LPC

Aerospace Manufacturer Adds LPC Furnace

An Asian aircraft parts manufacturer has chosen a horizontal vacuum furnace intended for vacuum carburizing aircraft parts. The furnace will produce gears used in aircraft structural sub-assemblies.

Maciej Korecki, VP, Vacuum Furnace Segment at SECO/WARWICK (source: SECO/WARWICK)

The SECO/WARWICK furnace is designed for low-pressure carburizing (LPC), equipped with a horizontal chamber with dimensions of 900 x 600 x 600 mm and a graphite chamber with a gas hardening system at a pressure of 6 bar.

“LPC technology,” said Maciej Korecki, Vice-President of the SECO/WARWICK Group Vacuum Segment, “is an increasingly popular solution. Its main advantage is the ability to carry out an efficient and effective carburizing cycle in a much shorter time than in atmospheric furnaces. This furnace ensures higher productivity and consequently, lower process costs and a quick return on investment. Carrying out the process in vacuum, on the other hand, increases the operational safety, because it does not involve explosive and flammable gases. LPC eliminates direct CO₂ emissions from the carburizing atmosphere.”

The original press release from SECO/WARWICK is available here.


Find Heat Treating Products And Services When You Search On Heat Treat Buyers Guide.Com

Aerospace Manufacturer Adds LPC Furnace Read More »

Case Study: Heat Treat Equipment Meets the Future Industry Today

OCModern industry trends and expectations pose new challenges to heat treating equipment; in addition to the expected requirements (e.g., safety, quality, economy, reliability, and efficiency), factors like availability, flexibility, energy efficiency, environmental, and the surrounding carbon neutrality are becoming increasingly important.

Maciej Korecki, vice president of Business Development and R&D at SECO/WARWICK, presents this special Technical Wednesday case study for the last day of FNA 2022 to focus on an equipment solution that meets these modern industry demands: a semi-continuous vacuum furnace for low-pressure carburizing (LPC) and high-pressure gas quenching (HPGQ).


Maciej Korecki
Vice President of Business of the Vacuum Furnace Segment
SECO/WARWICK

Introduction

At least 60 years ago, vacuum furnaces first appeared in the most demanding industries (i.e., space and aerospace), then spread to other industrial branches, and are now widely implemented in both mass production and service plants. Use of vacuum technology does not look like it is slowing down anytime soon.

Contact us with your Reader Feedback!

The driving forces behind this growth in vacuum technology are two-fold: first, the increasing heat treatment requirements that result from the directions of industrial development and production systems, and second, environmental protection, where the advantages of vacuum technologies are undeniable.

 

Traditional Atmospheric Technology

Case hardening by carburizing is one of the most widely used heat treatment technologies. It consists in carburizing (introducing carbon to the surface) followed by quenching of the carburized layer. Typically, the work is carburized in a mixture of flammable gases (CO, H2), and quenched in oil in an atmosphere furnace, using methods developed in the 1960s.

These methods have a history of development, though the question remains if the technological developments can keep up with the requirements of modern industry. Safety is an issue with this method due to the use of flammable (and poisonous) gases and flammable oil, as well as open flame, which in the absence of complete separation from the air can lead to fire, or poisoning.

In addition, they affect their environment by releasing significant amounts of heat, polluting the surroundings with quenching oil and its vapors. They require the use of washers and cleaning chemicals, emit annually tens or even hundreds of tons of CO2 (greenhouse gas, the main culprit of global warming and dynamic climate change) coming from the carburizing atmosphere, and for these reasons, they need to be installed in dedicated so-called “dirty halls” separated from other production departments.

The resulting requirement to limit the temperature of the processes to 1688-1706 oF (920-930oC) is also not without importance, as it blocks the possibility of accelerating carburization and increasing production efficiency (due to the use of metal alloys in the construction, the service life of which drops dramatically at higher temperatures) and the formation of unfavorable intergranular oxidation (IGO), which is a characteristic feature of the atmospheric carburizing method.

Quenching in oil is effective, but it does not have precise controllable, repeatable, and ecological features that heat treaters may need. Due to the multiphase nature of oil quenching (steam, bubble, and convection phase) and the associated extremely different cooling rates, it is characterized by large and unpredictable deformations within a single part and the entire load. Furthermore, there is no practical method to influence and control the quench process.

Modern Vacuum Technology with LPC and HPGQ

Vacuum carburizing appeared as early as the 1970s, but it could not break through for a long time due to the inability to control and predict the results of the process, and heavy contamination of the furnaces with reaction products.

