Metallography Techniques and Fundamentals Classes Offered in U.S., U.K.
SumMet™ Fundamentals of Metallographic Techniques, a three-day course designed for both metallographers without formal training and experienced metallographers who want to learn the latest preparation techniques, will be offered throughout 2018 in the United States and Europe.

Buehler, an ITW company and a global industrial manufacturer of value-added consumables and specialty material testing equipment, announces that classes will be held at the Buehler headquarters in Lake Bluff, Illinois and in the company’s laboratories in Düsseldorf and Esslingen in Germany, and Coventry in the United Kingdom. The courses begin in March 2018 and run through November 2018.
According to Dr. Mike Keeble, United States laboratory and technology manager, “Buehler recognizes the need to educate lab technicians with the most current equipment and methods. The fundamentals of sectioning, mounting, grinding and polishing are covered both in theory and practice in this course. They are based on the SumMet methods developed at Buehler since 1936. Students will also be exposed to optical microscopy, etching, hardness testing, and microstructural interpretation.”
In the United States, the class is taught by Dr. Mike Keeble, who has 12 years of experience with Buehler specializing in applications support, as well as more than 10 years of experience in metallurgy Research and Development for key industries like aerospace, automotive, electronics, energy, metals and medical devices.
In Düsseldorf, Germany, the class is taught by Matthias Pascher, Buehler product manager for hardness testing and imaging analysis. Mr. Pascher has extensive applications support in metallography, hardness testing, and imaging analysis combined with a solid background in material science.

In Coventry, United Kingdom, the class is taught by Dr. Evans Mogire, EMEA laboratory and technical manager. Dr. Mogire has extensive experience in metallography of metallic, polymeric, and ceramic materials, as well as more than nine years of experience in metallurgy R&D.
Technicians and engineers can register on the Buehler website https://www.buehler.com/training.php . For additional information on Buehler please visit the Buehler website.
Metallography Techniques and Fundamentals Classes Offered in U.S., U.K. Read More »