New Vacuum Furnace for Michigan Heat Treater

HTD Size-PR Logo

The new transformer
Source: Solar Atmospheres

Solar Atmospheres of Michigan took delivery of a new vacuum furnace this week, which will be used primarily for aerospace applications. The Chesterfield, MI, location is set to begin heat treating later this year.

The furnace has a working hot zone of 36″ wide x 36″ high x 48″ deep and can handle workloads up to 5,000 lbs. To power this furnace along with nine other vacuum furnaces, a new 2600kVA transformer was installed. The new facility anticipates being fully operational by the fall of 2023 and will gather all of Solar Atmosphere’s Michigan heat treating under one roof.


Find heat treating products and services when you search on Heat Treat Buyers Guide.com