The breakthrough came in the 1990s, when acetylene began to be used as a carbon-bearing gas and computers were employed to control and simulate the process. Since the beginning of the 21st century, there has been a rapid development of the low pressure carburizing (LPC) technology and an increase in its industrial demand, which continues today with an upturn.

Vacuum carburizing occurs with the aid of hydrocarbons (usually acetylene), which catalytically decompose at the surface, providing carbon that diffuses into the material. The process is carried out under negative pressure (hundreds of times less than atmospheric pressure) and is very precise, efficient, and uniform due to the very high velocity and penetration capacity of the gas molecules, allowing the carburizing of large and densely packed loads and hard-to-reach surfaces such as holes.

In addition, the use of non-oxygen-containing hydrocarbon atoms eliminates the qualitative problem of intergranular oxidation (IGO). The process is completely safe, there is no flammable or poisonous atmosphere in the furnace and no open flame, and the furnace can work unattended and is fully available and flexible, i.e., it can be turned on and off on demand, which does not require any preparation. Similarly, changing the carburizing parameters takes place efficiently.

Due to the design of the vacuum furnace and the use of materials with high resistance to temperature, i.e., graphite — the only limitation for the temperature of the carburizing process is the steel from which the parts are made — it is possible to carburize at higher temperatures than traditional methods allow. The result is a significantly shorter carburizing time and increased furnace efficiency versus what can be achieved in an atmosphere furnace.

Neutral gas cooling was included with the vacuum furnaces. Initially, engineers used a cooling gas (nitrogen or argon) at near ambient pressure and natural convection. Subsequent solutions introduced fan-forced gas flow in a closed circuit. The cooling efficiency under such conditions was hundreds of times lower compared to that of oil, allowing only high-alloy steels and parts with very limited cross-sections to be hardened. Over the following decades, the development of HPGQ was focused on improving cooling efficiency by increasing pressure and velocity and using different types of gas and their mixtures. Current systems have cooling efficiencies on a par with oil-based systems and enable the same types of steel and parts to be hardened, with the advantage that deformation can be greatly reduced and reproducible, and the process is completely controllable (through pressure and gas velocity) allowing any cooling curve to be executed.

Vacuum technologies have an ecological edge. Because of their design and processes, vacuum furnaces do not interfere with the immediate surroundings and are environmentally friendly, so they can be installed in clean halls, directly in the production chain (in-line). They emit negligible amounts of heat and post-process gases which are not poisonous and contain no CO 2 at all. Gas quenching eliminates harmful quenching oil and the associated risk of fire and contamination of the immediate environment, as well as the need for equipment and chemicals for its removal and neutralization. Nitrogen used for cooling is obtained from the air and returned to it in a clean state, creating an ideal environmentally friendly solution.

The presented advantages of vacuum technologies influence its dynamic development and increase the demand of modern industry, and the gradual replacement of atmospheric technologies.

Vacuum furnaces are available in virtually any configuration: horizontal, vertical, single, double, or multi-chambered, tailored to the process and production requirements. In light of recent global changes, requirements, and industrial trends, special attention should be paid to disposable, flexible, and rapidly variable production and process systems, as well as independent and autonomous systems, which include a three-chamber vacuum furnace for semi- continuous heat treatment, equipped with LPC and HPGQ.

Three-Chamber Vacuum Furnace — CaseMaster Evolution Type CMe-T6810-25

This is a compact, versatile, and flexible system designed for vacuum heat treatment processes for in-house and commercial plants, dedicated to fast-changing and demanding conditions in large-scale and individual production (Fig. 1). It enables the implementation of case hardening by LPC and HPGQ processes and quenching of typical types of oil and gas hardened steels and allows for annealing and brazing. It is characterized by the following data:

  • working space 610x750x1000 mm (WxHxL)
  • load capacity 1000 kg gross
  • temperature 2282oF (1250oC)
  • vacuum range 10-2 mbar
  • cooling pressure 25 bar abs
  • LPC acetylene gas
  • Installation area 8x7m

The furnace is built with three thermally and pressure-separated chambers (Fig. 2.), and operates in a pass-through mode, loaded on one side and unloaded on the other, simultaneously processing three loads, hence its high efficiency. The load is put into the pre-heating chamber, where it is pre-heated to the temperature of 1382oF (750oC), depending on the requirements: in air (pre-oxidation), nitrogen or vacuum atmosphere. It is then transferred to the main heating chamber, where it reaches process temperature and where the process is carried out (e.g., LPC).

