Name: Danielle Cote
Company: Worcester Polytechnic Institute
Position: Research Scientist, Research Assistant Professor, Assistant Professor
As a research scientist, research assistant professor, and assistant professor at Worcester Polytechnic Institute, Danielle has been the leader in developing heat treat processes for aluminum ally powders. Her work has changed the powder preparation processes for the cold spray industry. She is a great mentor and advisor, overseeing the work of 5 PhD students on thermal processes.
Nominated from within her own company, WPI