Three heat treat systems have recently been delivered and commissioned to joint base San Antonio-Randolph for maintaining the T-38 Talon Trainer aircraft.

These systems are a dual chamber model DCAHT®-181248-1200/500-MIL, a DCAHT®-241672-1200/500-MIL, and a large single chamber SCAHT®-303048-1200-MIL.

USAF depot level heat treating requires full compliance to AMS2750G.  The heat treating systems provided by DELTA H were for replacing existing systems which were too troublesome or costly to try to qualify and were never designed for modern pyrometry standards. The furnace systems were placed into production service the week following qualifying and training.

JBSA-Randolph – SCAHT®-303048-1200-MIL & DCAHT®-241672-1200/500-MIL Includes Power Driven Quench Tank
Source: DELTA H

Richard Conway, director and CTO of DELTA H, states, "We are grateful and humbled to be recognized among the mission critical technology partners supporting this very important project, and pleased to play a part in extending the service life of the valuable T-38 airframe."

JBSA-Randolph, TX – DCAHT®-181248-1200/500-MIL Heat Treat Computer Work Station
Source: DELTA H

Third party compliance and initial qualifying certification of all 5 chambers were provided by Conrad Kacsik Instrument Systems of Solon, Ohio.

Jake Kacsik, president of Conrad Kacsik Instrument Systems, shares, “The results are always impressive when testing DELTA H furnaces. By far the most reliable and consistent systems for maintaining the strict standards of aerospace pyrometry. Richard and I not only have a career-long professional relationship, but also, we both served in the USAF.”

DELTA H is exclusively represented worldwide by PHILLIPS FEDERAL Division for all military and government sales.

JBSA-Randolph, TX – SCAHT®-303048-1200-MIL & DCAHT®-181248-1200/500-MIL
Source: DELTA H

John Murray, retired SMSgt of USAF and product manager of Phillips Corporation, Federal Division added, “DELTA H compliments our product offerings to Metals Tech facilities. Regardless of traditional machining or additive manufacturing, Phillips Corporation – Federal Division strives to meet the needs of the USAF Fabrication Flight Warfighter, providing the best solutions for their support of US power projection and strategic deterrence. Phillips Corporation – Federal Division stands beside USAF Fabrication Flights around the globe ready to cut, fabricate, manufacture, and metallurgically process any part-anytime-anywhere."


Find heat treating products and services when you search on Heat Treat Buyers Guide.com


Skip to content