In the next step, the charge is transported to the quenching chamber, where it is quenched in nitrogen under high pressure. All operations are automatic and synchronized without the need for operator intervention or supervision.

Fig. 2. Construction and schematic furnace cross-section CMe-T6810-25.
Source: SECO/WARWICK

Particularly noteworthy is the gas cooling chamber, which in nitrogen (rather than helium) achieves cooling efficiencies comparable to oil (heat transfer coefficient >> 1000 W/m2K), thanks to the use of 25 bar abs pressure and hurricane gas velocities in a highly efficient closed loop system. The cooling system is based on two side-mounted fans with a capacity of 220 kW each, forcing with nozzles an intensive cooling nitrogen flow from above onto the load, then through the heat exchanger (gas-water), where the nitrogen is cooled and further sucked in by the fan (Fig. 3). The cooling process is controllable, repeatable, and programmable by gas pressure, fan speed and time. An intense and even cooling is achieved. The result is the achievement of appropriate mechanical properties of parts with minimal hardening deformations, without the use of environmentally unfriendly oil or very expensive helium.

Fig. 3. Cross-section of the furnace CMe-T6810-25 cooling chamber.
Source: SECO/WARWICK

An integral part of the furnace system is the SimVaC carburizing process simulator, which enables the design of furnace recipes without conducting proof tests.

Distinctive Features of the CMe-T6810-25 Furnace

The advantages of this type of furnace — versus more traditional or past forms — can be demonstrated in a number of usability and functional aspects, the most important of which are the following:

Safety:

  • Safe, no flammable and poisonous atmosphere
  • No open fire

Production and installation:

  • Intended for high volume production (two to three times higher output when compared to single- and double-chamber furnaces)
  • Effective and efficient LPC (even five times faster than traditional carburizing)
  • Total process automation & integration
  • Clean room installation
  • Operator-free
  • Compact footprint

Quality:

  • High precision and repeatability of results
  • Uniform carburizing of densely pack loads and difficult shapes (holes)
  • No decarburization or oxidation
  • Elimination of IGO
  • Ideal protection and cleanliness of part surfaces
  • Accurate and precise LPC process simulator (SimVaC)

Quenching:

  • Powerful nitrogen quenching (neither oil nor helium is needed)
  • Reduction of distortion
  • Elimination of quenching oil and contamination
  • Elimination of washing and cleaning chemicals

Operational:

  • Flexible, on-demand operation
  • No conditioning time
  • No human involvement and impact
  • High lifespan of hot zone components — i.e., graphite
  • No moving components in the process chamber

Ecology:

  • Safe and environmentally friendly processes and equipment
  • No emission of harmful gases (CO, NOx, SOx)
  • No emission of climate-warming gas CO2

Based on the CMe-T6810-25 furnace performance, it is rational and reasonable to build heat treatment systems for high-efficiency and developmental production in a distributed system by multiplying and integrating further autonomous and independent units. The reasons for doing so are because the furnace design affords:

  • No risk of production total breakdown
  • Unlimited operational flexibility
  • Less initial investment cost
  • Unlimited multiplication
  • No downtime while expansion
  • Independent quenching chamber
  • Independent transportation
  • Independent control system

The characteristics, capabilities and functionalities of the CMe-T6810-25 furnace fit very well with the current and developmental expectations of modern industry and ecological requirements, which is confirmed by specific implementation cases.

Case Study

The three-chamber CaseMaster Evolution CMe-T6810-25 vacuum furnace was installed and implemented for production at the commercial heat treatment plant at the Polish branch of the renowned Aalberts surface technologies Group in 2020.

Fig. 4. Gearwheel used in the case hardening process.
Source: SECO/WARWICK

The CMe furnace, together with the washer and tempering furnace, forms the core of the department's production, which is why the furnace is operated continuously. Last year, the furnace performed over 2000 processes and showed very high quality (100%) and reliability (> 99%) indicators. The very high efficiency of the furnace was also confirmed, which, with relatively low production costs, contributes to a very good economic result.

