amazingly well.

Doug Glenn: No kidding. Well, that’s sweet when that goes well.

Michael Kay: Yeah. That was a little nerve-wracking though.

Doug Glenn: Those types of experiences are fun though.

Great successes or moments when you thought things were going to fall apart in the history of the company?

Michael Kay: That was one of them.

Doug Glenn: Whether or not these burners would work?

Michael Kay: Right. That was a big job back in the ’90s. Because you had the valves, you know, it was a big job.

Doug Glenn: Whole gas trains and whatnot.

Michael Kay: And this was their main furnace.

Doug Glenn: Well, that one went well.

Michael Kay: Yeah, that was good.

Doug Glenn: I assume you had difficult times just business-wise at some point in time, right? Were the 2008 to 2010 years rough times?

Michael Kay: Well, Detroit wasn’t that great in the ’80s, you know?

Doug Glenn: Right. I remember, because you and I are roughly the same age, getting out of college didn’t feel like a great job market.

Michael Kay: Right. It wasn’t good at all. So, this one job in particular, we bought some furnaces from this guy in Indiana. I think it was either an auction or something. We bought four furnaces, and the riggers in Indiana loaded them up, and the furnaces never showed up.

Doug Glenn: You bought them, but they never got here?

Michael Kay: Right. And we tracked it down, and these guys were like gypsies, and they took our furnaces right to the scrapyard and scrapped them. So, it was like, “Who are these guys?”

Doug Glenn: Did you ever find them?

Michael Kay: No. Never found them. The police in Indiana knew about them, and they were like, “You don’t want to chase these guys.” So, I’m like, “Fair enough.” Our bad.

Doug Glenn: But how would you know? I mean…

Michael Kay: They were at the auction, giving out cards. But you didn’t know. That was one job in 40 years. It’s unusual for someone to take your furnaces and just scrap them.

Doug Glenn: They’re not exactly easy to move around or hide.

Michael Kay: No, they were something, those guys.

Getting in the Flow (40:58)

Doug Glenn: You guys have been in business for 90 years, and I’m kind of curious if there’s something in your mind at least that says, “You know, the reason this company is successful is because we’re committed to X or Y or Z.” I’m curious what that thing might be. And also, we were talking earlier about difficult times and how you get through the difficult times. Any comments on either of those, getting through, or how it is you’ve lasted 90 years, which is no small task?

Michael Kay: Well, just going out with my uncle and father: sales are all about getting in the flow. That means making an effort to be proactive. You just can’t wait for orders to come in. When you’re proactive, you also have to listen a lot, because what you initially get called in for, they might not be looking for that at all.

Doug Glenn: They may think that’s what they want.

Michael Kay: Right. We’ll get inquiries about a furnace that a guy’s interested in. We’ll go out and he’s like, “It’s a 1600-degree furnace, but…” I said, “Well, when you get right down to it, what temperature are you running? 900 degrees. Well, then this is the wrong furnace.” So, recommending and being able to find solutions for people has been key. Also, you have to appear well in any company. In other words, you could be talking to the guy on the floor who’s covered in oil, or the CEO of Alcoa, and anyone in between. So, you’ve got to appear well in anyone’s company.

Doug Glenn: When you say appear well, you mean make a good impression?

Michael Kay: Yes, just be comfortable and not dismiss people. You’ve got to find out who’s really making the decision. It might not be the president at all.

Doug Glenn: And you just kind of assume anybody you talk to is going to be involved in the decision.

Michael Kay: It might be the guy covered in oil who’s really wanting the solution, so you’ve got to know what you’re doing there. And it’s establishing a rapport. That’s the most important thing. If you know what they need, then you can quote what’s going to help them out, as opposed to quoting something that’s not going to work for them.

Doug Glenn: When you said get in the flow, it made me think about something I believe relatively strongly, and that is you’ve got to be out with the customers. Now, you would think that wasn’t the case here, because I’ve known you for 30-plus years and I’ve never been here. But in spite of that little piece of evidence that suggests otherwise, I assume that you personally have spent a good bit of time out and about. Are you still getting out and seeing them?

Michael Kay: You have to. Go see a furnace you sold two years ago. See how it’s running. People appreciate that. And you might stop there and do that, and then you will find something else. “Well, you know, that furnace over there, I’m not using.”

Doug Glenn: You would’ve never known it if you weren’t there.

Michael Kay: Exactly. Or they mention something, like, “My neighbor was looking for an oven.” “Who’s that?” Well, that turns out to be they’re setting up a whole heat treat operation. You never know. But you won’t know unless you’re in and out and about.

My father used to say you can waste a lot of time coming into the office every day. You can always make yourself busy.

Doug Glenn: There you go. Good point. Need to be out with the customers.

Michael Kay: You need to. It’s pretty interesting because we still have outside sales. A lot of people don’t anymore. The number of people has been reduced.

Doug Glenn: You have outside sales. Tell me about this now. You had mentioned the one gentleman who’s doing mostly phone work.

Michael Kay: Roger and I are outside sales.

Doug Glenn: I tend to be a big believer in that. Are you finding it more difficult these days to get into places, or is it still doable for you?

Michael Kay: It’s still doable. I mean, I think the number of salespeople that show up is one-tenth of what it was.

Doug Glenn: Way down.

