New Diffusion Hardening Vessel Expands Stainless Steel Processing in North America
Bodycote has installed a new treatment vessel at its Mooresville, North Carolina facility, expanding its capability to process larger stainless steel components and broadening surface hardening capabilities for manufacturers in North America.
The new treatment vessel can accommodate components up to 79 inches (2 meters) in length and 47 inches (1.2 meters) in width, enabling the surface hardening of larger and heavier stainless steel parts than previously possible in North America for industries such as oil and gas, food and beverage, and medical technology.

S³P Technical Manager in North America
Bodycote
The installation supports a low-temperature diffusion hardening process that increases the surface hardness of stainless steel components while maintaining the corrosion resistance. This capability is part of Bodycote’s ADM® stainless steel treatment offering now available in North America. The process can treat austenitic, duplex, and martensitic stainless steels, including alloys commonly used in load-bearing and high-strength applications.
Reflecting this demand, Temitope Oluwafemi, Bodycote’s S³P technical manager in North America, said, “Demand is growing for stainless steel components that can deliver longer service life in harsh operating environments and to demanding standards, without introducing the risks associated with coatings. Bringing ADM capability to the U.S. allows us to support [clients] locally, reduce lead times, and expand what’s possible for larger stainless steel components across multiple industries.”
Press release is available in its original form here.
The main image shows the microstructure of surface hardened stainless steel AIS1660 (1.4980) | Image Credit: Bodycote