How are Vacuum Furnaces Used for Minting Coins?

Source: TAV VACUUM FURNACES

How does coin production benefit from vacuum heat treating? Is hardening, tempering, and machining required?

In this Best of the Web, take a look at what it takes to create “the master die” and the importance of vacuum heat treating in the minting process. The article offers a few contextualizing points around the topics of green energy and maintaining a safe workplace.

An excerpt:

[blockquote author=”TAV VACUUM FURNACES” style=”1″]The master die is then hardened and tempered to produce a positive tool called hob. Note that the master die is not used to produce coins. What do we need to produce our first coin?[/blockquote]

 

Read more at “Minting Industry: The Importance of Vacuum Heat Treatments”

 

 

 

 

 

All images sourced from TAV VACUUM TECHNOLOGIES.