Nippon Steel & Sumitomo Metal Make Titanium Fuel Tank for Honda CRF450R Motocrosser

BOTW-50w  Source:  Webike Moto News

This is the first time in the world that titanium sheet has been used as fuel tank material for a mass produced motorcycle.  Read more to find out the other features of the CRF450R.

Read More: Titanium Sheet Developed by Nippon Steel & Sumitomo Metal is Now Adopted to Fuel Tank on Honda DRF450R Motocrosser