A specialty tungsten alloy products manufacturer in the eastern United States will receive a high temperature pusher furnace.
The furnace, from Gasbarre Thermal Processing Systems, is designed for high temperature sintering with operating temperature capabilities up to 2750°F (1510°C). The system is electrically heated using molybdenum elements and utilizes the latest in refractory materials for efficient operation.
The pusher system processes trays 8” wide x 12” long under 100% hydrogen atmosphere and includes an automated return conveyor for effective loading and unloading.
Gasbarre was selected as the equipment provider based on their knowledge of high temperature sintering and ability to service and support the client.