Heat Treat Expansion Complete at McGinnis Rolled Rings
McInnes contracted with Can-Eng Furnaces Intl. Ltd. to design and install the most advanced technology to process large diameter product. The furnace & quench tank designs are augmented by a customized material handling system by Dango & Dienthal Hollerbach GmbH capable of processing loads up to 25 tons. The system’s fast transfer from furnace to quench tank provides optimal and repeatable process controls.
“This new bay nearly doubles our quenched and tempered offerings to the power transmission industry and adds the ability to solution anneal large diameter stainless steel rings. Also, the addition of water quenching improves our ability to meet the high property demands of the custom flange markets,” said Shawn O’Brien, VP Sales & Marketing.
The expanded heat treat operation will officially begin service on March 1, 2016.