Titanium Processing News
Titanium Processing Capacity Expands with New Water Quench Furnace
Solar Atmospheres of Western PA is commissioning a new water quench furnace designed to solution anneal large titanium components, adding capacity ...
Vacuum Furnace Expands Titanium Castings Capacity
A British foundry technology center is adding a large-scale vacuum furnace to expand its annealing capabilities for oversized titanium castings used ...
Vacuum Arc Remelting Supports Aerospace Casting
A titanium casting manufacturer is expanding its vacuum melting capacity with the installation of a vacuum arc remelting consumable casting furnace, ...
Defense Funding Backs US Titanium Production
Federal funding will support expanded domestic production of titanium plate and large-format titanium components for defense applications, helping strengthen U.S. manufacturing ...
12-Foot Vacuum Furnace Expands Titanium Processing Capacity
Solar Atmospheres, a North American commercial heat treating company, has expanded its vacuum heat treating and titanium processing capabilities with the ...
Powder Metallurgy Press Strengthens Titanium Component Production
IperionX has commissioned new powder metallurgy equipment to expand U.S. titanium component manufacturing capacity, supporting the production of near-net-shape parts for ...
Heat Treating Supports Aerospace Components for Artemis II Mission
Solar Atmospheres has provided thermal processing services for materials and components used in the Artemis II mission, supporting aerospace applications that ...
IperionX To Produce Titanium Components for Military Vehicles
IperionX has received a prototype order for lightweight titanium components intended for U.S. Army heavy ground combat systems. The order directly ...
Accelerated Titanium Component Production Targets Naval Shipbuilding Bottlenecks
IperionX continues to advance domestic titanium manufacturing and thermal processing capabilities in a recent commitment to reduce long lead times for ...
IperionX Receives $25M to Accelerate Titanium Production
Iperion X has received $25 million from the U.S. Department of War to support the build-out of a resilient, fully integrated, ...
Fringe Friday: Riverspan Partners Acquires United Titanium
We’re celebrating getting to the “fringe” of the weekend with a Heat Treat Fringe Friday installment: Riverspan Partners has acquired United Titanium, a leading ...
Batch Oven Shipped for Aerospace Exploration
An electrically heated batch oven has been shipped to a leading space exploration company. The custom batch oven will be used ...
IperionX To Receive $12.5 Million for Primary Titanium & Components
IperionX Limited will receive $12.5 million from the U.S. Department of Defense (DoD) to accelerate the scale-up of a resilient, low-cost, ...
ATI Expands Aerospace Agreement with Titanium Components
ATI Inc. and The Boeing Company have expanded their agreement for high-performance titanium materials for aerospace. ATI will supply high-performance titanium ...
Titanium Drop Bottom Furnace To Be Installed
Following foundation preparations, Solar Atmospheres will be installing a new titanium drop bottom water quench furnace at their Hermitage, Pennsylvania, location. ...
Heat Treater Triples Surface Hardening Capacity at Ohio Facility
A heat treating company that processes stainless steel, titanium, and other specialty alloys is expanding its operations with a major investment ...
IperionX Delivers First Titanium Furnace Production Run
IperionX, a U.S. titanium metal and critical materials company, recently delivered its first successful titanium furnace production run at the company's ...
Titanium Production & Recycling To Increase for Aerospace Sector
EcoTitanium, a European plant for recycling and refining titanium alloys for critical applications, was opened in France in 2017. It was ...
IperionX and Vegas Fastener To Co-Produce Titanium Fasteners for US Army
IperionX Limited and Vegas Fastener Manufacturing, LLC (Vegas Fastener) have agreed to partner to develop and manufacture titanium alloy fasteners and ...
IperionX Titanium Furnace Set To Arrive in Virginia
HAMR titanium furnace for Virginia facility (Source: IperionX) IperionX announced their HAMR (Hydrogen Assisted Metallothermic Reduction) furnace has completed its final ...
IperionX Grows with New Virginia Titanium Facility
IperionX, a producer of high-quality titanium alloys, has commissioned a titanium production facility in Virginia. Anastasios (Taso) Arima, CEO of IperionX, ...
AM Supplier Delivers Components to GA-ASI
Nicholas Mayer President of Commericial Norsk Norsk Titanium, a global additive manufacturing supplier for aerospace-grade structural titanium components, announces delivery of ...
South Carolina Facility To Increase Titanium Processing Potential with Heat Treat Furnace
Solar Atmospheres has announced the order of a new 10-bar vacuum furnace for their Greenville, South Carolina, heat treat facility. This ...
Fringe Friday: Airbus Expands Capabilities with AM and 3D Printing
Sometimes our editors find items that are not exactly "heat treat" but do deal with interesting developments in one of our ...
