Effect of Heat Treatment on the Tensile Strength of ‘Elgiloy’ Orthodontic Wire

BOTW-50w  Source:  Dental Materials –

Elgiloy is the trade name of a cobalt–chromium–nickel superalloy that is offered for orthodontic use as wire. Despite some years of use, there is very little information in the dental literature on its mechanical properties, and especially on the effect of the hardening heat treatment (HT), that may be used after forming, on the tensile strength (TS) in relation to the four ‘tempers’ that are available.

Read More:  The Effect of Heat Treatment on the Tensile Strenght of “Elgiloy” Orthodontic Wires by S.M. Philip and B. W. Darvell