Michael Kay: Way down. So, in some cases they’re like, “I haven’t seen a sales guy in six months.” So that way you have an advantage by getting out. In my opinion.

Doug Glenn: I think so. There’s a lot to be said about it. I think the whole email and text thing has also made it more difficult. Did you know Kelvin Spain? He was the president over there, general manager of Radyne, which is an Inductotherm company, and he passed away years ago. But I remember sitting with him at lunch, and it was probably during that ’08 to ’10 era when the economy was really down, and we were talking with him, and he was always such a positive, optimistic person. And I made some mention about how it seemed like people were finding it very difficult these days. And he just said, “No. You just need to work harder. That’s all. You just need to get out there and keep doing the fundamentals,” which is basically getting out and seeing people and whatnot.

Michael Kay: Yeah.

Doug Glenn: It’s difficult, but sometimes you just need to do it.

Michael Kay: Some things never change.

Doug Glenn: Meaning what? I was going to tell you what I thought that meant, but I’m curious what you mean.

Michael Kay: Well, you know who the good sales guys are. You create your own good luck. Why does this guy always get lucky with a sale? Because he’s in the flow. Sooner or later, you’re going to stub your toe on something good.

Doug Glenn: I forget who said it. I’m thinking Abraham Lincoln, but I don’t know. He says, “The harder I work, the luckier I get.”

Michael Kay: Exactly right. I think you do create your own good luck, for sure, in some respects.

Doug Glenn: Do you have a lot of interaction with AI here?

Michael Kay: I think AI is going to help people find us and our products. I haven’t tapped into that yet, but I think of AI as, what are the products that are going to come out of it? Drone technology, you see that. We have a couple of ovens going to people building drones. Because they’re all composite. They have to be light to fly.

Doug Glenn: Lightweight and strong.

Michael Kay: So yes, it’s probably going to diminish some aspects, but it’s going to create other industries too. Like anything.

Doug Glenn: Pretty optimistic about it, not too worried about it?

Michael Kay: Not too worried about it. It seems like no matter what year it is, process heating is going to come into play in whatever, computer chips, drone manufacturing, or aerospace. It’s not going away.

Doug Glenn: Another industry legend like yourself, who you would know if I mentioned his name, has said, “Nobody really wants to heat treat. Nobody really wants to thermal process.” If they could build whatever they’re building without doing it, they would.

Michael Kay: Oh, 100%. They would.

Doug Glenn: Some people think that with AI, we’re going to find ways to build products and eliminate unnecessary processes, like heat treating. I don’t know. We’ll see.

Michael Kay: I don’t think so.

Doug Glenn: We’ll see.

Michael Kay: 3D printing is interesting. You see some of these parts being made, but I think they still have to stress relieve them.

Doug Glenn: At this point, they do need to stress relieve, and I don’t know how it would work.

Michael Kay: It’s always going to be something.

Doug Glenn: So, you guys have been around 90 years. You’re kind of like the granddads of the industry, right? Because you’ve had a lot of experience. Any sage advice that you’d give to companies who are out there trying to be successful?

Michael Kay: I like the one that you can create your own good luck. You keep at it and get in the flow. Get out of the office. That’s what we’ve been doing. Well, I’ve been doing it for 41 years. Maybe not when I started. I had to haul this massive catalog around.

Doug Glenn: Right. Well, that’s why you’re in such good shape.

Michael Kay: I remember he’s like, “Just go out and make some sales calls.” I’m like, “With what?”

Doug Glenn: “What is that?”

Michael Kay: So that’s so funny.

Doug Glenn: Just a little bit of diligence is what keeps…

Michael Kay: Diligence, yeah. Exactly right.

Doug Glenn: Keep after it. So, next 90 years for you guys?

Michael Kay: Someone’ll be selling furnaces. Whether it’s us, I think I’ve got another 10 years probably. That’s my goal.

Doug Glenn: Well, you got inspired by your dad. I think I’m saying you’ve got 30 years.

Michael Kay: He’s the exception. But you never know. It’s nice to have an office to come to.

Doug Glenn: Yeah, it is. Purpose in life.

Michael Kay: Right. Whether you do anything or not. My father comes in; he’s 93. He comes three days a week, and then he plays bridge the other two.

Doug Glenn: Is that right?

Michael Kay: It keeps him occupied. You need to be pretty smart to play bridge.

Doug Glenn: You need to keep your mind and your body going.

Michael Kay: Keep your mind sharp.

Doug Glenn: And he’s in good physical shape?

Michael Kay: He’s pretty good.

Doug Glenn: For 93?

Michael Kay: He still drives.

Doug Glenn: That’s good.

Michael Kay: But yeah, he’s in pretty good shape. Oh, one other thing.

Michael Kay: When I first started it was always, “When is Eclipse going to can us?” So, it was always explained to me, just make yourself hard to get rid of. If you’re selling, it’s hard to get rid of someone who’s always selling.

Doug Glenn: It’s like the guy on the basketball team. It’s hard to get rid of your top scorer. You can have a guy that’s really good at assists, and he’s probably going to go before the guy that’s putting the ball in.

Michael Kay: They can yell at you but then send in an order. So, make yourself less expendable.

Doug Glenn: Less expendable. Fair enough. Very good.