The case hardening process on gearwheels used in industrial gearboxes was taken as an example. The wheel had an outer diameter of about 80 mm and a mass of 0.52 kg (Fig. 4), and the load consisted of 1344 pieces densely packed in the working space (Fig. 5) with a total net weight of 700 kg (920 kg gross) and 25 m2 surface to be carburized. The aim of the process was to obtain an effective layer thickness from 0.4 – 0.6 mm with the criterion of 550 HV, surface hardness from 58 – 62 HRC (Rockwell Hardness C), core hardness at the gear tooth base above 300 HV10 and the correct structure with retained austenite below 15%.

Fig. 5. A photograph of the arrangement of gearwheels in the load.
Source: SECO/WARWICK

The LPC process was designed using the SimVaC® simulator at a temperature of 1724oF (940oC) and a time of 45 min, with 3 stages of introducing carburizing gas (acetylene), obtaining the appropriate profile of carbon concentration in the carburized layer, with a content of 0.76% C on the surface (Fig. 6).

The process was carried out in the CMe-T6810-25 furnace and had the following course from the perspective of a single load (Fig. 7):

  1. Loading into a pre-heating chamber, heating and temperature equalization in 1382oF (750oC) (100 min in total).
  2. Reloading to the main heating chamber, heating and temperature equalization in 1724oF (940oC), LPC, lowering and equalizing the temperature before quenching in 1580oF (860oC), reloading to the cooling chamber (total 180 min).
  3. Gradual quenching at a pressure of 24, then 12 and 5 bar, discharge of the load from a quenching chamber (total of 25 min).

The load stayed the longest in the main heating chamber – for 180 minutes. This means that with the continuous operation of the furnace in this process, the cycle will be just 180 minutes, i.e., once every three hours the raw load will be loaded, and the processed load will be removed from the furnace.

In the next step, the parts underwent tempering at a temperature of 160oC.

The result of the process was tested on ten parts taken from the reference corners and from the inside of the load. The correct layer structure (Fig. 8) and hardness profile (Fig. 9) were achieved, and all the requirements of the technical specification were met (Tab. 1).

Tab. 1. Comparison of the parameters required and obtained in the process.
Source: SECO/WARWICK

During the process, the consumption of the costliest energy factors was monitored and calculated, and the results per one load are as follows:

  • Electricity – 550 kWh
  • Liquid nitrogen – 160 kg
  • Acetylene – 1.5 kg
  • CO2 emissions – 0 kg

Cooling water and compressed air consumption have not been included as they have a negligible impact on process costs.

Summary: Efficiency and Economy

As a result of the process, all technological requirements have been met, obtaining the following indicators of efficiency and consumption of energy factors calculated for the entire load and per unit net weight of the load (700 kg):

  • Capacity: 3h/load; 233 kg/h; 5 thousand tons/year (6500 h)
  • Electricity: 550 kWh; 0.79 kWh/kg
  • Liquid nitrogen: 160 kg; 0,23 kg/kg
  • Acetylene: 1,5 kg; 2,1 g/kg
  • CO2 emissions : 0 kg; 0 kg/kg

On this basis, it is possible to estimate the total cost of energy factors in the amount of approximately EUR 100 per load or approximately EUR 0.14/kg of net load (assuming European unit costs of 2021). It is important that these costs are not burdened by CO2 emission penalties, as can happen with more traditional furnaces.

To sum up the economic aspect, based on an example process, a CMe furnace capacity of 1,500 net tons of parts per year was achieved for 6500 hours of annual furnace operation, at a cost of energy factors of about 100 EUR per load, or 0.14 EUR per kg of parts. The economic calculation is very attractive, and the return on investment (ROI) is estimated at just a few years.

Conclusion

While the advantages of this type of vacuum application are clear from this case study, the example discussed here does not represent the full capabilities of the CMe-T6810-25 furnace, even this process can be optimized and shortened, thereby increasing the furnace's efficiency, and reducing costs. It is possible to carry out carburizing processes (LPC) or hardening alone in a 1.5 h cycle, which would double the capacity of the furnace and similarly reduce the cost of energy factors and shorten the ROI time.

 

For more information:

Go to www.secowarwick.com


Find heat treating products and services when you search on Heat Treat Buyers Guide.com


 

Case Study: Heat Treat Equipment Meets the Future Industry Today Read More »

Heat Treat Radio #65: The Future of Heat Treat, a Conversation with Piotr Zawistowski

Heat Treat Today publisher, Doug Glenn, sat down with heat treating specialist, Piotr Zawistowski, the managing director at SECO/VACUUM, to hear what he believes the future of heat treat holds. Karen Gantzer and Bethany Leone from Heat Treat Today also joined the conversation, recorded at the ASM Heat Treat Show 2021. In this episode, you’ll learn why Piotr believes LPC, automation, and predictive maintenance are the future of heat treat and  how to get there.

