United States Air Force in UK Receives Aerospace Furnace and Heat Treat Training

HTD Size-PR LogoUnited States Air Force personnel stationed at Royal Air Force (RAF) Base Mildenhall in the United Kingdom recently commissioned and received full training on the use and maintenance of a heat treating furnace for aerospace parts. The furnace will help maintain KC-135, CV-22, C-130 aircraft, and F-15 fighter jets assigned to RAF Mildenhall or nearby RAF Lakenheath air stations. The installation was interrupted by an impromptu visit from the U.S. President.

Richard Conway
Chief Technology Officer
Delta H Technologies

The DELTA H® TECHNOLOGIES dual chamber heat treating furnace for aerospace (DCAHT®) was designed by the supplier to rapidly heat treat all common aviation grade metals and alloys necessary for aircraft maintenance and is fully compliant with USAF/NAVAIR Tech Order 1-1A-9 and SAE-AMS2750F. The training received by the USAF airmen at RAF Mildenhall included essential instructions in heat treating, as well as furnace calibration practices like temperature uniformity surveys (TUS) and system accuracy tests (SAT) and culminated with each airman receiving Certificates of Training.

The specialized furnace features an upper chamber convection system, 18" wide x 12" high x 48" deep, capable of Class 1 (+/-5°F) from 200°F to 1200°F and a lower chamber radiant heat system, 12" wide x 12" high x 36" deep, capable of Class 3 (+/-15°F) from 1000°F to 2000°F with air or argon atmosphere. A roll-away quench tank features dual baths for water and oil quenchant. The controls and data acquisition provide detailed batch records of heat treated parts, including quench delay, as well as automatic tracking of thermocouple usage and calibration intervals.

Air Force One at RAF Mildenhall

The training was interrupted by an unexpected visitor to RAF Mildenhall. The hangar next to the Metals Tech Shop, where the furnace was being commissioned and the training was being conducted, was the epicenter for the arrival of a top-secret VIP. When the Air Force Band began practicing "Hail to the Chief," it became obvious that U.S. President Joe Biden would be making an unexpected visit to the base. While the President’s visit was not related to the furnace commissioning, Richard Conway, DELTA H® founder and chief technology officer, and wife Mary Conway, witnessed this presidential visit and got a few candid photographs of Air Force One (see above).

United States Air Force in UK Receives Aerospace Furnace and Heat Treat Training Read More »

Heat Treat Equipment Manufacturer Expands to Broaden Aerospace Supply

 

Source: Lancaster Eagle-Gazette

 

A heat treating equipment manufacturer based in Carroll, Ohio, recently announced plans to expand its facility and broaden its capability to produce furnaces for aerospace manufacturers equipping in-house heat treat operations.

Delta H Technologies LLC’s investments will cover the purchase of machinery and equipment for the design and production of furnaces for aerospace components. The expansion confirms the company’s nearly 30-year commitment to providing state-of-the-art heat treat equipment manufacturing to keep pace with the growth in aerospace technology and production.

“Richard Conway, director and chief technology officer, started the company in 1990 while attending Ohio State University to get his bachelors of science in industrial engineering. He did maintenance and tuning work for industrial furnaces and ovens.  . . . Richard’s wife, Mary Conway, is a retired teacher who taught honors chemistry and physics at Pickerington North High School. And she was the one who came up with the name Delta H as it is a math symbol for change of heat.”  ~ Lancaster Eagle-Gazette

 

Read more: “Delta H in Carroll To Double Workforce and Invest $300,000 in the County”

Heat Treat Equipment Manufacturer Expands to Broaden Aerospace Supply Read More »