Furnace Expansion for Portland Heat Treater
Stack Metallurgical Services has added a new furnace to their Portland facility. The furnace adds significant capacity for stress relieving, sub-annealing, and high-temperature annealing, under protective atmosphere.

The furnace has a working zone of 48″ W x 96″ L x 36″ H, it can handle up to 12,000 lbs, and is certified for temperatures up to 1650°F.
Jeff McLaughlin, owner of McLaughlin Furnace Group, was on-site to help commission the new equipment. Stack also partnered with Super Systems, Inc for charting, testing, and running simulated loads.

General Manager
Stack Metallurgical Group
“We are very happy to partner with McLaughlin Furnaces to add this new equipment to Stack’s Portland facility. We’ve always taken a proactive approach to expanding our capabilities and capacity to stay ahead of our clients’ evolving needs. I want to thank Jeff McLaughlin and his team for designing, building, and commissioning this equipment on schedule — it’s been a seamless collaboration,” shared Kimberly Chaussee, general manager at Stack Metallurgical Group.
Stack plans for other significant short-term and long-term investments in both equipment and facilities. They are anticipating additional major announcements later this year. These ongoing investments reflect their commitment to meeting the needs of their clients.
Find heat treating products and services when you search on Heat Treat Buyers Guide.Com