About the Guest

Michael Kay
President and Owner
W.H. Kay Company

Michael J. Kay is President and third-generation owner of The W.H. Kay Company, a Cleveland-area company that has served the industrial heat treating and process heating industry since 1936. A graduate of Furman University, Michael earned degrees in business and U.S. history in 1984 and began his career the following year selling Eclipse burner systems and heat treating furnaces. He now brings more than 40 years of experience in industrial thermal processing to the business.

Under Michael’s leadership, W.H. Kay continues the work begun by his grandfather, William Henry Kay, providing combustion systems, heat treating furnaces, industrial ovens, controls, and practical process heating solutions to manufacturers and commercial heat treaters. The company also buys, sells, and trades used heat treating equipment, maintaining an extensive inventory of furnaces, ovens, atmosphere generators, vacuum furnaces, and related equipment at its Solon, Ohio, facility. W.H. Kay’s relationship with Eclipse dates back to the company’s founding and today includes combustion technologies from Eclipse, Maxon, and Kromschroder.

 

For more information: Contact Michael Kay at sales@whkay.com.

Heat Treat Radio #138: 90 Years in Heat Treat — The W.H. Kay Story Read More »

22 News Chatter To Keep You Current

Heat Treat Today offers News Chatter, a feature highlighting representative moves, transactions, and kudos from around the industry. Enjoy these 22 news items.


Equipment

  1. ROGESA Roheisengesellschaft Saar GmbH has commissioned SMS group to carry out a comprehensive modernization of blast furnace 4 (BF4), which will extend the service life of the blast furnace and ensure effective monitoring of the hearth lining. The contract includes the planning and delivery of the Paul Wurth hearth lining and multi thermocouple sensor probes (MTPs), as well as technical support during the installation phase at the in Dillingen, Germany, location. Additionally, Future Forgeworks, a steel manufacturer based in Brisbane, Australia, has commissioned SMS group to supply the nation’s first continuous mill technology (CMT® 350) mill. Future Forgeworks’ landmark project, the Swanbank Green Steel Mill Project, will produce rebar steel in an endless process for the Australian company, guaranteeing low carbon emissions and highly efficient production. 
  2. Piper Industrial Manufacturing Company, a Piper Aircraft, Inc., subsidiary, has acquired a Flexform™ fluid cell press from Quintus Technologies, expanding its equipment inventory to target the growing demand for low volume, high-complexity sheet metal forming. The company provides turnkey world-class manufacturing solutions.
  3. Steel producer Colakoğlu Metalurji AS, has placed an order with SMS group for the modernization of the laminar cooling section and the downcoiler in its 1,850-millimeter hot strip mill. With the completion of the laminar cooling system upgrade, the Turkish company plans to enter the market for wear-resistant steel grades. Additionally, Fujian Kebao Metal Products Co., Ltd., a subsidiary of Fujian Sanbao Group, has contracted with SMS for two tinplate continuous annealing lines (TIN CALs).
  4. A heat and energy management company that produces approximately 2 million complex parts per year has expanded with a custom-made VAB furnace for vacuum aluminum brazing. SECO/WARWICK has delivered the furnace to the company, located in the Czech Republic.
  5. Aluminum and renewable energy company Hydro has decided to invest in a new sow casting line at Husnes to increase its primary aluminum casthouse flexibility. The company’s primary plant produces low-carbon extrusion ingot for the European construction and automotive industries. The sow caster, which will have a capacity of 100,000 tonnes per year, will give flexibility to produce sow ingots in periods of lower demand for the plant’s main products.
  6. Secat, Inc., recently announced the addition of the Alubin extrusion press to its Nicholasville Pilot Lab. The press was donated by Wagstaff, Inc., which manufactures direct chill aluminum casting systems. This equipment will elevate the company’s testing, development, and small-scale production capabilities.
  7. Tenova will supply a new hot dip galvanizing line for PT Tata Metal Indonesia. The flexibility of the new line for zinc aluminum magnesium alloys will enable production of three types of coated coils.

Company & Personnel

  1. Can-Eng Furnaces International, Ltd. has announced the promotion of two long-standing employees to new leadership roles in 2025. Jason Clay has been promoted to manufacturing operations manager, overseeing the future direction of the company’s manufacturing strategies. Adam DeCiccio has been promoted to purchasing and logistics manager and will focus on implementing innovative strategies and improvements within purchasing, supply chain, and inventory planning to support company growth.
  2. thyssenkrupp Aerospace, a logistics service provider for the commercial aerospace industry, and aluminum manufacturer Novelis have renewed their strategic partnership through a multi-year agreement.
  3. Kolene Corporation recently announced the promotions of Timothy D. Shoemaker and Peter L. Shoemaker, both to co-chief operating officers for the corporation. Tim Shoemaker is responsible for sales and has oversight of the company’s engineering, field service, and project management departments. Peter Shoemaker continues to lead the company’s chemical supply chain and order fulfillment departments, as well as its critical replacement parts revenue segment.
  4. Gasbarre‘s new 150,000-square-foot facility in St. Marys, Pennsylvania, recently became fully operational, with expanded floor space, upgraded infrastructure, and state-of-the-art equipment.
  5. JSW Steel Dolvi Works has selected SMS group for a major expansion of its steelmaking facility, increasing the annual capacity of the existing steel mill by 3.7 million tons per year.
  6. Watlow, a provider of industrial technology and thermal systems, recently expanded its executive leadership team by appointing two regional presidents to oversee operations in Asia and Europe. Shiyi Zhou will serve as regional president of Asia, and Klaus Aarestrupp as regional president over Europe.
  7. Ipsen announced the 2025 schedule for its comprehensive training course on vacuum furnace equipment. Ipsen U will take place on April 1-3, June 10-12, August 12-14, and October 7-9 in Cherry Valley, Illinois.
  8. CAN-ENG Furnaces International Ltd has formed a strategic partnership with Piotr Pelian, founder of Industrial Process Technology to expand its European presence.
  9. Hydro and Northvolt have signed an agreement where Hydro will acquire the remaining shares in the battery recycler Hydrovolt for NOK 78 million, increasing its ownership in Hydrovolt from 72 to 100 percent through this transaction. Hydrovolt is a raw materials company established in 2020 as a 50/50 joint venture between Hydro and Northvolt.

