Austenitizing, Salt Quenching Processes Enhance Auto Supplier’s Heat Treating Capabilities

A Mexico-based automotive supplier recently awarded a contract for the design and manufacture of a 1,500 lb/hr mesh belt furnace system for the austenitizing and molten salt quenching of unique components used in the manufacture of its drivetrain systems.

This contract was awarded to Can-Eng Furnaces International Ltd, which has scheduled the project to be commissioned early 2018 in Mexico’s centralized automotive manufacturing corridor. Incorporating several technological advancements for continuous atmosphere processing of products requiring carbon diffusion and quenching via a molten salt system, known as austempering, the new system includes: automated bin-dumping loading, mesh belt atmosphere hardening furnace, salt quench, post-quench wash and rinse system, mesh belt temper oven, and endothermic gas generator.

 