Two CAB Lines en route for Automotive Industry

A Scandinavian manufacturer of heat exchangers has purchased two CAB lines, which will be delivered to factories in Mexico and Poland. They will be used for brazing heat exchangers for trucks and buses as well as power generators. The deliveries will be synchronized to arrive to the factories in the same timeframe.

The order is being carried out by SECO/WARWICK Group’s Chinese branch. This partner has been operating globally since 2016, offering large-size heat exchangers for buses and trucks. The CAB lines on order meet the protective Nocolok® atmosphere aluminum brazing technology requirements.

Said Piotr Skarbiński, vice president of the Aluminum and CAB Products Segment at SECO/WARWICK, “This is a unique project for us, as we have sold two furnaces with the same delivery date to one customer at two different locations. It will be a logistical challenge overseen by SECO/WARWICK China.”