A car radiator manufacturer has expanded its heat treatment capacity with an EV/CAB line adapted for the production of oversized battery coolers. The aluminum brazing furnace facilitates the ability to make quick modifications and switch from gas to electric heating in order to meet climate change challenges.

Vice President of Aluminum and CAB Products Segment
SECO/WARWICK
Source: LinkedIn
SECO/WARWICK designed the CAB line with temperature uniformity across the entire belt width in order to accommodate the size specifications of the battery coolers.
“This order is for an aluminum brazing furnace adapted to the production of oversized battery coolers,” said Piotr Skarbiński, vice president of the aluminum and CAB product segment at SECO/WARWICK. “The EV/CAB line with a belt width of 2100 mm (6.89 ft) is designed to produce oversized battery coolers. It consists of a preheating and main heating chamber, a radiation brazing furnace, an air jacket cooling chamber, a final cooling chamber and a control system.”
The press release is available in its original form here.