TPIM 2018 Promises Heat Treaters Technical Presentations and Keynotes from Industry Leaders

The ASM Heat Treating Society and IFHTSE are joining together to present “Thermal Processing in Motion, including the 4th International Conference on Heat Treatment and Surface Engineering in Automotive Applications” on June 5-7, 2018, in Spartanburg, South Carolina.

With more than 50 technical presentations, the conference will offer attendees many opportunities to learn the latest research and developments in their field during sessions focused on Advances in Thermal Processing, Additive Manufacturing, Phase Transformations, Microstructure/Property Relationships, Quenching and Quenchants, Thermomechanical Thermal Processing, Surface Hardening, and others. In addition, there will be keynote presentations from well-known industry leaders, including Rafael Colas, Joe Epperson, and Richard Sisson.

Click here for more information or to register: Thermal Processing in Motion.