Below, you can watch the video, listen to the podcast by clicking on the audio play button, or read an edited transcript.




The following transcript has been edited for your reading enjoyment.

Bethany Leone (BL): Peter first shared how SECO/WARWICK was on a mission to actualize the future of heat treat.

Piotr Zawistowski (PZ):  I think we are on a mission, that is, SECO/WARWICK and I.  I think the future of heat treatment will be LPC for carburizing, and gas quenching for quenching instead of oil.  I think the future is LPC and hydrogen quenching, to be honest.  Right now, most of carburizing is done in a carburizing atmosphere, and most of the quenching, as I know it.  I think that everything is moving in the vacuum direction, if you will, but we're not there yet.  So, that's our mission, in general.

Members of Heat Treat Today sat down with Piotr Zawistowski, managing director of SECO/VACUUM, at the ASM Heat Treat Show 2021.

I think I showed you a graph with what is the difference in quenching between oil and gas.  Right now, with 25 bar quenching, we are on the level of slow oil.  To get there, we have to use helium, but it's expensive, it's not economical.  We can go to hydrogen, which is the speed of oil and it's everywhere, it's cheap.  I think this is the future.

BL: This idea that the future of heat treat will be LPC and gas quenching – specifically with hydrogen – means moving in the vacuum direction, as Peter noted. But how fast will this transition come, especially given safety concerns with the use of hydrogen as a quenchant?

PZ: Exactly, that is the concern right now.  I think it will come, but we are far away from it.  Anyway, we don't have to go to hydrogen immediately, but I think we should go to nitrogen for now.  We have some solutions for that, and on top of that, I think we will go from regular carburizing to LPC.  It's not easy for people to switch, so our mission is for us to try to convince people to switch to LPC.  We would like to make it as easy as possible for them so that's why—maybe 20 years ago—we thought about starting.  Because we had quenching and carburizing, we thought, let's maybe leave quenching the same and start with carburizing.  So, we developed vacuum oil quench furnaces just to make it easier so they only have to change one thing at a time.  But then, we thought, it's a leap for them anyway because those are different oils and it's a vacuum oil.  So, right now, we're introducing a furnace with vacuum carburizing with the regular atmosphere is a quenching chamber in regular oils that all the heat treaters have known for years.

DG:  This is the SuperIQ?

PZ:  This is the SuperIQ.  I don't want to make it commercial, but this is another step.  If you look at our wall here, we have six different products and five of them are for carburizing.  It starts with Vector.  It can have carburizing but it doesn't have to be, but anyway, they all are connected with carburizing.  I think the mission is to convince people and to switch, in the industry, from all the messy dangerous, open-fire furnaces to new, clean, better technology.

Piotr sharing SECO/WARWICK vision for the future of heat treating.

BL: As we just heard, these are big transitions. So, if the first step towards heat treat with LPC is for heat treaters to use atmosphere carburizing with oil quench, what are the next steps to move to a fully vacuum-based future?

PZ:  Step number two is vacuum oil quench and step number three is vacuum carburizing or LPC and high pressure gas quench.  That is the future, in my opinion, and with hydrogen.

BL: As a review, moving to LPC could look like, first, using a traditional vacuum furnace with atmosphere capabilities, then, heat treating with vacuum oil quench, and finally, heat treating with LPC and high pressure gas quench. If such a transition is appealing, it would be good know what the productivity improvements of LPC are. . .

PZ:  So, it depends; there are a couple factors.  First, we have to take into account what kind of a case that we're talking about.  But, in general, I can tell you that the productivity increase should be 50%, or even 100%, or more.

DG:  You can double the amount of product through in the same amount of time?

Piotr walks through challenges to overcome to achieve an LPC and hydrogen heat treat future.

PZ:  Yes.  And, it's just as simple with increasing the temperature, so we are not limited with low pressure carburizing with the temperature, whereas there is a limit that atmosphere carburizing can be done. So, we have a lot of possibilities here.

BL: So, a 50-100% increase in productivity and an increased temperature range comes along with low pressure carburizing, LPC. When considering LPC, there is the question of how traditional specification, which clearly state the necessity of atmosphere carburizing, can be compatible with this newer technology.

PZ:  Yes, and those specs are changing.

