ALLOY FABRICATIONS NEWS

Endothermic Gas Generator Added to Brazilian Fastener Heat Treatment System

A major fastener manufacturer in South America recently received delivery of an endothermic gas generator intended for heat treatment operations at the company’s Brazilian plant.

Jomarca, a Brazilian producer of fasteners for the furniture, tooling, construction, and do-it-yourself markets, purchased the Atmosphere Engineering™ EndoFlex™ generator from United Process Controls (UPC) in reaction to doubled carburizing operations and increased production capacity. Carburizing operations now include ten large continuous rotary retort furnaces that process over 2200 US tons (2,000,000 kg) of fasteners a month.

The high-capacity generator was integrated into the plant’s existing gas distribution system in the first quarter of 2018 and is supplying endothermic gas to all carburizing furnaces. The EndoFlex operates at a lower cost and mixes to more accurate ratios, aimed at maintaining a constant furnace atmosphere and a consistent gas quality at all times. The enhanced control capabilities of the EndoFlex allow for continuous control and monitoring of CH4, dew point, differential pressure, gas temperature, and retort burnout, as well as data logging, which is critical for troubleshooting and meeting regulatory requirements.

Mr. Eric Jossart (Sales Director, UPC USA), Mr. João Marques Castelhano (President, Jomarca), and Marcio Torres Boragini (General Manager, UPC Brazil). In the background is an Atmosphere Engineering™ EndoFlex™ endothermic gas generator installed at Brazilian fastener manufacturer Jomarca

Endothermic Gas Generator Added to Brazilian Fastener Heat Treatment System Read More »

Alcoa Unveils Four New Specialty Alloys

BOTW-50w Source: Alcoa

“Lightweight, high-performance metals leader Alcoa (NYSE:AA) today launched a family of innovative foundry alloys designed to meet the growing need for both part performance and lightweighting in the automotive industry and beyond.”

Read More: Alcoa Launches Four New Specialty Alloys that Deliver Lightweight, High-performance Solutions to Meet Growing Automotive Demand

Alcoa Unveils Four New Specialty Alloys Read More »