A firearms manufacturer based in the U.S. has ordered a vacuum heat treating furnace from a Pennsylvania manufacturer.
Solar Manufacturing Inc. announced the receipt of the heat treat furnace, a model HFL-5748-2IQ, which has a hot zone of 36” x 36” x 48” deep with a weight capacity of 5,000 lbs. Its maximum operating temperature is 2400°F and it heats to 2500°F for hot zone bake out. The furnace design also has a temperature uniformity of ±10°F and is AMS2750 compliant with vacuum levels in the low micron range.
For rapid turnaround for work cooling, a 100 HP gas blower is provided for operating at 15 PSIG (2-bar) in nitrogen gas. The furnace is complete with a SolarVac® Polaris fully automated and programmable industrial controls package, and a Eurotherm digital chart recorder.
The system also includes a Magnetic Specialties, Inc. SCR-based dry power supply rated at 225 kVa.
Firearm Image Photo Source: Jay Rembert at unsplash.com
Find heat treating products and services when you search on Heat Treat Buyers Guide.com