DG:  Is that going to be a hindrance?

PZ:  Yes, it is right now, especially in aerospace.  The automotive industry, they moved already to LPC, but aerospace we are trying to help to change those specs, and they are changing as we speak.  A lot of those specs are still from the '80s, and there was no LPC back then.  As you know, in aerospace, it is not easy to change a spec, but this is happening right now, as we speak.

DG:  Are you guys involved with changes from Nadcap and all?

PZ:  Yes, and we are involved in major aerospace players.  We are doing tests for them and we are delivering them LPC furnaces.  Some of them are still doing R&D, but this is a first step.  With some of them, we are starting to see real production with LPC in aerospace, so we are getting there.

BL: To be sure, integrating the technical creation of specs by bringing heat treaters in touch with key end-users in the industry is necessary to have standards reflect effective heat treating techniques. Aside from standards, is there any resistance to adopting low pressure carburizing?

PZ:  I think, people are afraid of what is new: atmospheric carburizing is very simple and it is well known, vacuum carburizing is something different.  So, for atmosphere carburizing, it's only to control the potential in the furnace and time of carburizing.  In vacuum carburizing, it's not that easy- you have to have a special simulator to create a recipe.  People are afraid of it, but they shouldn't be because there is software.  We have software that can make that recipe really easy and pretty quick.  People are just afraid of something new.

SECO/WARWICK's SimVac

We have it [simulator] to create a recipe for LPC for the purpose of carburizing and we actually provide it.  This is our own simulator and we provide it with the equipment so it's very, very easy.

BL: In addition to an aversion to the new and the changes that may be involved, folks have a real concern with distortion. Peter then addressed this concern. . .

PZ:  High pressure gas quenching, in general, is better, but there are other methods.  It is not only us, but we are all trying to limit the distortions; we cannot say “eliminate” because that is impossible, but we can try to limit the distortion and control the distortions.  What we introduced to the market is our 4D quench technology, “fourth” dimension is that we rotate the part during quenching.

BL: While there is resistance that may be from outdated industry specs, a suspicion of the new, or technical concerns which the industry is continually addressing, Peter was sure note that there are, in fact, drivers that are encouraging heat treaters to move towards LPC.

PZ:  I think, the driver is both productivity and safety.  As an example, the [US] Biden administration just committed to reduce CO2 emission by 50% by the end of the decade.  This is good technology and there is a lot of fuel to emission out of atmosphere carburizing, internal and external.  But, there will be a push for climate change and CO2 emission.  I think, it's not only mandates, but, I think, in Europe, for example, they have a lot of grant; there is a lot of government money you can get if you are reducing the CO2 emission.  I think, for the heat treaters, it should be easy to capitalize on it.  As I said, no CO2 emission on LPC.  There is no emission at all.  That is the beauty of the technology.

Kanthal notes the electric shift that is predominantly occurring in Europe

Find this article in the August 2021 digital edition

BL: Certainly, financial incentives to adopt “greener” technologies as well as personal desire to do so would be motivating. Is there anything about the heat treated parts cosmetically that would make LPC attractive?

PZ:  Of course.  And, you don't have to wash it after, which is great.  It depends, as we still can have LPC and oil quench, you have to wash it, but if you can get to the gas quench, you've eliminated the wash part.  They just look nice and shiny and bright.  The color is better and you can eliminate washing.

BL: It is clear that LPC, one of the factors that plays into the future of heat treat as Peter envisions, has challenges and benefits for heat treaters to consider. Peter then talked about two additional factors for the future of heat treat: automation and predictive maintenance.

PZ:  There are two other factors.  One is automation, which is something big and it's more and more especially nowadays with the labor issue.  But, it is to eliminate the human error part of it.  On top of that, it is the traceability of the parts.  More and more customers would like no operators and the machine has to run by itself.  We have that—a full system of equipment.  You just place the basket with parts, or several baskets, and then the robot takes it to the furnace, carburizes, quenches, tempers, washes and then it comes out, completely untouched.  Robots are the automated loader. That is the direction.

Another is predictive maintenance, which is a big deal right now.  By predictive maintenance, I mean that the system has to predict the failures or the downtimes.  A lot of systems, which are available on the market are called “predictive maintenance”, but they are reactive.  For example, they have sensors on the machine and if something breaks, it sends you an email message, or whatever.  Our SECO/PREDICTIVE, which is our predictive maintenance, is based on an algorithm.  The algorithm is written in such a way that the system learns on failures and the more equipment we have connected to it, the more data we have, like everything we have around us right now, all the Googles and Amazons and so on.  I think this is the future, as well.  So, everything has to be connected to one database to predict what will happen before it happens.

