Special Springs Enhances Production Capabilities with Nitriding System
Springs and gas cylinders manufacturer Special Springs has bolstered its heat treating capacity with a new nitriding turnkey system. By adding to their production capabilities, the company aims to meet the growing demands of their client base, which includes the automotive, appliance, agriculture, and heavy equipment sectors.

Technical Sales Manager
NITREX Poland
This expansion follows a long-standing collaboration, which began in October 2004 with the commissioning of Special Springs‘ first Nitrex nitriding turnkey system and continues with the installation of an NXK series furnace in July 2024.
The springs manufacturer installed the compact NXK-812 furnace, which incorporates the heat treat technologies Nitreg and ONC, to accommodate increased capacity and optimize production efficiency. The system has a load capacity of 1,200 kg (2,600 lbs); the two furnaces work alongside each other, utilizing interchangeable material handling equipment to ensure continuity and efficiency in their production process.
“[Special Springs’] decision to expand with a second Nitrex system highlights the strength of our solutions and the trust we’ve built over the years. We look forward to seeing future advancements supporting advanced gas springs exemplifies the synergy achieved through strategic collaboration, advanced heat treat technologies, and exceptional support,” said Marcin Stoklosa, technical sales manager of EMEA region at Nitrex.
The press release is available in its original form here.