Rolls Royce Grants Approval

Rolls Royce has granted approval to Solar Atmospheres of Western Pennsylvania to conduct certain commercial aerospace heat treat processes. Rolls Royce requires strict specification requirements, strict process execution, and a daily commitment to quality processing from its suppliers in order for this to be granted.

Susan Generalovich, Quality Manager said: “The successful certification of our western Pennsylvania facility is a testament to our commitment to continual improvement, and to growing our business within the aerospace industry.  We are excited about the opportunities this certification will allow and the added confidence it provides to our customers.”

More information about Solar Atmosphere’s Quality Certifications: click here.