DG:  Can you give me an example?  Let's say you've got a high temperature fan inside a vacuum furnace.  How would the SECO/PREDICTIVE or predictive maintenance work on that?

PZ:  I think we would control the vibration on it.  I think that's one way to do it.  And, at a certain level, it would send a signal – "Watch out! - you are about to have a problem".  It is better to do it that way because, then, there is time to order a replacement or schedule something so it will not break.  But, the goal is to predict the failure before it happens.

BL: With thoughts of LPC, automation, and predictive maintenance on our minds, we then walked over to a display of various furnaces to see how SECO/VACUUM applied these insights to their own furnaces. Peter began with the Vector, a versatile high pressure gas quench furnace.

PZ:  This is a single chamber, multipurpose furnace.  It is for LPC carburizing and high pressure gas quenching.  This is the main furnace and, I think, 70% of what we sell. Maybe this is, like 50%.

Then 20% are the vacuum oil quench furnaces.  The vacuum oil quench furnaces heat processing chambers are the same as the Vector but then we can quench it in oil or we can have three chambers that can be continuous production or you can have oil quench on one side and high pressure gas quench on the other side.  We call it CaseMaster Evolution.  This is our middle step.  As I said, our goal is to go for LPC.

But, then, there is another one, the new baby in the family. [Peter then gestures to, what they call, the Super IQ vacuum furnace.]

For people, it was not easy to make a switch, so this is like a hybrid.  The processing chamber is vacuum carburizing but the quenching chamber is like a traditional atmosphere quench.  It is like a pure replacement: you can take one out and put this guy in.  You have all the benefits from low pressure carburizing but you operate mainly like an old and traditional furnace.  This is to make it easier in the transition.

BL: After learning how certain furnace designs can be helpful to heat treaters who have different processing needs or who are trying to convert to LPC, we then moved to see how LPC is being brought to pit-furnace size loads.

PZ:  This is another one, another tool in our mission, I would say.  This is a pit carburizing furnace but with LPC.  Right now, for big, heavy parts, they are carburizing atmosphere in pit furnaces and then they open the furnace and they just transfer it with a crane to an oil tank.  This is basically the same, but the pit furnace is with LPC.  There is nothing like this on the market right now.

We are trying to bring the LPC advantages to big parts and pit-style carburizers, as well.

BL: From LPC for large loads, we ended our tour with an LPC furnace with an interesting way to maintain traceability.​

PZ:  This is a single-piece carburizing furnace which we talked about.

So “CaseMaster”, which was the name of our traditional integral quench carburizing furnace in the past, we no longer do. Right now, if we have an RFQ for atmosphere carburizer, we go with LPC.

Thank yous from the group.

Doug Glenn <br> Publisher <br> Heat Treat Today

Doug Glenn
Publisher
Heat Treat Today

 

 

 

 

 

 

 

 

 

 

 

 

 


To find other Heat Treat Radio episodes, go to www.heattreattoday.com/radio and look in the list of Heat Treat Radio episodes listed.

 

Heat Treat Radio #65: The Future of Heat Treat, a Conversation with Piotr Zawistowski Read More »

Mercury Marine Launches Heat Treat Upgrades

HTD Size-PR LogoMercury Marine of Fond du Lac, Wisconsin, recently launched a plan to upgrade its heat-treating capabilities with a move to the low-pressure carburization and high-pressure gas quench system. The new plan incorporates completely automated vacuum heat treating systems.

In the partnership with ECM Technologies, the Nano vacuum heat treating system (pictured above) incorporates 20 bar nitrogen gas quenching along with low pressure carburizing (aka vacuum carburizing). The Nano will operate several different carburizing, hardening, and spheroidizing processes simultaneously.

