Global Auto Manufacturer Deploys Heat Treat System
A global manufacturer of automotive, power, and aerospace components has commissioned a new heat treat system. This system from SECO/WARWICK is the first furnace with LPC technology for this large Indian company.
This three-chamber vacuum furnace delivers economical case hardening using low-pressure carburizing (LPC) technology and oil quenching. It can replace existing lines and generators used for mass heat-treatment under protective atmosphere while ensuring higher precision and process repeatability. This solution stands out because of improved process quality, cost reduction from doubling yields, and increased production flexibility.

“Since our . . . furnace was the first LPC technology used in the client’s facility, we had to take a learning curve into account. We worked closely with the engineering staff of the client to ensure they understand and use the technology correctly, exploring all the possibilities, advantages, performance and optimizations it offers,” said Maciej Korecki, VP of Vacuum Business Segment at SECO/WARWICK.
“Successful implementation took time but paid off with much higher quality standards the company can now offer to their clients, who are currently operating on all continents. The client benefited from pre-sale consultation and post-sale installation as well as training assistance,” added Manoranjan Patra, Managing Director at SECO/WARWICK India.

Global Auto Manufacturer Deploys Heat Treat System Read More »