Temperature Monitoring and Surveying Solutions for Carburizing Auto Components: AMS2750E and CQI-9 Temperature Uniformity Surveys

This is the final installment in a 4-part series by Dr. Steve Offley (“Dr. O”) on the technical challenges of monitoring low-pressure carburizing (LPC)

12
Mar

Temperature Monitoring and Surveying Solutions for Carburizing Auto Components: Thermal Barrier Design

This is the third in a 4-part series by Dr. Steve Offley (“Dr. O”) on the technical challenges of monitoring low-pressure carburizing (LPC) furnaces.

12
Feb

Temperature Monitoring and Surveying Solutions for Carburizing Auto Components: The Data Logger

This is the second in a 4-part series by Dr. Steve Offley (“Dr. O”), Product Marketing Manager at PhoenixTM, on the technical challenges

08
Jan

Temperature Monitoring and Surveying Solutions for Carburizing Auto Components: Introduction

This is the first in a 4-part series by Dr. Steve Offley (“Dr. O”), Product Marketing Manager at PhoenixTM, on the technical

27
Nov

LEAX Installs Low Pressure Carburizing Furnace: Boost Hardening Capabilities

LEAX Group, a Swedish manufacturer of advanced components and subsystems for automotive, commercial vehicles, mining, construction, and general industry sectors,

06
Jul

ThermTech Expands Heat-Treat Furnace Line to Support Oil & Gas Industry

ThermTech, based in Waukesha, WI, recently added a batch integral quench furnace to their atmosphere heat-treat furnace line. The expansion

16
Feb

Patent Awarded to Endocarb System for Novel Carburizing Method

On January 10, 2017, the United States Patent and Trademark Office awarded patent number 9,540,721 to George Barbour, President of

09
Dec

Heat Treat Basics: Metal Urgency – Carburizing

  Source:  Thermal Processing Magazine “While some heat treatments are used to soften the material or improve its machinability, most

09
Nov

How to Minimize Axial Cracking Failures

  Source:  North American Windpower “Although the root cause of axial cracking failures in gearboxes is not well understood, there

08
Nov

Practical Approach to Determining Effective Case Depth of Gas Carburizing