This change marks a departure from Mercury’s traditional atmospheric carburization and oil quench system while benefiting from advantages that come with vacuum processing:

  • Applies vacuum heat treating in lieu of traditional atmosphere (elimination of intergranular oxidation & highly repeatable process with consistent results)
  • Employs preventive maintenance planning, remote system status access, and facility information systems integration
  • Relocates heat treat from a secondary location to the clean, controlled environment of the machining centers
  • Converts to small batch processing principles to maximize process efficiency
  • State-of-the-art growth with ECM’s advanced system automation and robot capability with load building and breakdown
  • Controls downstream operations by matching incoming dunnage with exiting workpieces
  • Takes advantage of vapor and vacuum-based pre-cleaning technology to remove multiple machining lubricants
  • Incorporates cryogenic and tempering processes within the automated system

The system uses all CFC workload fixtures and ECM’s advanced automation fixture tracking to maintain a precise cycle count to know fixture life. For Mercury, this significantly reduces energy consumption and process cost per piece. Additionally, the vacuum process takes their heat treatment to a near-zero emissions for drivetrain components processed within the system.

Mercury Marine Launches Heat Treat Upgrades Read More »

GKN Gears Up with LPC Heat Treat Capabilities

HTD Size-PR LogoGKN Driveline Bruneck AG (GKN) is modernizing its hardening shop with two low pressure carburizing plants, gearing up for the future as a key location for the development and production of E-powertrains in the GKN group.

For the last three years, the GKN group has been concentrating the development and European production of E-powertrains at the Bruneck site in South Tyrol, Italy. Through an extensive investment program, the site was equipped with modern production technology, placing it at the core of GKN’s E-mobility strategy. Dating back to the 1960’s, the hardening shop consists of several conventional pusher furnace systems and will now be modernized with ALD Vacuum Technologies GmbH's vacuum furnaces.

"This state-of-the-art heat treatment technology puts GKN in a position to meet the unique challenges of E-powertrain production," states Matthias John, sales engineer at ALD.

Source: ALD-VT
ModulTherm plant installed at GKN

In comparison with conventional combustion engine transmissions, the transmissions installed in modern electric cars are exposed to significantly higher speeds and torques. Therefore, the mechanical and metallurgical properties, as well as the dimensional accuracy of the highly stressed parts have to meet particularly high requirements. In the future, GKN intends to meet this challenge with a multi-chamber plant-type ModulTherm, and for special applications, a SyncroTherm plant. Both plants were started up in the second half of 2020.

"ALD convinced us with both, the very good results regarding metallurgical properties and low distortion of the parts. Their excellent and competent consulting reinforced us in our decision in favor of the state-of-the-art technology," explains Gianni Del Favero, value stream manager Machining and Heat Treatment at GKN. "The process combination of low-pressure carburizing (LPC) and subsequent high-pressure gas quenching (HPGQ) allows GKN to optimally adjust the parts’ properties – flexibly and component-specifically," adds John.

During the first expansion phase, in addition to the ModulTherm plant consisting of a mobile quenching module and five treatment chambers, ALD delivered fully integrated peripheral tempering and preheating furnaces, a cleaning plant, a batch buffer, and an external charge transport system.

Source: ALD-VT
SyncroTherm plant installed at GKN

The plant can be expanded up to 10 treatment chambers, depending on demand over the following years. Consequently, GKN will be able to gradually replace the aging protective gas furnaces.

The SnycroTherm plant will mainly be used for parts which are especially susceptible to distortion. The small batch size allows for a more targeted and finely tuned quench, resulting in little change in the dimensions of the parts.

Additionally, heat treatment of small batches enables a more flexible and faster throughput of smaller load sizes throughout the overall production.

GKN Gears Up with LPC Heat Treat Capabilities Read More »

Enhancing Energy Efficiency of Thermochemical Vacuum-Processes and Systems

BOTW-50w  Source:  Heat Processing

“The energy optimization of thermoprocessing equipment is of great ecological and economical importance. Thermoprocessing equipment consumes up to 40 % of the energy used in industrial applications in Germany. Therefore it is necessary to increase the energy efficiency of thermoprocessing equipment in order to meet the EU’s targets to reduce greenhouse gas emissions. In order to exploit the potential for energy savings, it is essential to analyze and optimize processes and plants as well as operating methods of electrically heated vacuum plants used in large scale production. For processes, the accelerated heating of charges through convection and higher process temperatures in diffusion-controlled thermochemical processes are a possibility. Modular vacuum systems prove to be very energy-efficient because they adapt to the changing production requirements step-by-step. An optimized insulation structure considerably reduces thermal losses. Energy management systems installed in the plant-control optimally manage the energy used for start-up and shutdown of the plants while preventing energy peak loads. The use of new CFC-fixtures also contributes to reduce the energy demand.”

Enhancing Energy Efficiency of Thermochemical Vacuum-Processes and Systems Read More »

Skip to content