OWZ Ostalb received a new electrically heated endothermic gas generator. The company wanted to replace the old generator since it had no automatic process control and was unable to control the dew point efficiency in situations where the ambient air changed too much. The old components, which were difficult to replace, further reduced the generator’s overall efficiency.
OWZ Ostalb, a commercial heat treatment company in Aalen, Germany, received the EndoFlex™ S from UPC-Marathon, a Nitrex business unit, in late 2021.
"The customer chose us," says Daniel Panny, product manager at UPC-Marathon in Germany, "because we offered [a] gas mixing and control system, the EndoInjector™, and the [. . .] ReactionCore™ multi-retort system to deliver a reliable, on-demand supply of quality endogas, resulting in significant CO2 savings for their heat-treating operations."
The EndoFlex™ S that was purchased is the electrically heated version with an air cooler, an automatic nitrogen purge system, and additional CH4 monitoring to meet the highest safety standards.
Find heat treating products and services when you search on Heat Treat Buyers Guide.com