New Material Retains High Transmissivity After Heat Treatment, Applied to Optical Devices
Source: Phys.Org
Researchers at Toyohashi University of Technology have collaborated with their counterparts at Massachusetts Institute of Technology (MIT) to develop a new material capable of retaining high transmissivity after annealing at 850°C (1562°F). The results address the challenge manufacturers face when combining different materials that react differently to heat treatment at certain temperatures.
Read more: “High-Refractive-Index Material Retains High Transmissivity After Annealing at 850 Degrees C”