In-House Heat Treatment Process Works Too Well

BOTW-75w Source:  Today’s Motor Vehicles

“We developed our own hot-stamping process to be cost competitive,” says Elie Mordovanaki, general manager of operations and engineering for Merit Technologies Worldwide, GNS America’s hot-stamping division. “However, mechanical trimming is not optimal after the heat treating process takes place.”

Read More:  Laser Cutting Supports Hot Stamping