A manufacturer of saw blades and tool steels will amp up its heat treating capabilities with two floor-standing box furnaces. The new furnaces will be used for stress relieving and tempering large steel castings.
L&L Special Furnace Co., Inc. will deliver the model XLE3648 furnace with an electric vertical door, an alloy hearth, and a complete control system. This model has an effective work zone of 34" x 34" x 44" and will be used for heat treating various tool steels for saw blades. The model FB336, with an effective work zone of 36" x 36" x 72", is fiber-lined and will be used to temper and stress relieve steel castings.