Chinese Expansion To Double Capacity of Heat-Treated Aluminum for Automotive Industry

The leading manufacturer of rolled aluminum products recently broke ground on the expansion of its automotive aluminum manufacturing facility in Changzhou, China, where the facility will double its capacity of heat-treated aluminum sheet.

Satish Pai, Managing Director of Hindalco Industries, the parent company of Novelis Inc.

Novelis, Inc., hosted members of the community, customers and government officials in the groundbreaking ceremony launching the $180 million investment to increase capacity by 100,000 metric tons in order to better meet the growing demand for automotive aluminum in Asia. The facility will be equipped with a high-speed slitter and a fully automated packaging line. The project is scheduled to be complete in 2020 in order to align with key customer’s vehicle-launch plans.

“As market demand for lighter, more fuel-efficient vehicles continues to grow, Novelis will play a critical role in supporting the next generation of automotive innovation and design,” said Satish Pai, Managing Director of Hindalco Industries, the parent company of Novelis Inc. “This expansion reinforces our steadfast commitment to our customers and communities, and reaffirms our continued confidence in this ever-growing market.”

 

Chinese Expansion To Double Capacity of Heat-Treated Aluminum for Automotive Industry Read More »

Novelis China Supplying Sheet for Aluminum-Intensive Jaguar XFL

BOTW-50w  Source:  Light Metal Age –

Novelis China is supplying aluminum solutions for the all-new, aluminum-intensive Jaguar XFL, the first Jaguar model from Chery Jaguar Land Rover Automotive Co., Ltd. Chery Jaguar Land Rover started up production at its Changzhu Plant – China’s first purpose-built aluminum body shop, where the Jaguar XFL will be assembled. Most of the aluminum alloys for the Changzhu body shop will be supplied by the Novelis sheet finishing and heat-treatment plant located in Changzhu, China.

Read more:

Novelis China Supplying Sheet for Aluminum-Intensive Jaguar XFL Read More »