A prominent aerospace company known for producing advanced, high-precision components for the global aviation and aerospace engine industry has been shipped a vacuum carburizing furnace. Headquartered in North America, the company’s aerospace division has been a trusted resource for the aeroengine sector for decades.

Source: Solar Manufacturing
To support the development of a specialized carburizing process, Solar Manufacturing partnered closely with the R&D team at its sister company, Solar Atmospheres, a heat treating affiliate. Collaborative testing was conducted at Solar Atmospheres’ Technology Center in Souderton, Pennsylvania, where engineers from both organizations worked together to fine-tune the process to meet the specific metallurgical specifications.
“This collaboration was invaluable in achieving the desired metallurgical results,” said Rick Jones, regional sales manager at Solar Manufacturing.
The delivered system features a graphite-insulated hot zone measuring 48” wide × 48” high × 60” deep, capable of reaching temperatures up to 2400°F (1370°C). The furnace can accommodate workloads up to 5,000 pounds and includes an internal gas cooling system that provides rapid 2-bar nitrogen quenching.
Press release is available in its original form here.