Kudos

  1. Solar Atmospheres, Inc. has been recognized as the industry leader in the Surface Treatment Services category of the 2024 Leadership in Medtech Awards.
  2. Phoenix Heat Treating has announced that their furnaces have received approvals from Pratt & Whitney and Bell Helicopter, increasing the company’s capacity to process orders that require specifically approved furnaces, ensuring compliance with stringent aerospace and defense standards.
  3. Steelhead Technologies recently announced the launch of the Tides of Steel Sweepstakes, in partnership with Calvary Industries. The contest offers an opportunity for job shops to win prizes that will accelerate 2025 growth and reward hard-working teams.
  4. The Otto Junker Foundation announced the winners of the Otto Junker Prize 2024, honoring outstanding academic achievements at the RWTH (Technical University of Aachen). The recipients are: Daniel Baggen, Moritz Diewald, Gerrit Ipers, and Jan Krusenbaum.
  5. Mark Thomason and John Blauser, both of Gasbarre, have received the 2025 Distinguished Service to Powder Metallurgy Award from the Metal Powder Industries Federation (MPIF). The award recognizes individuals who have dedicated at least 25 years to the powder metallurgy (PM) industry and made outstanding, long-term contributions that have earned the admiration of their peers.
  6. The inaugural class of field service engineers recently graduated from the Ipsen FSE Academy, a next-generation training program building on the foundation of the former Ipsen Corporate Academy. This revamped initiative reflects Ipsen’s ongoing commitment to developing top-tier talent. These engineers successfully completed an intensive 20-week training program focused on mastering the complexities of heat treatment furnace repair and service

Find Heat Treating Products And Services When You Search On Heat Treat Buyers Guide.Com

22 News Chatter To Keep You Current Read More »

Heat Treat Radio #85: Salt Bath Heat Treating with Kolene Corporation

Heat Treat Radio host and Heat Treat Today publisher, Doug Glenn, is bringing us to the world of salt bath heat treating. To take on what this is and why heat treaters should consider this method, Doug is joined by three gentlemen with Kolene Corporation: Dennis McCardle, Ken Minoletti, and Jay Mistry.

Below, you can watch the video, listen to the podcast by clicking on the audio play button, or read an edited transcript.




The following transcript has been edited for your reading enjoyment.

Doug Glenn (DG): Well, welcome everyone to another episode of Heat Treat Radio. I’m really excited today to be talking about salt bath heat treating with the good people at Kolene Corporation. Let me introduce the folks and then we’ll get rolling.

Contact us with your Reader Feedback!

First off, gentlemen, welcome to Heat Treat Radio, I’m really glad to have you. The first person I would like to introduce is Ken Minoletti who is vice president of Thermal Processing at Upton Industry, now a Kolene Corporation company. Ken has 45 years of experience in all areas of the company operations relating to the design and manufacture of salt bath furnace systems and other thermal processing systems. When Kolene purchased Upton in 2021, retaining Ken was a critical part of the terms of the sale. He’s an expert in the field and well respected in the industry. I have known Ken for many, many years. Ken, it’s really good to be visiting with you today.

Kenneth Minoletti
VP of Thermal Processing
Upton Industries, Inc. - a Kolene Company

Ken Minoletti (KM):  Thank you for the invitation, Doug.

DG:  The next person is Dennis McCardle. He is the executive VP of Kolene Corporation and has 34 years of experience at Kolene in all aspects of salt bath manufacturing and operation. As executive VP, he is very well respected and considered an expert in salt bath technologies for industry, serving hundreds of customers. Dennis, welcome, it’s really good to see you. I’ve known you for many years as well.

Dennis McCardle (DM):  Thank you, Doug.

DG:  And finally, last but not least by any stretch: Jay Mistry, senior sales representative of heat-treating chemicals at Kolene and Upton. Jay came to Kolene in 2001, as well, with 33 years of experience at Park Thermal International as their former CEO. Jay is a high-energy, forward thinker, which I can attest. He cultivates and maintains strong industry relationships as the head of Kolene’s heat treat chemical sales. Jay is a wealth of important historical information and ideas.

So, there you go. Gentlemen, you sound good to me already!

We were talking before we hit the record button that when I read these bios, I said, “Boy, we sound good.” Fortunately, we can say, those are true. It’s really good to have you guys.

