Nitriding
Nitriding heat treatment is one of several surface hardening heat treat processes. Nitriding diffuses nitrogen into the surface of certain metals creating a hard surface more resistant to wear and corrosion. Low-carbon, low-alloy steels are often nitrided but it is also possible to nitride titanium, moly, aluminum and some medium and high-carbon steels. Most often, high-wear parts like gears, crank- and camshafts are nitride. Extrusion or forging dies are also frequently nitrided. Other hardening heat treatments competitive with nitriding are carburizing, nitrocarburizing and ferritic nitrocarburizing (FNC).
Nitriding Technical Content
Heat Treat Radio #137: Gas, Plasma, or Salt Bath? Making the Right Nitriding Choice
In this episode of Heat Treat Radio, host Heather Falcone sits down with Dan Herring and Dr. Ed Roliński to explore how manufacturers can choose the ...
Nitriding Selection Guide: Gas, Plasma, or Salt Bath?
Nitriding offers a unique combination of surface hardness, wear resistance, fatigue performance, and dimensional stability, making it a preferred thermochemical treatment ...
Why Choose Gas Nitriding?
Among today's nitriding technologies, gas nitriding remains the most widely used process for enhancing surface hardness, wear resistance, and fatigue performance ...
Why Choose Plasma Nitriding?
As manufacturers look for greater control, precision, and flexibility in surface hardening, plasma nitriding has emerged as a versatile alternative to traditional ...
Why Choose Salt Bath Nitriding?
For applications requiring exceptional wear resistance, corrosion protection, and rapid processing, salt bath nitriding continues to be a reliable surface engineering ...
Ask The Heat Treat Doctor®: Why and How Do We Heat Treat Gears? Part One
Ask The Heat Treat Doctor® has returned to bring sage advice to Heat Treat Today readers, answer questions about heat treating, brazing, sintering, ...
Anodic Plasma Nitriding of Titanium Alloys
In this Technical Tuesday installment, Dr. Edward Rolinski and Dan Herring, respectively known as "Doctor Glow" and The Heat Treat Doctor®, ...
Nitruración anódica por plasma de aleaciones de titanio
En esta entrega de Martes Técnico, el Dr. Edward Rolinski y Dan Herring, conocidos respectivamente como "Doctor Glow" y The Heat ...
Nitriding News
New Heat Treatment Cell Designed for Nitriding
A new modular heat treatment cell has been developed to handle nitriding, nitrocarburizing, carbonitriding, and dry oxidation, giving manufacturers the ability ...
Partnership Strengthens Regional Access to Nitriding Technologies
A new sales representation agreement will provide regional support for plasma nitriding, gas nitriding, and plasma coating technologies across six U.S. ...
Nitriding Furnace to Treat Aluminum Extrusion Dies
An aluminum profile manufacturer has ordered a gas nitriding furnace to treat extrusion dies, improving their wear resistance and extending service ...
Heat Treat Capacity Expands in Northern Mexico
Bodycote announced plans to open a new heat treatment facility in Apodaca, Mexico, expanding regional capacity for case hardening and nitriding ...
Large-Capacity Nitriding Furnace Enhances Processing Capabilities
Vacu-Braze, a commercial heat treater specializing in vacuum heat treating and brazing, has added a large-capacity nitriding furnace to support processing ...
Induction Hardening and Gas Nitriding Capacity Added at Alabama Plant
Advanced Heat Treat Corp. (AHT) has expanded induction hardening and gas nitriding capacity at its Cullman, Alabama facility, increasing throughput and ...
Spectrum Thermal Processing Expands Aerospace Reach
Spectrum Thermal Processing, a heat treatment provider based in Cranston, Rhode Island, has joined a broader thermal processing network through a ...
2 Large Scale Furnaces for Automotive and Marine Propulsion
Two intensive furnace projects are poised to bring heat treating to the automotive brake rotor and marine propulsion systems industries. An ...
NITREX (NTS & UPC) Acquired By Global Furnace Manufacturer Group
Breaking News: The NTS & UPC business divisions of NITREX, a manufacturer of industrial furnaces focused on nitriding solutions, will be ...
Michigan Heat Treater Completes Building Expansion
Advanced Heat Treat Corp. (AHT) has completed a building expansion at their Monroe, Michigan facility. The new 6,000 sq. ft. addition increases ...
Michigan Heat Treater Increases Gas Nitriding Capacity
Advanced Heat Treat Corp. (AHT) has increased operations at their Monroe, Michigan facility with additional gas nitriding equipment. Chad ClarkPlant ManagerAdvanced ...
AHT Expands Footprint and Nitriding Capacity
A North American nitriding company recently announced a building expansion to accommodate more equipment and services. The new production space at ...
Special Springs Enhances Production Capabilities with Nitriding System
Springs and gas cylinders manufacturer Special Springs has bolstered its heat treating capacity with a new nitriding turnkey system. By adding ...
Wrocław University of Science and Technology Enhances Metallurgy Research Capabilities with Nitriding System
Wrocław University of Science and Technology (WUST) is expanding its R&D capabilities in heat treatment and materials testing with a horizontal nitriding ...
Volkan Steels Expands Production Capabilities With Nitriding/Nitrocarburizing System
A tool supplier has boosted its production capabilities with the installation of a new nitriding/nitrocarburizing system, expanding its heat treatment services ...
Piston Rings Manufacturer Bolsters Production with 3rd Nitriding System
Asimco Shuanghuan Piston Ring Co., Ltd. has added a third nitriding system to its heat treating operations, enhancing piston ring production ...
Two Manufacturers Expand Operations With Nitriding Systems
Nitriding systems have expanded the operations at two global companies: a gear manufacturer for the automotive industry and a fuel injection ...
EV Chassis Production Expands With Retort Furnace
ev chassis production expands with retort furnace An international manufacturer of electric vehicles (EVs) is adding an advanced retort pit furnace ...