The Properties of Titans vs. Poor Tribological Performance

Source: Advanced Heat Treat, Corp.

There seems to be no limit to what heat treated titanium alloy products can do -- just listen to the name: "titans." However, its poor tribological performance means that a surface treatment is necessary in most applications.

This best of the web article shares a quick technical run-down of all you need to know about plasma/ion nitriding of titanium alloy products with guidelines and graphs to show you the way.

An excerpt:

At the moment, nitriding is the most common and rational diffusion treatment which can be used for all-over surface hardening of titanium products. Nitrided titanium has a gold/yellow color of the TiN nitride enhancing attractiveness of the treatment in many applications.

Read more at "Plasma / Ion Nitriding of Titanium Alloy Products for Enhancing Their Tribological and Anticorrosion Properties"


Find heat treating products and services when you search onĀ Heat Treat Buyers Guide.com


 