Vacu-Braze Receives New Quenching Furnace for Specialty Aerospace Materials
Vacu-Braze recently installed a new water quenching furnace in their Quakertown, PA, facility. This acquisition will allow for the expansion of ...
Solar Atmospheres of Souderton, PA Adds Furnace for Titanium Reclamation
Solar Atmospheres Souderton, PA incorporated a high-production vacuum furnace with a work zone of 48"x48"x72" and a weight capacity of up ...
Aero and Turbine Heat Treat Expands for Titanium Steel Castings Manufacturer
A front-loading box furnace delivered to a northeastern U.S. supplier of titanium castings will expand the manufacturer's aerospace and gas turbine ...
Solar Atmospheres of Souderton, PA Adds Furnace for Titanium Reclamation
Solar Atmospheres Souderton, PA incorporated a high-production vacuum furnace with a work zone of 48"x48"x72" and a weight capacity of up ...
Specialty Metals, Vacuum Furnace Group Finalizes Acquisition of Titanium Producer
A global company that produces specialty metals and provides related vacuum heat treating equipment and services recently announced the acquisition of ...
Aerostructures Manufacturer Transitions Breakthrough Titanium Fabrication Technology from Lab to Factory
A manufacturer of aerostructures for both commercial and defense headquartered in Wichita, Kansas, recently announced it is transitioning recent research breakthroughs—a ...
Boeing’s Structural Applications Supplier Tests Additive Titanium Alloy for Performance
Building upon their collaboration begun last year, two aerospace titanium and alloy component suppliers recently concluded successful testing for optimizing alloy ...
Metal A.M. Solutions Provider Enters Initiative to Develop Processes for Titanium Alloys Aero Parts
A leading provider of metal additive manufacturing solutions recently announced that it has entered into an ambitious research and development (R&D) ...
Agreement Reached to Initiate Titanium 3D Printing for Boeing 787
A Wichita, Kansas-based, manufacturer of fabricated parts for the aerospace industry recently announced its partnership with the world's pioneering supplier of aerospace-grade, ...
“Titanium Man” Recognized for Developing Titanium Heat Treating Protocol
Source: Santa Monica Daily Press If there's one thing that can be determined by reading through the reasons ...
Swedish Group Invests in Titanium, Nickel-Based Metal Powders Production
Annika Roos, head of product area powder at Sandvik Materials Technology A Swedish engineering group in metal-cutting and materials technology recently ...
PA, Wash to See Increased Titanium Heat Treat Activity
Rich Harshman, ATI’s chairman, president, and CEO A Pennsylvania-based manufacturer of specialty materials and complex components predominantly for aerospace & defense industries ...
Scissors Maker Goes for the Gold with Titanium Coating
William Whiteley & Sons, the oldest scissor-makers in the western world, has chosen a UK-based company that specializes in hard coatings, ...
Titanium Producer Boosts Melt Capabilities with New Furnaces
Frank Perryman, president and chief executive officer of Perryman Company Perryman Company, a metal fabricator headquartered in Houston, Pennsylvania, recently announced it will ...
ATI and GE Aviation Announce Titanium JV
Allegheny Technologies Incorporated, a global leader in the production of technically advanced specialty materials and components, announced a joint venture (JV) ...
Aerospace Supplier Orders Titanium Rotary Hearth Forging Furnace
A leading North American aerospace supplier ordered a 36 ft. diameter pancake style rotary hearth furnace for the production of large ...
GE Purchases Titanium Alloy from Kobe Steel
Kobe Steel, Ltd. announces that it has begun supplying titanium alloy forged material for shafts to IHI Corporation. The forged material ...
Titanium Success
Source: Russian Aviation Insider Russia’s VSMPO-AVISMA Corporation, the world’s largest titanium producer, is successfully increasing the share of machining in ...
Nippon Steel & Sumitomo Metal Make Titanium Fuel Tank for Honda CRF450R Motocrosser
Source: Webike Moto News This is the first time in the world that titanium sheet has been used as fuel ...
Norsk Titanium to Build World’s First Industrial-Scale Aerospace Additive Manufacturing Plant in New York
State Releases First Funds for Signature Economic Development Project for Initial Lot of 20 Norsk Titanium MERKE IV™ Rapid Plasma Deposition™ ...
Norsk Titanium Achieves Aerospace Technology Readiness
OSLO – December 21, 2015 – Norsk Titanium AS announced today that the company has achieved Technology Readiness Level Eight (TRL ...
How Do They Do It? Titanium
How Do They Do It? Titanium (7 mins., Uploaded: 7 January 2012) A great, short overview of titanium, how it is ...
Heat Treating Oven Part of Norsk Titanium’s Ultra Lean Manufacturing Line
Norsk Titanium AS, the world’s leading provider of aerospace-grade, titanium additive manufacturing technology, today announced the groundbreaking of a new European ...