We want to talk about salt bath heat treat a bit. Just for the listeners, I want to lay out a bit of an outline. What we’re going to do is we’re going to talk a bit about Kolene Corporation first because there’s been some pretty significant activity at Kolene. We’re going to talk to Dennis about that for a minute. Then, we’re going to talk about the equipment -- salt bath equipment; we’re going to talk to Ken mostly about that. Then, we’re going to talk about materials.

I want to talk to you a bit about Kolene. There is a lot of activity over there.

DM:  There’s a lot of activity. We’re very excited.

DG:  Tell us a bit about the history, first, very briefly.

Dennis McCardle
Executive Vice President
Kolene Corporation

DM:   Sure, my pleasure. Kolene Corporation was founded in 1939. We’re a privately held, small business in Detroit. We’re a single-source supplier of process equipment, process chemistries, technical service and support, R & D, development, lab support services, engineering design capabilities -- I mean, we’ve got basically the whole gamut of supply chain.

Our processes are used in a wide variety of industries, Doug, so it’s really hard to go into them all. But typically, the difficult metal cleaning applications is where we’ve made our bones.

Then, when you look at it in 2021, we entered the heat treat marketplace with the acquisition of Upton Industries. It is a renowned name in the heat-treating industry, of both supplier of equipment but also technologies. We also, at the same time, took on the industry-proven chemistries of Park Thermal International. Those chemistries are really the lifeblood of what we’re going to be doing in the heat treat industry.

We’re very excited about the future and what we see coming along. When you think about it, both Ken and I were talking, and now, with the combined companies, we have 170 years of salt bath experience. It’s unbelievable synergy that we bring to our company now. It’s really exciting.

DG:  That is exciting. I want to be clear on before the acquisition of Upton and things of that sort. What were the core markets that you guys were serving? You mentioned it was metal cleaning?

DM:  Metal cleaning, yes. When you look at it traditionally, when we were initially founded, we were doing cast iron cleaning for the navy. We still do that process that was developed in the forties. When you look at it, steel, of course, to scaling, is the largest portion of our business. We also are in the engine remanufacturing sector, the aerospace sector. We’ve got a great deal of breadth, if you will, of the different industries that we supply our cleaning technologies too.

DG:  The company has been around a long time. You mentioned Upton as being a well-established name. I have been in the industry a long time; I’ve heard of Kolene for quite a long time, even in the thermal processing industry, heat treat industry, if you will. You guys have been around.

DM:  We have, yes.

DG: Before we move on to Ken and ask him some questions about the equipment, specifically, I’m curious -- and I’m sure many people out there would like to know -- What is driving this? You’ve acquired two companies, basically. What’s behind it? It sounds like you’re on a growth mode.

DM:  We are. We’re a family-held company. We’re in our fourth generation now. We have always looked at that sector, the heat treat sector, as an opportunity. Obviously, when we were doing the salt bath nitriding, we touched on it a bit, but we really didn’t get into it as we wanted to see and experience. When we looked at it, it was always in the back of our minds, should we enter that marketplace?, It was one of the owner’s sons, Tim Shoemaker, who really started making the inroads of -- Why don’t we go after this? Why don’t we look at this more seriously? He was the driving influence along with his brother, Peter, to move into this. The opportunity arose. Everything fell together just beautifully at the right time, place, and it just worked out fantastic.

DG:  Let me transition over to Ken because I want to just kind of piggyback on that. Dennis, thank you very much. I want to talk to Ken just a minute about the whole acquisition -- Upton becoming a part of Kolene. Can you give us a quick overview of how that happened?

Peter Shoemaker
Vice President of Purchasing
Kolene
Source: PRNewsWire

KM:  Sure. Obviously, everybody looks to continue the longevity of the corporation as we proceed. We’re all not getting any younger! Upton was started in 1937, so we were two years ahead of Kolene Corporation. It had always appeared, in my opinion, to be a very good fit. They are parallel lines of salt bath treatment. We actually competed against Kolene for a number of years, primarily, but we found our mainstay to be in the heat treat industry when it came to thermal processing. The passing of the president of our company opened up the potential for the merger or acquisition, and it worked out very well. We worked with the Shoemaker family and came to an agreement back in October. So, we’re really completing our first year from October of 2021. We’re one year into our leadership as a Kolene company. But they said they understand the importance of the brand name of Upton and, obviously, that will not be going away.

DM:  It is a key point. That name is really very important to us in the branding. It’s something we don’t ever want to lose.

DG:  Both those companies are very good names in the industry -- Park Thermal International and Upton.

So, Ken, Upton has been located where?

KM:  We’re in suburban Detroit in Roseville. We’re probably about a half hour drive door-to-door with the Detroit campus.

DG:  Is that location going to stay, or are you going to consolidate?

KM:  We’re going to stay, yes.

DG:  Let’s talk about the salt bath equipment. A lot of the people who listen to this are manufacturers who have their own in-house heat treat. I’m guessing a large portion of them have stuff that’s not salt bath, although I’m quite sure there are some that do. Talk to those people who don’t have salt baths at this point. Why should they be considering salt bath equipment?

KM:  Some of the big advantages, number one is temperature uniformity (+/-5 degrees Fahrenheit), being a conductive liquid, meeting the spec of AMS2750. Plus, its variables -- you can really run multiple differing grades of materials through the furnace merely buying limited by the operating temperature range of the salts. You run carbon steels, alloys. It’s a simple operation -- there are no generators, there is no carbon balancing for an atmosphere, so you don’t decarb. You rectify the bath to maintain pH, and that will prevent decarburization.

