6 Vacuum Furnaces to Amp Up Precision Processing

HTD Size-PR LogoVacuum furnace manufacturer announced it is building six furnaces for various applications in the precision processing of metals in heat treating, brazing, and annealing applications.

The product line from which these furnaces will come from, Centorr Vacuum Industries Workhorse®, was introduced in the 1960’s and has been one of the company’s best-selling furnaces over the past six decades. Available in sizes from 1 cubic ft to over 100 cubic ft, this versatile furnace design has a refractory metal hot zone and high-vacuum pumping system for the processing of advanced materials requiring an extremely clean high-vacuum environment.

The furnace can also handle a variety of customer loads in either high-vacuum or partials pressures of inert gas, when necessary to protect the customer’s load.