A leading Eastern European ammunition manufacturer expand their heat treat capabilities with a dual-chamber heat treating and temper furnace along with an oil quench tank. The equipment will play a supportive role in keeping key production equipment up-and-running with thermal processing of munitions projectiles.
The L&L Special Furnace Co., Inc. model QDS124 has two chambers: the top chamber rated to 2350°F is used for heat treating various steels and other non-ferrous materials. The bottom chamber, which is rated for 1250°F, includes a recirculation fan and baffle for tempering, stress relief, or pre-heating.
Shipped with the furnace was an accompanying QTO1224 oil quench tank. The quench tank has a working size of 12” high by 12” across by 24” deep and holds 65 gallons of oil. Included is a hinged safety lid, immersion-style heater with thermostat, and an agitator with explosion-proof motor for use with oil. The quench tank and furnace are NFPA86-compliant for safety.