DG:  How about the different processes that can be run? In a salt bath, what are the different processes that can be run?

KM:  Our core business is neutral hardening. Austempering, marquenching and tempering, be it in salt or oil, aluminum solution treating for the aircraft industry, and also aluminum dip brazing. We’re becoming the worldwide leader in the supply of dip brazing equipment. and we have really opened up in the international markets. Again, it’s that temperature uniformity aspect of the equipment.

One sector that’s been taking off is the processing of Nitinol material for the medical industry. Again, uniformity. Molten salt heat transfer systems where the salt bath is generating, obviously, going to discharge into other equipment for heating practices.

A final one that’s unique is ion-exchange glass hardening. Cellphones. It provides for the transfer in the atomic structure of the potassium element into the glass, Gorilla Glass. We’ve talked over the years with quite a few manufacturers. It’s a little bit of a niche market, but it is beginning to expand.

Jeep® introduces Corning® Gorilla® Glass option for Wrangler and Gladiator windshields
Source: CORNING

DG:  That’s interesting! I’ve heard a lot about the processing of Gorilla Glass. I didn’t realize that some of that is done in salt.

KM:  Along with aircraft windshields and a whole myriad of glass products that can be done in a molten salt bath furnace.

That’s kind of our core industry of what thermal processes we utilize.

DG:  I want to come back to the dip braze, for a second. In dip braze, typically what type of materials are we brazing together? Is it a copper braze? How does it work?

KM:  It’s strictly aluminum. A furnace that will run within the salt range, I believe it’s about 1170-1200 Fahrenheit. It’s 61-grade of aluminum. It goes through extensive cleaning practice. You’ll preheat gradually for no distortion. You’ll have your fillermetals in place; it’s textured on the product. They’ll dip braze usually within 45 seconds. The filler metal melts. It’s removed; it’s either air-cooled, fog or immersion quenched.

DG:  Is that the type of brazing that takes place, like with clad material? Are you talking about heat exchangers and things of that sort?

KM:  I’m talking about heat exchangers. We’re talking about wave guides, antenna, any number of products, primarily into the communications, satellite, aerospace industries.

DG:  Typically, those braze processes, the temperature tolerances have got to be within 5 degrees because otherwise you start melting down either your base or your fins or whatever.

KM:  Yes. The criticality of brazing in the aerospace industry is definitely one advantage that molten salts have.

DG:  One last question for you, Ken, well actually two. The materials that you’re processing -- did we hit on that already?

KM:  In neutral hardening, it can be medium to high-grade carbon steels, alloys. Obviously, the aluminum, the Nitinol materials, stainless steels somewhat. Again, you’re really only limited by the temperature operating range of the bath. You can run tool steels to 150 degrees.

DG:  One last question I’ve got for you on this is:  In your experience, you’ve probably seen ebbs and flows as far as interest in salt bath heat treating. Where are we on that spectrum right now? Are we at the peak, are we growing, where are we?

KM:  I think we’re still growing. Again, one of the avenues is the aerospace -- aluminum dip brazing. Neutral hardening, the advantage of the conductive heating in a liquid, you can heat material up. Kind of a rule of thumb is 3-4 times faster than you can in an atmosphere furnace. If you’re able to heat up more quickly, it will reduce the size of the equipment. Plant floor spaces are always at a high commodity opposed to a potential continuous atmosphere line. It can be run by a single operator, delivering a rack of lawnmower blades every 8 minutes. You’ll offload 120 lawnmower blades.  It is very, very high-volume production.

DG:  Jay, I want to jump over to you with a few questions. Materials in salts and things of that sort, I’m probably going to ask you the most difficult questions. When we deal with salts, I know immediately most peoples’ minds go to -- “Uh oh, salts, I’ve got to be careful.” Let’s talk about that for just a little bit. Are there any types of new materials, if you will, new media out there that people should know about, new salts or things of that sort?

Jay Mistry
Senior Sales Representative - Heat Treat Chemicals
Kolene Corporation /Upton Industries, Inc.

Jay Mistry (JM):  The salt products have not really changed very much over the years. You have your standard neutral salts and the quench salts. They haven’t changed a whole lot over the decades. That is good for all the customers using the product because they want that continuity.

The most difficult sell to a customer is when you start changing salts. That seems to create some problems because the specs have already been established for what type of salts to use. When you start playing with the formulations and things like that, that discourages a lot of customers from trying new things. A lot of them are aerospace-based, automotive-based, and they need to get the approvals from those sources before they make any of those changes. So, you tend to maintain those salts with very little changes.

DG:  And I assume, the reason they’re given those specs -- let’s say they’re aerospace specs or whatever -- is because they want to be sure that the salts are cleaned off, that the salts have the same properties during the thermal process, that they’re able to be cleaned off as well, is that right? Is there anything else that is of concern?

JM:  100%. Salt maintenance in the salt bath, desludging in the case of brazing salts, sheeting -- all of those things are crucial to maintaining a good salt bath system, achieving temperature uniformity, and getting excellent results. All of those things go hand in hand, for sure.

