A heat treat furnace was recently shipped and installed at commercial heat treat facility in Eastern PA. The equipment will expand the company's vacuum heat treat and gas quench capabilities.

Solar Manufacturing recently delivered a Mentor® vacuum furnace. The furnace has stainless steel chamber, a work zone of 12” x 12” x 18” deep, and a maximum operating temperature of 2400°F with a workload capacity of 250 pounds. The furnace includes a VHS 6” diffusion pump for vacuum performance in the 10-6 Torr range, a 7.5HP fan motor for internal gas quenching up to 15PSIG (2-bar), and the SolarVac® fully automated and programmable controls package with a Eurotherm digital recorder.