DG:  The other question I’ve got for you is a supply chain question. We’re recording this the last day of September (2022) and supply chains are messed up, let’s just say.

ALL:  They’re challenged. They’re totally challenged.

DG:  How about on salts, Jay -- are we having any supply chain issues?

JM:  We still have challenges and so on in terms of raw materials but Pete Shoemaker and his group have done a fantastic job making sure that our needs are met. Deliveries sometimes alter based on deliveries of raw materials, but we still continue.

Costs are difficult to hold at any given time; they are everchanging. We spend a lot of time with our customers to try and explain the changes in costs. Salt products have generally been very stable, but today’s world has changed everything. As opposed to holding pricing for 3 months to 6 months, now you’re literally changing from an order to an order, and that’s difficult for a lot of our customers.

DG:  You and I were talking, about customers who might want to change suppliers. Let’s say somebody is having a supply chain issue with their current supplier and they want to come over and talk to Jay Mistry about buying salts from Kolene/Park Thermal International.

We discussed a little bit about the concern about mixing salts. Can you address that a little bit? Are there any concerns there we need to worry about?

JM:  Going back earlier when I mentioned that not much has changed in the salt products, per se, and that’s in line with in keeping with the salt supplies that we have with the current customers.

To answer your question, the formulations are essentially the same from one product to the other, and so customers really have nothing to worry about blending one salt to the other. In fact, it’s to their advantage to have a secondary source or alternate sources because of supply chain issues. But a lot of them have concerns. They don’t have a chemical background, so there is always the hesitation changing formulations and so on. But we can match any salt product that’s out there, and our clients would be able to use it without any interruption.

DG:  Even if there was a question and they’d like validation, I assume you guys could probably do some sort of chemical analysis of their salts and verify that there’s going to be no problem, if necessary.

JM:  Absolutely. We have a full lab here that we could do salt analysis. In fact, we provide a service for quarterly analysis and maintenance and so on.

DG:  Salts are hazardous, Jay. How do you address that? When I hear of salts, I automatically think, “Oh, boy, the EPA is going to be knocking at my door.”

JM:  There is no doubt -- they are a hazardous product. One has to be aware of proper handling, disposal issues, and so on. But I think with Ken’s group, our group at Kolene, we can educate the customer and help them through all of the regulatory processes and make them aware.

Handling the products, as Ken mentioned, is not very labor-intensive. Typically, one guy can run a salt line, type of thing. From a worker exposure, it’s minimized. The continuous lines that Ken’s facility provides, it’s always an enclosed system with the proper exhaust system. So, all of those effluents and emissions are taken care of and handled. We just spend extra time with new customers to make them feel comfortable with using salt products. Once they get the hang of it, I think most of them would say that their worries were unfounded.

DG:  Ken, do you agree? I mean, this is the handling of salts. Does the cost/benefit analysis of going to a salt line far outweigh the downside?

KM:  I think so. As Jay was talking about the discretional areas (maybe east coast/west coast as far as remediation), strict remediation is going to vary from locale to locale what your discharge requirements are. Out of the automated systems, we build strictly vent to atmosphere; there is no wet scrubber or any type of remediation on the fume. You will have metallic oxides in the disposal media from the bottom of the high heat pot; that always needs to be analyzed to determine what is the proper disposal method. Nitrate salts, any thermal process equipment company is going to be quenching in nitrates. We’re austempering, they’re austempering. It’s the common challenge of the industry, because it is the same equipment, same process.

DG:  Dennis, how about you? Any comments on this whole concept of the hazards of salts? I mean, you guys have been doing this for decades, right?

DM:  We’ve been doing it for decades, Doug, and we’ve, over time, optimized our systems and our processes to minimize any hazards or any potential risk. I mean, we take a great deal of pride in building a properly designed system that minimizes exposure, minimizes anything that could come along in the way of hazard. So, we’ve learned through the years how to do it, and we’ve gotten very good at doing it.

KM:  This also opens up an avenue for our Roseville campus -- we can rely on Detroit on given situations where we need to take a more critical look at remediation.

DG:  Focusing more on the heat treat side of things -- any interesting case studies that you can tell us about where somebody has either purchased equipment, purchased salts or whatever, that has just really been helpful to them?

KM:  With regard to processing salt -- repeatability. Your quench transfer, quench delay -- that is all PLC controlled. We use encoders, variable speed drives. Our Dan Murphy has done an excellent job in that capacity over the years. Again, it’s just everything can program into a PLC, everything is brought in by ethernet communication. We actually have a module that Dan uses which allows him onto their plant floor from our engineering department in Roseville. He can debug issues if programs are a problem.

DG:  A little Industry 4.0 or whatever we’re calling it.

JM:  One of the things to remember in the salt, when we talk about heat treat, and Ken mentioned Nitinol medical sources, we, at Park, went through a scenario with a customer that was having issues with his salt bath. We managed to help him clean the bath out and recharge it. But the interesting point with this customer was that he was producing the glass capsules that go into an EpiPen which is crucial for a lot of people out there. With the recent pandemic, all of the syringes, the billions of syringes used, that’s all heat treated in connection with what Ken was saying with glass tempering. And that’s a salt process that’s actually right out there for everybody to experience. Without the heat treating, the glass tempering, we wouldn’t be able to produce needles, EpiPens and things of that nature.

DG:  One last question:  You guys know your customers very well, much better than I do. If there was a single message you would want to throw out there to your customers/potential customers, what would it be? Dennis, if you don’t mind, we’ll start with you. What’s the message you want to leave with them here about salt bath?

DM:  I think salt baths, as you said, they can oftentimes bring a bit of trepidation in regards to whether I want to put a salt bath into my facility. But I think when you really set foot and talk with us about what we’re doing today, about the systems that we design today, I think you are really going to be put in a comfort zone when you see the efforts that we go through from a design and engineering standpoint, and all aspects of it. I mean, we take a great deal of pride in bringing not only the best system as is available, technology wise, but also in keeping people’s comfort levels at a good position through training. When we go and put a system in, we train people on how to operate it, how to work it safely. We take it very seriously when we put a system in making sure everyone fully understands the operation and fully understands that they can come to us at any time. We’re there 24/7 to take their questions and to help them and provide assistance. We try to be a one stop source for all of that.

DG:  I assume, also, Dennis, that if anyone out there has a question and just isn’t quite sure if they want to do salt, I assume there are probably places you can take them to show them some installed lines.

DM:  Absolutely. And that’s the sort of relationship that we have with our customers. Depending on the process, we can almost always get them to see a facility that’s operating a system today.

DG:  It’s always good when your customers let you back into the plant -- that’s a good sign!

Jay, how about you? Any last message? Then, Ken, we’ll finish up with you.

JM:  Just to follow-up on what Dennis said:  I think the biggest advantage all of our customers, or potential customers, would have is that we are the single source for anything related to equipment to process to operation to pump outs -- from start to finish. You make one phone call and we’re here to answer all of it. You don’t need to go to many various people. So, it truly is a one stop shop where you can get all your answers with one phone call.

DG:  Ken, how about you?

KM:  I agree 100% with Dennis and Jay. The only thing I would add is being allowed the opportunity to communicate with customers. Don’t dismiss something at face value just because the rumor mill is saying it’s nasty, you’re going to have hazardous waste and everything else. Allow us to present the advantages of the equipment. I think a lot of times that opens a lot of eyes. Everybody thinks of the old salt pot furnace with salt over the floor. That’s not the issue anymore. They’re automated, enclosed, they’re ventilated, and limited operator access. There are advantages.

DG:  Gotcha. So, basically don’t believe the questions I was asking about the nastiness of salts. I threw that out there just as devil’s advocate. I do think that’s probably a great point to conclude on is that, listen, if you have thoughts from the past, ideas and perceptions from the past of salt bath, let’s not limit to that. At least give it a shot.

DM:  Come and see us. Come and ask us. Let us show you what we’re doing today. It’s a remarkable advancement from what we had 80 years ago.

KM:  As Dennis said, we can use a referral to a customer, we can do site visits. Upton Roseville has always been the advantage we have a very good customer base. We always had the dialogue to be able to bring potential Upton customers in to take a look.

DG:  Well, it sounds to me, gentlemen, like Kolene/Upton/Park Thermal is on the upswing. I congratulate you. I congratulate you guys and look forward to talking with you again. Thanks for your time, today, I really appreciate it.

Doug Glenn <br> Publisher <br> Heat Treat Today

Doug Glenn
Publisher
Heat Treat Today


To find other Heat Treat Radio episodes, go to www.heattreattoday.com/radio .


.

Search heat treat equipment and service providers on Heat Treat Buyers Guide.com


 

Heat Treat Radio #85: Salt Bath Heat Treating with Kolene Corporation Read More »

Upton Industries Acquired by Kolene Corporation

HTD Size-PR LogoHeat treat solution manufacturer in Roseville, MI has been acquired by Kolene Corporation, a global leader of custom-designed and engineered molten salt bath equipment and specialty chemical formulations.

Upton Industries, Inc.

"We are proud to carry on Upton's strong brand and legacy as a part of Kolene Corporation as we move forward," commented Roger L. Shoemaker, chairman & CEO of the company.

Founded in 1937, Upton Industries, Inc. design and manufacture thermal processing systems in the metal heat treating industry. They apply their Engineered Thermal Solutions methodology to heat treat equipment including box type, car bottom, lift-off and specialty furnaces that utilize either electric heating or gas-fired systems.

Kolene will maintain both its Detroit headquarters location and the Upton Roseville location, which will be home to all Kolene’s manufacturing and fabrication. Bringing the two companies together will give the new company 50,000 sq. ft. of manufacturing, fabrication, and commercial processing capabilities.

W. Scott Schilling
President
Kolene Corporation

"After thoroughly evaluating Upton’s capabilities," said W. Scott Schilling, president of Kolene, "it was apparent that there are tremendous synergies between the two companies. Capitalizing on these synergies will allow [the company] to expand into applications and revenue segments where we have not historically been. [We] will also have the ability to become more vertically integrated due to Upton’s manufacturing and fabrications capabilities, which will allow us to strengthen our overall margins."

In its 82nd year, Detroit-based Kolene Corporation provides custom-designed and engineered equipment, specialized chemical formulations, and processes for cleaning and conditioning metal surfaces. Currently, their products are used worldwide for casting cleaning, alloy descaling, coatings removal, engine rebuild and other demanding automotive, industrial, and military applications.

Upton Industries Acquired by Kolene Corporation Read More »